Study on Tellurium Recovery Process from SbTe-containing Waste Catalyst AITranslate

Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tellurium was recovered from SbTe-containing waste catalyst by 4hagitation leaching with 2.5mol/L NaOH solution as the leaching agent under room temperature,atmospheric pressure and solid to liquid ratio 1∶5.And the leaching rate of tellurium reaches 95%.The deposition rate of tellurium is above95% under 1.5~4.0Vcell voltage and 5hdeposition with steel plate as the anode and stainless steel plate as the cathode.Finally,56.76%tellurium enriched product is obtained.

KeyWords AITranslate

SbTe-containing waste catalyst tellurium recovery process alkali leaching electrowinning tellurium enriched product

1林河成.从钴催化剂废料中回收氧化钴的研究[J].世界有色金属,1998(9):19-22. 被引量:3

2孟宪红,李悦,刘玉珍.加氢精制催化剂废料中钼的回收[J].环境保护,1996,24(4):39-41. 被引量:4

3林河成.用含钴催化剂废料制取氧化钴的研究[J].金属材料研究,2009,35(2):35-37.

4Daniel Veras Ribeiro,Joao A. Labrincha,Maircio R. Morelli.Use of Red Mud as Addition for Portland Cement Mortars[J].材料科学与工程:中英文版,2010,4(8):1-8. 被引量:1

5程耀庚,冯法伦,魏绪钧.以铈富集物为原料制取稀土抛光粉的研究[J].稀土,1998,19(4):39-41. 被引量:6

6章小明,刘晓红,陈剑军.回收锌制备氧化锌粉体的新工艺[J].云南化工,2011,38(6):50-53. 被引量:3

7祝优珍,赵由才.硫化物沉淀法选择性分离碱性锌溶液中的铅[J].上海应用技术学院学报:自然科学版,2001,1(1):59-63.

8吕福英,闵航,陈美慈,刘颖.一个高温厌氧直接转化纤维素为乙醇的高纯富集物[J].浙江大学学报:农业与生命科学版,2000,26(1):56-60. 被引量:19

9ZincOX公司在韩国的再生处理厂一季度产量创新高[J].中国铅锌,2015,0(5):50-50.

10毕舒.一种预处理金矿石和提取黄金的方法[J].黄金科学技术,2007,15(3):27-27.

Basic Information:

DOI:

Chinese Library Classification Number:TQ125.3[化学工程—无机化工]

Citation Information:

Tellurium was recovered from SbTe-containing waste catalyst by 4hagitation leaching with 2.5mol/L NaOH solution as the leaching agent under room temperature,atmospheric pressure and solid to liquid ratio 1∶5.And the leaching rate of tellurium reaches 95%.The deposition rate of tellurium is above95% under 1.5~4.0Vcell voltage and 5hdeposition with steel plate as the anode and stainless steel plate as the cathode.Finally,56.76%tellurium enriched product is obtained.

quote

GB/T 7714-2015 [1] LIU Yu-hui. Study on Tellurium Recovery Process from SbTe-containing Waste Catalyst[J]. Rare Metals and Cemented Carbides, 2015(3): 13-15.
MLA [1] LIU Yu-hui. "Study on Tellurium Recovery Process from SbTe-containing Waste Catalyst." Rare Metals and Cemented Carbides, no. 3, 2015, pp. 13-15.
APA [1] LIU Yu-hui. (2015). Study on Tellurium Recovery Process from SbTe-containing Waste Catalyst. Rare Metals and Cemented Carbides(3), 13-15.
IEEE [1] LIU Yu-hui, "Study on Tellurium Recovery Process from SbTe-containing Waste Catalyst," Rare Metals and Cemented Carbides, no. 3, pp. 13-15, 2015. keywords: {SbTe-containing waste catalyst;tellurium recovery process;alkali leaching;electrowinning;tellurium enriched product}