Abstract AITranslate

Study was made on recovery of RE from the elution deposit ore in weatheringcrust of biotite granite. The raw material is leached by a selected strong-acid ammonium salt(ammonium sulfate .ammonium chloride and ammonium nitrate, etc. ). The extraction ratereached more than 95%. Leached solution of RE is controlled for PH by aqua ammonia, purified with ammonium sulfide, and precipitated with oxalate or ammonium bicarbonate to obtain pure oxide of RE.

KeyWords AITranslate

biotite granite. elution deposit ore of RE recovery of RE

1贺伦燕,王似男.我国南方离子吸附型稀土矿[J].稀土,1989(1):39-44. 被引量:52

1周新木,谈宏宇,徐招弟.蛭石对稀土离子的吸附性能研究[J].非金属矿,2004,27(2):5-7. 被引量:13

2党丽丽,金秉福,樊水淼,张伟,施楠.暖温带花岗岩风化壳中黑云母微量元素的富集与流失变化——以山东半岛院格庄花岗岩体风化壳为例[J].地球科学前沿(汉斯),2020,10(10):959-972.

1李燕,汪立今.蛭石矿物材料应用及开发初探[J].矿物岩石地球化学通报,2007(z1):104-107. 被引量:2

2孙杰,李洪元,吴爱菊.蛭石吸附Cu^(2+)、Pb^(2+)的影响因素研究[J].中国水运:下半月,2009,9(5):250-251.

3赵欣,张树礼,周丽娜.镍钛交联改性蛭石对染料废水的吸附性能研究[J].环境与发展,2011,23(10):145-147.

4胡光锁,李政一.废水处理中蛭石的应用研究进展[J].北京工商大学学报:自然科学版,2006,24(3):13-16. 被引量:12

5戴清清,宋绵新,张宝述,彭同江.溶液pH值对不同粒径蛭石吸附Cu^(2+)、Pb^(2+)的影响[J].矿业研究与开发,2006,26(3):56-58. 被引量:5

6耿曼,石林,徐稳定.蛭石作为燃煤固硫添加剂的实验研究[J].非金属矿,2006,29(4):28-30. 被引量:4

7徐景华,李益民,陈霞.改性蛭石对有机污染物的吸附特性研究[J].矿产综合利用,2007(4):29-31.

8徐景华,张丹君.改性蛭石对对硝基苯酚吸附特性的研究[J].中南林业科技大学学报,2008,28(3):88-92. 被引量:5

9尹敬群,付桂明,万茵,田君.从风化壳淋积型稀土矿浸取液提取稀土技术与发展[J].江西科学,2012,30(5):574-578. 被引量:5

10刘建明,丁凝,孙峰.稀土废水处理技术及资源化利用研究进展[J].环境保护与循环经济,2014,34(10):31-35. 被引量:4

1万林生,郭邻生.钨吸附过程阴离子分布规律及局部淋洗研究[J].稀有金属,1992,16(6):401-404. 被引量:4

2杨幼平,黄可龙.混合稀土氧化物微粉的制备与表征[J].稀土,1996,17(4):20-23. 被引量:4

3张长庚.复合浸出剂提取风化壳淋积型稀土矿[J].湿法冶金,1993(2):27-30. 被引量:1

4卢盛良,卢朝晖,吴南萍,肖青.淋积型稀土矿原地浸矿几项技术问题的解决途径[J].湿法冶金,1997,16(2):22-24. 被引量:4

5张长庚,姚慧琴,欧阳克氙,饶国华.风化壳淋积型稀土矿原矿品位测定的探讨[J].湿法冶金,1994,13(2):64-65. 被引量:1

6伍建军,刘与枫.火山岩风化壳淋积型稀土分离厂设计探讨[J].有色冶金设计与研究,1992,13(3):145-150. 被引量:1

7桑原考夫,李挺.吸附于藻类的金,银,钴的洗提[J].国外锡工业,1994,22(1):16-21.

8曾之琪,肖连生,张贵清.碱性钨萃余液返回高压浸出的试验研究[J].稀有金属与硬质合金,2013,41(6):1-6. 被引量:1

9李裕芳.硫化铵中硫离子浓度的化学测定法[J].江西有色金属,1990,4(2):59-60. 被引量:1

10张登凯,王子阳,张泽彪,张利波,刘能生,周科华.硫化铵提硫过程中汞、银、锌的浸出行为研究[J].有色冶金设计与研究,2013,34(3):34-37. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF845.032[冶金工程—有色金属冶金]

Citation Information:

Study was made on recovery of RE from the elution deposit ore in weatheringcrust of biotite granite. The raw material is leached by a selected strong-acid ammonium salt(ammonium sulfate .ammonium chloride and ammonium nitrate, etc. ). The extraction ratereached more than 95%. Leached solution of RE is controlled for PH by aqua ammonia, purified with ammonium sulfide, and precipitated with oxalate or ammonium bicarbonate to obtain pure oxide of RE.

quote

GB/T 7714-2015 [1] HE Lun-yan, ZHOU Xin-mu, HE Yi, et al. Study on Recovery of RE from Elution Deposit Ore in Weathering Crust of Biotite Granite[J]. Rare Metals and Cemented Carbides, 1997(2): 1-6.
MLA [1] HE Lun-yan, et al., "Study on Recovery of RE from Elution Deposit Ore in Weathering Crust of Biotite Granite." Rare Metals and Cemented Carbides, no. 2, 1997, pp. 1-6.
APA [1] HE Lun-yan, ZHOU Xin-mu, HE Yi, & WANG Shi-nan. (1997). Study on Recovery of RE from Elution Deposit Ore in Weathering Crust of Biotite Granite. Rare Metals and Cemented Carbides(2), 1-6.
IEEE [1] HE Lun-yan, ZHOU Xin-mu, HE Yi, and WANG Shi-nan, "Study on Recovery of RE from Elution Deposit Ore in Weathering Crust of Biotite Granite," Rare Metals and Cemented Carbides, no. 2, pp. 1-6, 1997. keywords: {biotite granite. elution deposit ore of RE, recovery of RE}