Progress in Hydrometallurgy Process of Tungsten AITranslate
Abstract AITranslate
The theoretical breakthrough of the mainstream technology in hydrometallurgy of tungsten and its existing problems in engineering and technology are summarized.The factors of China's tungsten re sources, technology and environmental protection policies are also comprehensively analyzed. A new tung sten metallurgy technology, sulfuric-phosphoric mixed acid decomposition technology of scheelite, developed by Central South University is introduced. The new technology can solve these problems in the cur rent tungsten hydrometallurgy. It provides a new way for promoting the healthy development of tungsten industry in China under the new situation.
KeyWords AITranslate
1何利华,赵中伟,杨金洪.新一代绿色钨冶金工艺——白钨硫磷混酸协同分解技术[J].中国钨业,2017,32(3):49-53. 被引量:19
2宁华.苏打压煮钨矿工艺及其发展[J].稀有金属与硬质合金,1996,24(4):44-48. 被引量:4
3赵中伟,杨金洪.关于钨矿苏打压煮工艺几个理论问题的讨论[J].稀有金属与硬质合金,2002,30(2):1-3. 被引量:1
4肖连生,张启修,张贵清,龚柏藩,王金明.膜电解法回收钨酸钠溶液中游离碱工业试验研究[J].膜科学与技术,2001,21(2):14-16. 被引量:12
5肖连生,王玮,张启修,龚柏藩,曹家树.钨酸钠溶液膜电解体系的阳极选择研究[J].膜科学与技术,2000,20(6):16-19. 被引量:2
6李洪桂,刘茂盛,孙培梅,李运姣,苏鹏抟.适应钨资源形势的变化开拓钨冶金的新工艺[J].中国钨业,1999,14(5):136-139. 被引量:11
7刘茂盛.碱法热球磨分解钨矿物专利技术综合介绍[J].中国钨业,1995,0(2):26-29. 被引量:1
8李洪桂,刘茂盛,孙培梅,李运姣,苏鹏抟.白钨精矿与黑白钨混合矿碱分解的方法与设备[J].中国科学基金,1997,11(3):210-212. 被引量:6
9李洪桂,孙培梅,刘茂盛,李运姣,刘志立.Na_2WO_4在NaOH-H_2O系中的溶解度研究[J].中南矿冶学院学报,1991,22(6):644-649. 被引量:5
10彭泽田.高钙黑钨精矿的低压高碱浸取[J].中国钨业,1996,0(10):16-19. 被引量:3
1薛祥,张新英,杨亮.磷酸钠-氢氧化钠浸出氟化钙动力学研究[J].有色金属科学与工程,2021,12(1):8-12. 被引量:2
1崔梦倩,杜婷婷,刘建军,罗英涛,孙丽贞.铝工业含氟溶液实验研究[J].世界有色金属,2022(21):196-198.
2李朝阳,杨亮,张新英,龚丹丹,万林生.氯化镧从钨酸钠溶液中沉淀除氟新工艺研究[J].稀有金属与硬质合金,2023,51(2):8-12.
1汪炜.低品位白钨矿选矿技术的研究发展[J].中国金属通报,2018(10):224-224. 被引量:4
2唐凤翔,郑允权,陈海军,黄剑东.基于成果导向教育的制药工艺学教学改革探索[J].药学教育,2019,35(3):45-50. 被引量:7
3李天宇.江西钨矿床主要成因类型及找矿潜力分析[J].世界有色金属,2019,0(7):266-267.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
The theoretical breakthrough of the mainstream technology in hydrometallurgy of tungsten and its existing problems in engineering and technology are summarized.The factors of China's tungsten re sources, technology and environmental protection policies are also comprehensively analyzed. A new tung sten metallurgy technology, sulfuric-phosphoric mixed acid decomposition technology of scheelite, developed by Central South University is introduced. The new technology can solve these problems in the cur rent tungsten hydrometallurgy. It provides a new way for promoting the healthy development of tungsten industry in China under the new situation.
quote
| GB/T 7714-2015 | [1] REN Hui-chuan, TANG Zhong-yang, LIU Xu-heng. Progress in Hydrometallurgy Process of Tungsten[J]. Rare Metals and Cemented Carbides, 2019(3): 1-8. |
| MLA | [1] REN Hui-chuan, et al., "Progress in Hydrometallurgy Process of Tungsten." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 1-8. |
| APA | [1] REN Hui-chuan, TANG Zhong-yang, & LIU Xu-heng. (2019). Progress in Hydrometallurgy Process of Tungsten. Rare Metals and Cemented Carbides(3), 1-8. |
| IEEE | [1] REN Hui-chuan, TANG Zhong-yang, and LIU Xu-heng, "Progress in Hydrometallurgy Process of Tungsten," Rare Metals and Cemented Carbides, no. 3, pp. 1-8, 2019. keywords: {tungsten hydrometallurgy;theoretical breakthrough;engineering technology;environmental pro tection policy;sulfuric-phosphoric mixed acid} |