Thermal Latent Reductants for Controlled Degradation of Polyperoxides and Their Application to High Performance Dismantlable Adhesives AITranslate

Osaka City University; Osaka City University; Osaka City University; Osaka City University; Osaka City University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

1-Phenyl-3-pyrazolidone (PhP) having an active hydrogen was blocked by phenyl isocyanate derivatives to reduce its nucleophilicity, and the potential of the blocked PhP as a thermal latent reductant generating the organic reducing agent, PhP, was revealed for the first time. The degree of dissociation of the blocked PhP during heating in solution can be controlled by the steric hindrance of the isocyanate-blocking agents. The thermal latency of the blocked PhP for the sorbic ester-based polyperoxides, which undergo a serious reductive decomposition by PhP even at 30 °C, was investigated to accelerate the decomposition of the polyperoxides only at elevated temperatures. It was revealed that the stability of the polyperoxides was not significantly affected at 30 °C, and marked reductive decomposition of the polyperoxides together with thermal decomposition took place at elevated temperatures. For the block PhPs, which are highly compatible with the polyperoxides, the decomposition promotion effect increased with increasing the steric hindrance of the blocking agents, and the controlled decomposition of the polyperoxides was successfully achieved. Moreover, the addition of the blocked PhP resulted in the complete solubilization of sorbic ester-based cross-linked polyperoxides by heating, which was not able to be achieved without the blocked PhP. The performance of the debondable adhesive by using the sorbic ester-based cross-linked polyperoxides was improved by the addition of the blocked PhP, although hazardous isocyanate formation during the activation process may limit the practical application. Specifically, a faster decrease in the lap-shear adhesion strength by heating was accomplished. Furthermore, the same level of dismantlability was achieved in the wide range of heating temperatures and time, which is an important requirement for polyperoxides undergoing significant exothermic decomposition bringing about undesired temperature rise.

KeyWords AITranslate

degradable polymer network polymer polyperoxide redox reaction deprotection thermal latency dismantlable adhesive
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00422

Chinese Library Classification Number:

Citation Information:

1-Phenyl-3-pyrazolidone (PhP) having an active hydrogen was blocked by phenyl isocyanate derivatives to reduce its nucleophilicity, and the potential of the blocked PhP as a thermal latent reductant generating the organic reducing agent, PhP, was revealed for the first time. The degree of dissociation of the blocked PhP during heating in solution can be controlled by the steric hindrance of the isocyanate-blocking agents. The thermal latency of the blocked PhP for the sorbic ester-based polyperoxides, which undergo a serious reductive decomposition by PhP even at 30 °C, was investigated to accelerate the decomposition of the polyperoxides only at elevated temperatures. It was revealed that the stability of the polyperoxides was not significantly affected at 30 °C, and marked reductive decomposition of the polyperoxides together with thermal decomposition took place at elevated temperatures. For the block PhPs, which are highly compatible with the polyperoxides, the decomposition promotion effect increased with increasing the steric hindrance of the blocking agents, and the controlled decomposition of the polyperoxides was successfully achieved. Moreover, the addition of the blocked PhP resulted in the complete solubilization of sorbic ester-based cross-linked polyperoxides by heating, which was not able to be achieved without the blocked PhP. The performance of the debondable adhesive by using the sorbic ester-based cross-linked polyperoxides was improved by the addition of the blocked PhP, although hazardous isocyanate formation during the activation process may limit the practical application. Specifically, a faster decrease in the lap-shear adhesion strength by heating was accomplished. Furthermore, the same level of dismantlability was achieved in the wide range of heating temperatures and time, which is an important requirement for polyperoxides undergoing significant exothermic decomposition bringing about undesired temperature rise.

quote

GB/T 7714-2015 [1] Eriko Sato, Chisato Omori, Michihiro Yuri, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00422.
MLA [1] Eriko Sato, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00422.
APA [1] Eriko Sato, Chisato Omori, Michihiro Yuri, Yuta Koda, & Hideo Horibe. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00422
IEEE [1] Eriko Sato, Chisato Omori, Michihiro Yuri, Yuta Koda, and Hideo Horibe, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00422. keywords: {degradable polymer;network polymer;polyperoxide;redox reaction;deprotection;thermal latency;dismantlable adhesive}