Cellulose Nanofibril/Talc Composite Films with Excellent Barrier Properties by Alternate Hierarchical Method AITranslate
Abstract AITranslate
Cellulose-based materials offer a promising alternative to non-biodegradable plastics in packaging applications due to their biodegradability and abundance. However, the fabrication of cellulose-based materials with a facile method and high barrier properties remains an ongoing challenge. To solve this problem, two-dimensional (2D) platelets with large specific surface areas are employed to improve the barrier properties. Herein, an alternate hierarchical structure was constructed by incorporating talc platelets into a cellulose nanofibril (CNF) matrix through a one-step vacuum filtration process. The fabricated CNF–talc composite films showed significantly improved oxygen and water vapor barrier properties in the preservation test. This composite film also possessed excellent UV blocking with high thermal stability, which meets the requirements of various outdoor applications. More importantly, the prepared CNF-based films had excellent biodegradability compared with conventional plastic films. This ecofriendly and cost-efficient fabrication method of CNF–talc films, in which inorganic nanosheets and organic layers are alternately intercalated, can further inspire the design and development of packaging materials with high barrier properties.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01643
Chinese Library Classification Number:
Citation Information:
Cellulose-based materials offer a promising alternative to non-biodegradable plastics in packaging applications due to their biodegradability and abundance. However, the fabrication of cellulose-based materials with a facile method and high barrier properties remains an ongoing challenge. To solve this problem, two-dimensional (2D) platelets with large specific surface areas are employed to improve the barrier properties. Herein, an alternate hierarchical structure was constructed by incorporating talc platelets into a cellulose nanofibril (CNF) matrix through a one-step vacuum filtration process. The fabricated CNF–talc composite films showed significantly improved oxygen and water vapor barrier properties in the preservation test. This composite film also possessed excellent UV blocking with high thermal stability, which meets the requirements of various outdoor applications. More importantly, the prepared CNF-based films had excellent biodegradability compared with conventional plastic films. This ecofriendly and cost-efficient fabrication method of CNF–talc films, in which inorganic nanosheets and organic layers are alternately intercalated, can further inspire the design and development of packaging materials with high barrier properties.
quote
| GB/T 7714-2015 | [1] Gengye Lin, Jun Xu, Minghong Wu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01643. |
| MLA | [1] Gengye Lin, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01643. |
| APA | [1] Gengye Lin, Jun Xu, Minghong Wu, Qianqian Sun, Shiyun Zhu, Bin Wang, & Wei Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01643 |
| IEEE | [1] Gengye Lin, Jun Xu, Minghong Wu, Qianqian Sun, Shiyun Zhu, Bin Wang, and Wei Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01643. keywords: {alternate hierarchical structure;barrier properties;ecofriendly;talc platelets;cellulose nanofibrils} |