Application of Resin-in-Pulp Processin Molybdenum Metallurgy AITranslate
Abstract AITranslate
Description is made of the history and prcgress of resin - in - pulp(RIP)process development. In view of the complexity of low - grade and difficult molybdenite and characteristics of metallurgical process development, the future application and development tendency application of resin - in - pulp process for molybdenum metallurgy is prospected. The actual applications showed that the use of RIP process during leaching for treatment of nonstandard high - carbon molybdenite concentrates resulted in 〉 99 % adsorption and stripping rates of Mo in resin and the Mo recovery 92 % ~ 95 %.
KeyWords AITranslate
1赖声伟.阿希金矿提金工艺流程评述[J].黄金,1994,15(7):34-38. 被引量:3
2Л.波罗托娃,赖声伟,李长根.湿法提金中的离子交换工艺[J].国外金属矿选矿,2001,38(3):28-31. 被引量:4
3华金仓.国内外树脂矿浆法提金工业的现状及发展前景[J].新疆有色金属,1999,22(1):35-38. 被引量:5
4李洪桂.离子交换技术在钼冶金中的应用[J].中国钼业,1994,18(3):1-7. 被引量:16
5刘铭禹.论述俄罗斯等国家采用树脂矿浆法提金工业生产[J].黄金,1995,16(4):39-43. 被引量:3
6易国新.树脂矿浆法的消化实施及应用[J].新疆有色金属,1999,22(2):17-19. 被引量:3
7王云楚,饶邦兴.树脂矿浆法在安徽灌口铁帽型金矿的应用[J].金属矿山,1997(11):21-24. 被引量:4
8Carmen P G,et al.Gold recovery with ion exchange used resins[J].Separation and Purification Technology,2001,24(1):35.
9Zhang Hong-guang,et al.The recovery of gold from ammoniacal thiosulfate solutions containing copper using ion exchange resin columns[J].Hydrometallurgy,2004,72 (2) :225.
10Balliett H,et al.Production of pure molybdenum oxide from low-grade molybdenite concentrates[P].US Pat 20030086864,2003-05-08.
1杨大锦.2005年云南冶金年评[J].云南冶金,2006,35(2):28-37.
2张文朴.我国钼资源中稀贵金属的综合利用与再生回收研发进展[J].稀有金属与硬质合金,2007,35(2):35-39. 被引量:5
3张文朴.我国钼资源及稀贵金属的回收与综合利用[J].资源再生,2007(11):26-29. 被引量:2
1徐志昌,张萍.乏催化剂综合回收工艺现状与展望[J].中国钼业,2011,35(6):21-37.
2曹占芳,钟宏,刘广义,王帅.我国矿产资源的特点及其加工技术与专业教学现状[J].稀有金属与硬质合金,2012,40(5):18-22. 被引量:2
3邓攀,曾颜亮,王坤,刘德刚.钼资源的回收技术现状及发展[J].山西冶金,2012,35(5):1-3. 被引量:5
4蒲敬文,鲁兴武,李冠军,张析.钼精矿制取四钼酸铵实验研究[J].甘肃冶金,2013,35(1):7-9. 被引量:7
5张亨.可再生钼资源回收研究进展[J].中国钼业,2014,38(4):1-4. 被引量:1
6张亨.钼酸钠的生产研究进展[J].中国钼业,2014,38(6):1-6. 被引量:2
7甘敏,范晓慧,张麟,姜涛,邱冠周,王勇,邓琼,陈许玲.低品位钼精矿氧化焙烧过程的反应行为[J].中国有色金属学报,2014,24(12):3115-3122. 被引量:20
1俞宗衡.高硅低品位钼矿焙烧过程的研究[J].江苏冶金,1995,23(1):22-24.
2周金泉.国外小型钢厂电炉装备发展特点及对改造我国电炉装备的见解[J].重型机械,1989(6):4-11. 被引量:1
3王保士.国外非标准废合金钢的加工[J].废钢铁,1990(1):42-46.
4常见非标准单位符号示例[J].山东冶金,2009,31(4):63-63.
5常见非标准单位符号示例[J].山东冶金,2009,31(5):105-105.
6B.A.安德罗诺夫,傅以文.非标准工艺条件下的高炉热工[J].梅山科技,1994(3):59-61.
7蔡创开.碱性介质氧压煮-萃取法回收某非标准钼精矿中的钼[J].矿产综合利用,2010(4):19-23. 被引量:5
8谢铿,王海北,张邦胜.低品位钼矿及钼二次资源加压浸出工艺的研究进展[J].稀有金属与硬质合金,2014,42(3):23-27. 被引量:3
9任鸿国.浅论炼铜转炉辅助设备[J].有色冶金设计与研究,1997,18(2):56-59.
10俞宗衡.高硅低品位硫化钼矿氧化脱硫[J].中国钼业,1995,19(4):7-11.
Basic Information:
DOI:
Chinese Library Classification Number:TF803.2[冶金工程—有色金属冶金]
Citation Information:
Description is made of the history and prcgress of resin - in - pulp(RIP)process development. In view of the complexity of low - grade and difficult molybdenite and characteristics of metallurgical process development, the future application and development tendency application of resin - in - pulp process for molybdenum metallurgy is prospected. The actual applications showed that the use of RIP process during leaching for treatment of nonstandard high - carbon molybdenite concentrates resulted in 〉 99 % adsorption and stripping rates of Mo in resin and the Mo recovery 92 % ~ 95 %.
quote
| GB/T 7714-2015 | [1] FU Jian-gang, XIONG Qing-feng, LIU Ling-bo, et al. Application of Resin-in-Pulp Processin Molybdenum Metallurgy[J]. Rare Metals and Cemented Carbides, 2005(3): 26-28. |
| MLA | [1] FU Jian-gang, et al., "Application of Resin-in-Pulp Processin Molybdenum Metallurgy." Rare Metals and Cemented Carbides, no. 3, 2005, pp. 26-28. |
| APA | [1] FU Jian-gang, XIONG Qing-feng, LIU Ling-bo, & BO Xiang-ming. (2005). Application of Resin-in-Pulp Processin Molybdenum Metallurgy. Rare Metals and Cemented Carbides(3), 26-28. |
| IEEE | [1] FU Jian-gang, XIONG Qing-feng, LIU Ling-bo, and BO Xiang-ming, "Application of Resin-in-Pulp Processin Molybdenum Metallurgy," Rare Metals and Cemented Carbides, no. 3, pp. 26-28, 2005. keywords: {resin - in - pulp process (RIP);leaching;low - grade molybdenite;molybdenum extraction process} |