Effect of Temperature on Selective Reduction of Fe and Nb in Carbon-matched Pellets of Niobium Concentrate AITranslate

Key Laboratory of Integrated Exploitation of Bayan-Obo Multi-Metal Resources;Key Laboratory of Integrated Exploitation of Bayan-Obo Multi-Metal Resources;Key Laboratory of Integrated Exploitation of Bayan-Obo Multi-Metal Resources;Key Laboratory of Integrated Exploitation of Bayan-Obo Multi-Metal Resources
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The feasibility was explored of selective reduction of niobium concentrate,and the effect was studied of temperature on the selective reduction of iron and niobium in carbon-matched pellets of niobium concentrate,as well as the occurrence states of iron-bearing phases and niobium-bearing phases in the reduction process.The results show that as the reduction temperature of niobium concentrate increases,the reduction metallization rate of iron minerals also increases.When the reaction temperature is 1050℃,the hematite in the niobium concentrate can be effectively reduced to metallic iron.However,there is still a certain amount of iron olivine in the reduction product,resulting in a reduction metallization rate of only 76.16%.CO content of the reducing atmosphere inside carbon-matched pellets of niobium concentrate is around 72.4%,which is significantly lower than 99%,the theoretical equilibrium value of carbon gasification.During the reduction process,niobium minerals remain in an oxygen-bearing state,which is beneficial to the subsequent separation of iron and niobium.The technological expectation of selective reduction of iron and niobium in niobium concentrate can be realized.

KeyWords AITranslate

niobium concentrate carbon-matched pellet carbothermal reduction iron and niobium separation metallization rate phase transition CO partial pressure

1陈宏.直接还原法在铌提取上的应用[J].宝钢技术,1998(5):26-29. 被引量:12

2宁晓宇,薛庆国,王广,丁闪,佘雪峰,王静松.含碳球团直接还原熔分机理[J].北京科技大学学报,2014,36(9):1166-1173. 被引量:6

3李翔,刘勇,李光辉,刘牡丹,刘珍珍.从低品位稀土铌铁粗精矿中分离回收铁和稀有金属的新工艺[J].材料研究与应用,2014,8(1):67-72. 被引量:7

4Xiao-jiao FU,Jia-qi ZHAO,Shuang-yin CHEN,Zheng-gen LIU,Tong-lai GUO,Man-sheng CHU.Comprehensive Utilization of Ludwigite Ore Based on Metallizing Reduction and Magnetic Separation[J].钢铁研究学报:英文版,2015,0(8):672-680. 被引量:2

5潘刚,王子杰,李义科,赵增武,丁胜利,武文斐.白云鄂博矿含碳球团直接还原过程的实验及数值模拟研究[J].烧结球团,2016,41(4):24-28. 被引量:1

6刘玉宝,王静松,张先恒,赵二雄,薛庆国,佘雪峰.包头含铌铁精矿选择性还原试验[J].钢铁,2016,51(5):22-27. 被引量:7

7丁胜利,赵增武,盖少群,康毅,乔国平,韩春良.白云鄂博铁精矿配碳球团还原特性研究[J].钢铁钒钛,2018,0(2):115-120. 被引量:1

8张广庆,黄务涤,陈冰,赵玉华.包头铁水固氧提铌的工艺[J].北京科技大学学报,1993,15(5):453-459. 被引量:1

9曹明明,张建良,邢相栋,王春龙,白亚楠,文永才.钒钛磁铁矿含碳球团的还原机制[J].钢铁,2012,47(8):5-12. 被引量:8

10储满生,王兆才,柳政根,吕继平.热压含碳球团自还原过程限制性环节的实验研究[J].过程工程学报,2010,10(1):121-126. 被引量:10

1张芳,聂东娥,霍明鹤,王艺慈,罗果萍.钾长石对CO还原铁氧化物过程还原膨胀性的影响[J].钢铁研究学报,2020,32(11):958-967. 被引量:2

2屈少杰,李成军,汤志强,李斌东,熊刚.TiZr3V6合金微观组织及吸氢物相转变[J].材料导报,2020,34(S02):360-361.

3张可召,何超威,戚宋歌,包晔峰,牛红志,严春妍.热处理对激光焊接β钛合金组织及性能的影响[J].电焊机,2020,50(12):59-64. 被引量:4

4易天龙,吴华杰,孙悦,刘颖辉.AOD精炼双相不锈钢2101去碳保铬研究[J].工程科学学报,2020,42(S01):89-94. 被引量:2

5于浩博,姜鑫,高强健,王学斌,梁栋,沈峰满.红土镍矿高料层碳热还原试验[J].钢铁,2020,55(11):10-15. 被引量:2

6秦明晓.钒渣钙化焙烧过程物相转变机理研究[J].辽宁化工,2020,49(11):1366-1367.

7王小华,陈春华,朱鹏,赵鹏,俞胜捷,陈敏.600 MW机组锅炉前屏过热器吸热偏差诊断及优化调整[J].锅炉技术,2020,51(6):18-22. 被引量:4

8陈博文,王敬晓,姜佑霖,周海军,廖春景,张翔宇,阚艳梅,倪德伟.基于离心纺丝技术制备稳定的碳化锆纤维[J].无机材料学报,2020,35(12):1385-1390. 被引量:1

9谷卓训,林月,陈雁.广西马山县加方村壮族“打扁担”的调查研究[J].体育风尚,2021(1):115-116.

10万军营,陈铁军,周仙霖,罗艳红,陆启财,胡钺.高锰铁矿强化赤泥直接还原试验研究[J].烧结球团,2020,45(6):10-15. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]

Citation Information:

The feasibility was explored of selective reduction of niobium concentrate,and the effect was studied of temperature on the selective reduction of iron and niobium in carbon-matched pellets of niobium concentrate,as well as the occurrence states of iron-bearing phases and niobium-bearing phases in the reduction process.The results show that as the reduction temperature of niobium concentrate increases,the reduction metallization rate of iron minerals also increases.When the reaction temperature is 1050℃,the hematite in the niobium concentrate can be effectively reduced to metallic iron.However,there is still a certain amount of iron olivine in the reduction product,resulting in a reduction metallization rate of only 76.16%.CO content of the reducing atmosphere inside carbon-matched pellets of niobium concentrate is around 72.4%,which is significantly lower than 99%,the theoretical equilibrium value of carbon gasification.During the reduction process,niobium minerals remain in an oxygen-bearing state,which is beneficial to the subsequent separation of iron and niobium.The technological expectation of selective reduction of iron and niobium in niobium concentrate can be realized.

quote

GB/T 7714-2015 [1] ZHANG Fu-shun, ZHAO Zeng-wu, LI Yan, et al. Effect of Temperature on Selective Reduction of Fe and Nb in Carbon-matched Pellets of Niobium Concentrate[J]. Rare Metals and Cemented Carbides, 2020(6): 14-19.
MLA [1] ZHANG Fu-shun, et al., "Effect of Temperature on Selective Reduction of Fe and Nb in Carbon-matched Pellets of Niobium Concentrate." Rare Metals and Cemented Carbides, no. 6, 2020, pp. 14-19.
APA [1] ZHANG Fu-shun, ZHAO Zeng-wu, LI Yan, & DU Zhi-yu. (2020). Effect of Temperature on Selective Reduction of Fe and Nb in Carbon-matched Pellets of Niobium Concentrate. Rare Metals and Cemented Carbides(6), 14-19.
IEEE [1] ZHANG Fu-shun, ZHAO Zeng-wu, LI Yan, and DU Zhi-yu, "Effect of Temperature on Selective Reduction of Fe and Nb in Carbon-matched Pellets of Niobium Concentrate," Rare Metals and Cemented Carbides, no. 6, pp. 14-19, 2020. keywords: {niobium concentrate;carbon-matched pellet;carbothermal reduction;iron and niobium separation;metallization rate;phase transition;CO partial pressure}