Selective Purity Modulation of Semiconducting Single-Walled Carbon Nanotube Networks for High-Performance Thin-Film Transistors Selective Purity Modulation of Semiconducting Single-Walled Carbon Nanotube Networks for High-Performance Thin-Film Transistors AITranslate

Seoul National University; Seoul National University; Seoul National University; Korea Institute of Science and Technology; Seoul National University; Korea Institute of Science and Technology; Seoul National University; Seoul National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Single-walled carbon nanotube (SWCNT) random networks have become strong candidates for next-generation electronics due to their exceptional mechanical, electrical, and optical properties. However, metallic nanotubes in networks generally incur a trade-off between the charge carrier mobility and on/off ratio, limiting the performance of SWCNT-based devices. Therefore, various methods to increase the purity of semiconducting nanotubes in entire random networks have been reported, but this direction has faced other issues, such as nanotube shortening, higher cost, and higher energy. Here, we introduce SWCNT random network-based thin-film transistors (SWCNT TFTs) with a varying purity profile of semiconducting SWCNTs across the channel, exploiting the superior mobility of metallic SWCNTs by partially tuning the semiconducting SWCNT purity and developing a novel perspective on metallic nanotubes in semiconductor channels. Based on the high-precision drop-on-demand capability of inkjet printing and various concentrations of semiconducting SWCNT ink, we form selectively patterned channel regions with different semiconducting SWCNT purities. The metallic nanotube-dominant region drastically increases the carrier density with a minimized Schottky barrier, while high-purity semiconducting regions at the channel boundaries effectively block off-state leakage through carrier depletion. As a result, the SWCNT TFTs with selectively patterned metallic nanotube regions show superior carrier mobility (75.50 cm2 V–1 s–1) and channel width normalized on-current (34.33 nA μm–1) without compromising the on/off ratio (1.62 × 107). To show the feasibility of our device in high-performance electronics, we demonstrate all-inkjet-printed flexible display driving circuits with two transistors that enable low-power, high-performance operation in display applications.

KeyWords AITranslate

singlewalled carbon nanotube thinfilm transistor channel purity engineering energy band engineering inkjet printingShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01685

Chinese Library Classification Number:

Citation Information:

Single-walled carbon nanotube (SWCNT) random networks have become strong candidates for next-generation electronics due to their exceptional mechanical, electrical, and optical properties. However, metallic nanotubes in networks generally incur a trade-off between the charge carrier mobility and on/off ratio, limiting the performance of SWCNT-based devices. Therefore, various methods to increase the purity of semiconducting nanotubes in entire random networks have been reported, but this direction has faced other issues, such as nanotube shortening, higher cost, and higher energy. Here, we introduce SWCNT random network-based thin-film transistors (SWCNT TFTs) with a varying purity profile of semiconducting SWCNTs across the channel, exploiting the superior mobility of metallic SWCNTs by partially tuning the semiconducting SWCNT purity and developing a novel perspective on metallic nanotubes in semiconductor channels. Based on the high-precision drop-on-demand capability of inkjet printing and various concentrations of semiconducting SWCNT ink, we form selectively patterned channel regions with different semiconducting SWCNT purities. The metallic nanotube-dominant region drastically increases the carrier density with a minimized Schottky barrier, while high-purity semiconducting regions at the channel boundaries effectively block off-state leakage through carrier depletion. As a result, the SWCNT TFTs with selectively patterned metallic nanotube regions show superior carrier mobility (75.50 cm2 V–1 s–1) and channel width normalized on-current (34.33 nA μm–1) without compromising the on/off ratio (1.62 × 107). To show the feasibility of our device in high-performance electronics, we demonstrate all-inkjet-printed flexible display driving circuits with two transistors that enable low-power, high-performance operation in display applications.

quote

GB/T 7714-2015 [1] Hayun Kim, Hyunuk Oh, Hyunjun Yoo, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01685.
MLA [1] Hayun Kim, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01685.
APA [1] Hayun Kim, Hyunuk Oh, Hyunjun Yoo, Kyungjune Cho, Takhee Lee, Seungjun Chung, Byeongmoon Lee, & Yongtaek Hong. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01685
IEEE [1] Hayun Kim, Hyunuk Oh, Hyunjun Yoo, Kyungjune Cho, Takhee Lee, Seungjun Chung, Byeongmoon Lee, and Yongtaek Hong, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01685. keywords: {singlewalled carbon nanotube thinfilm transistor channel purity engineering energy band engineering inkjet printingShow More}