Abstract AITranslate

The dielectric spectra of the poly(thiourethane) network, HDI-S3, have been analyzed to know the nature and the cooperativity of each of the six dielectric processes observed. At low temperatures, γ1, γ2, and β dielectric relaxations were attributed to noncooperative local motions in the glassy state, in which apparent activation energies are 30, 36, and 60 kJ·mol–1, respectively. At higher temperatures, three dielectric relaxations are observed (αTg, α*, ρ). The αTg relaxation is attributed to the glass transition, and it is overlapped with the α* relaxation. The molecular origin of α* relaxation is associated with the bond exchange reaction. Finally, the ρ relaxation is ascribed to the heterogeneity of the sample although its origin is uncertain. The DC conductivity (σDC) is found to be an appropriate variable to analyze the bond exchange reaction. Accordingly, the HDI-S3 has a molecular exchange mechanism of dissociative nature.

KeyWords AITranslate

covalent adaptable networks broadband dielectric spectroscopy dielectric spectra poly(thiourethane) thermosets charge Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01543

Chinese Library Classification Number:

Citation Information:

The dielectric spectra of the poly(thiourethane) network, HDI-S3, have been analyzed to know the nature and the cooperativity of each of the six dielectric processes observed. At low temperatures, γ1, γ2, and β dielectric relaxations were attributed to noncooperative local motions in the glassy state, in which apparent activation energies are 30, 36, and 60 kJ·mol–1, respectively. At higher temperatures, three dielectric relaxations are observed (αTg, α*, ρ). The αTg relaxation is attributed to the glass transition, and it is overlapped with the α* relaxation. The molecular origin of α* relaxation is associated with the bond exchange reaction. Finally, the ρ relaxation is ascribed to the heterogeneity of the sample although its origin is uncertain. The DC conductivity (σDC) is found to be an appropriate variable to analyze the bond exchange reaction. Accordingly, the HDI-S3 has a molecular exchange mechanism of dissociative nature.

quote

GB/T 7714-2015 [1] B. PascualJose, S. De la Flor, A. Serra, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01543.
MLA [1] B. PascualJose, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01543.
APA [1] B. PascualJose, S. De la Flor, A. Serra, & A. RibesGreus. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01543
IEEE [1] B. PascualJose, S. De la Flor, A. Serra, and A. RibesGreus, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01543. keywords: {covalent adaptable networks;broadband dielectric spectroscopy;dielectric spectra;poly(thiourethane);thermosets;charge;Show More}