Abstract AITranslate
A simple and rapid spectrophotometric method for the determination of trace cerium in alloy has been deyeloped. Cerium reactswith chlorphosphonazo-ms to form a blue complex at PH 2-3 .The complexexhibits a maximum absorption at 664urn with an apparent molar absorptivity of 4.76X 10'Lmol-loin-1.Beer's law is obeyed for 0-25pg of Ce in25ml of solution.The method bas been applied to the determination ofcerium in alloy magnesium.
KeyWords AITranslate
1杨浩义,焦焕良.DBM-偶氮胂与稀土元素在高酸度下显色反应的研究[J].冶金分析,1992,12(3):50-51. 被引量:9
2何艺,潘教麦.用间磺酸基偶氮氯膦分光光度法测定钨铈合金中的铈[J]分析试验室,1985(09).
1杨姣,凌程凤,谈技,宗俊.DBM-FsaA的合成及在热镀锌合金中微量铈分析的应用[J].化学研究与应用,2005,17(1):100-102. 被引量:1
2杨姣,谈技,宗俊.热镀锌合金中微量铈的测定——新显色剂二溴羧基偶氮氟胂光度法[J].理化检验:化学分册,2005,41(2):84-86. 被引量:3
3杨姣,凌程凤,徐峰,宗俊.新试剂二溴氟基偶氮氟胂分光光度法快速测定热镀锌合金中微量铈[J].分析试验室,2005,24(6):1-4. 被引量:3
1倪英萍,史俊霞,凌程凤,宗俊.新显色剂二溴氟基偶氮甲胂分光光度法测定热镀锌中痕量镧[J].化学试剂,2006,28(9):529-530. 被引量:4
2马冲先,吴诚.金属材料分析[J].分析试验室,2006,25(12):103-122. 被引量:8
3柳玉英,周丽.光度法测定铈的研究进展[J].理化检验:化学分册,2009,45(8):1008-1010. 被引量:5
4刘文华.稀土元素分析[J].分析试验室,2011,30(6):106-122. 被引量:12
1杨勋,宋秀兰.铝合金中残余锶的测定[J].内燃机技术,1996(2):32-34.
2Р.,ТИ,曹川保.含用大量锆,稀土及其它元素时钪的光度法测定[J].国外钢铁钒钛,1990,3(4):85-87.
3郑礼胜,许认.二苯卡巴肼萃取分光光度法测定钢中微量铜[J].冶金分析,1994,14(1):37-38. 被引量:1
4李云华.不锈钢中镍的快速分析[J].昆重科技,1995(1):21-23.
5杨定国.分光光度法测定微量铈[J].冶金分析,1990,10(3):55-56. 被引量:1
6李莉,潘傥.直接分光光度法测定钛合金中的稀土元素钕[J].冶金分析,1990,10(5):7-10. 被引量:4
7邱林友,赵尔燕.分光光度法测定铸铁中的钒[J].现代铸铁,1991(3):35-37. 被引量:2
8管廷瑛.纯钨中十九个微量杂质元素的光谱分析[J].有色金属分析通讯,1994(2):25-27.
9李建华.钢中微量钛的测定[J].特钢技术,1994(2):51-54.
10杨申彦.金属锶中杂质的光谱测定[J].稀有金属材料与工程,1991,20(5):62-65. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.22[金属学及工艺—金属材料];TG115.335[金属学及工艺—物理冶金]
Citation Information:
A simple and rapid spectrophotometric method for the determination of trace cerium in alloy has been deyeloped. Cerium reactswith chlorphosphonazo-ms to form a blue complex at PH 2-3 .The complexexhibits a maximum absorption at 664urn with an apparent molar absorptivity of 4.76X 10'Lmol-loin-1.Beer's law is obeyed for 0-25pg of Ce in25ml of solution.The method bas been applied to the determination ofcerium in alloy magnesium.
quote
| GB/T 7714-2015 | [1] LUO Chong-qing, TAN Yu-li, FAN Jian. Determination of Trace Cerium in Alloy by Spectrophotometry[J]. Rare Metals and Cemented Carbides, 1995(2): 24-27. |
| MLA | [1] LUO Chong-qing, et al., "Determination of Trace Cerium in Alloy by Spectrophotometry." Rare Metals and Cemented Carbides, no. 2, 1995, pp. 24-27. |
| APA | [1] LUO Chong-qing, TAN Yu-li, & FAN Jian. (1995). Determination of Trace Cerium in Alloy by Spectrophotometry. Rare Metals and Cemented Carbides(2), 24-27. |
| IEEE | [1] LUO Chong-qing, TAN Yu-li, and FAN Jian, "Determination of Trace Cerium in Alloy by Spectrophotometry," Rare Metals and Cemented Carbides, no. 2, pp. 24-27, 1995. keywords: {cerium;chlorphosphonazo-ms;alloy magnesium;spectrophotometry} |