Effect of Boiling Pretreatment on Physicochemical and Transport Properties of Perfluorosulfonic Acid Membrane AITranslate
Abstract AITranslate
An in-depth understanding of pretreatment effects on a perfluorosulfonic acid membrane is essential for its application to vanadium redox flow batteries (VRFBs). The physicochemical properties and transport properties of perfluorosulfonic acid membranes (PFSA) can be modified and controlled by conditioning treatments. This work investigates the effects of boiling pretreatment on the water uptake, acid uptake, membrane density, and conductivity of 3M PFSA membranes when they are in contact with H2SO4 or VOSO4/H2SO4 electrolytes. Increased water and acid uptake and much higher membrane conductivity are outcomes of the boiling pretreatment. This is mainly attributed to the pretreatment-induced morphology change, which includes a higher normalized swelling volume and a larger number of continuous water channels. The reduction of the Donnan potential for boiled membrane contributes to a higher uptake and faster proton transport but also inevitably leads to a much higher vanadium permeability. The trade-off between membrane conductance and vanadium transport across the membrane is crucial and primarily driven by the propensity to absorb various solution components, as well as their intrinsic mobility. These findings shed light on addressing relationships among physicochemical properties, transport behavior, membrane morphology, and the pretreatment effects, all of which are crucial to the performance of PFSA membranes when applied in vanadium redox flow batteries.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01772
Chinese Library Classification Number:
Citation Information:
An in-depth understanding of pretreatment effects on a perfluorosulfonic acid membrane is essential for its application to vanadium redox flow batteries (VRFBs). The physicochemical properties and transport properties of perfluorosulfonic acid membranes (PFSA) can be modified and controlled by conditioning treatments. This work investigates the effects of boiling pretreatment on the water uptake, acid uptake, membrane density, and conductivity of 3M PFSA membranes when they are in contact with H2SO4 or VOSO4/H2SO4 electrolytes. Increased water and acid uptake and much higher membrane conductivity are outcomes of the boiling pretreatment. This is mainly attributed to the pretreatment-induced morphology change, which includes a higher normalized swelling volume and a larger number of continuous water channels. The reduction of the Donnan potential for boiled membrane contributes to a higher uptake and faster proton transport but also inevitably leads to a much higher vanadium permeability. The trade-off between membrane conductance and vanadium transport across the membrane is crucial and primarily driven by the propensity to absorb various solution components, as well as their intrinsic mobility. These findings shed light on addressing relationships among physicochemical properties, transport behavior, membrane morphology, and the pretreatment effects, all of which are crucial to the performance of PFSA membranes when applied in vanadium redox flow batteries.
quote
| GB/T 7714-2015 | [1] Jing Peng, Xicai Fan, Gabriel A. Goenaga, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01772. |
| MLA | [1] Jing Peng, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01772. |
| APA | [1] Jing Peng, Xicai Fan, Gabriel A. Goenaga, Catherine M. Weiss, Christopher Andrew Neal, Nelly Cantillo, & Thomas A. Zawodzinski, Jr.. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01772 |
| IEEE | [1] Jing Peng, Xicai Fan, Gabriel A. Goenaga, Catherine M. Weiss, Christopher Andrew Neal, Nelly Cantillo, and Thomas A. Zawodzinski, Jr., ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01772. keywords: {perfluorosulfonic acid membrane;pretreatment;conductivity;permeability;Donnan potential} |