daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Lysostaphin-Functionalized Waterborne Polyurethane/Polydopamine Coatings Effective against S. Aureus Biofilms AITranslate

Turkey|Sabanci University SUNUM Nanotechnology Research Center; Sabanci University; Turkey|Sabanci University SUNUM Nanotechnology Research Center; Turkey|Sabanci University Integrated Manufacturing Technologies Research and Application Center;Sabanci University SUNUM Nanotechnology Research Center
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hybrid waterborne polyurethane/polydopamine (WPU/PDA) matrix, showing the adhesive properties of PDA in its entirety, was utilized for the immobilization of lysostaphin (Lys), an important anti-staphylococcal agent, to obtain highly effective antibacterial and antibiofilm surface coatings. WPU/PDA matrix prepared by the encapsulation of WPU particles with PDA in aqueous dispersion was applied as coatings on substrates, and the facile incubation of the WPU/PDA-coated surfaces with Lys in aqueous solution resulted in WPU/PDA/Lys coatings that contained immobilized Lys on the surface. WPU/PDA/Lys coatings showed strong anti-Staphylococcus aureus activity with a 4 log reduction in the number of cells. Furthermore, WPU/PDA/Lys coatings were demonstrated to be durable without any enzyme leakage, and their antibacterial activity was preserved for at least 30 days and over multiple exposures to bacteria. WPU/PDA/Lys coatings presented significant antibiofilm activity against S. aureus with a 3.5 log reduction in the number of surface-attached bacteria. WPU/PDA/Lys coatings that are easy-to-apply to almost any surface, non-toxic, and environmentally friendly provide promising antibacterial and antibiofilm surfaces that are effective against S. aureus.

KeyWords AITranslate

waterborne polyurethane (WPU) polydopamine lysostaphin antibacterial coating antibiofilm coating
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00254

Chinese Library Classification Number:

Citation Information:

Hybrid waterborne polyurethane/polydopamine (WPU/PDA) matrix, showing the adhesive properties of PDA in its entirety, was utilized for the immobilization of lysostaphin (Lys), an important anti-staphylococcal agent, to obtain highly effective antibacterial and antibiofilm surface coatings. WPU/PDA matrix prepared by the encapsulation of WPU particles with PDA in aqueous dispersion was applied as coatings on substrates, and the facile incubation of the WPU/PDA-coated surfaces with Lys in aqueous solution resulted in WPU/PDA/Lys coatings that contained immobilized Lys on the surface. WPU/PDA/Lys coatings showed strong anti-Staphylococcus aureus activity with a 4 log reduction in the number of cells. Furthermore, WPU/PDA/Lys coatings were demonstrated to be durable without any enzyme leakage, and their antibacterial activity was preserved for at least 30 days and over multiple exposures to bacteria. WPU/PDA/Lys coatings presented significant antibiofilm activity against S. aureus with a 3.5 log reduction in the number of surface-attached bacteria. WPU/PDA/Lys coatings that are easy-to-apply to almost any surface, non-toxic, and environmentally friendly provide promising antibacterial and antibiofilm surfaces that are effective against S. aureus.

quote

GB/T 7714-2015 [1] Buket Alkan Taş, Ekin Berksun, Cüneyt Erdinç Taş, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00254.
MLA [1] Buket Alkan Taş, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00254.
APA [1] Buket Alkan Taş, Ekin Berksun, Cüneyt Erdinç Taş, Serkan Ünal, & Hayriye Ünal. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00254