Potassium poly(heptazine imide) (K-PHI) is a two-dimensional carbon nitride polymer that has recently attracted attention as a visible-light-driven photocatalyst. We developed a solid material that does not require a liquid electrolyte as a composite of K-PHI with an ionic liquid or insulating polymer matrix. The obtained K-PHI composites retained some of the unique optoelectronic properties of K-PHI and were in a semisolid state that could be easily shaped in a warm state. Simple devices using these K-PHI composites exhibited photoconductivity by the ionic conduction of potassium cations activated by white light irradiation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01457
Chinese Library Classification Number:
Citation Information:
Potassium poly(heptazine imide) (K-PHI) is a two-dimensional carbon nitride polymer that has recently attracted attention as a visible-light-driven photocatalyst. We developed a solid material that does not require a liquid electrolyte as a composite of K-PHI with an ionic liquid or insulating polymer matrix. The obtained K-PHI composites retained some of the unique optoelectronic properties of K-PHI and were in a semisolid state that could be easily shaped in a warm state. Simple devices using these K-PHI composites exhibited photoconductivity by the ionic conduction of potassium cations activated by white light irradiation.
quote
| GB/T 7714-2015 | [1] Miyu Nakamichi, Mai Hattori, Goichiro Seo, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01457. |
| MLA | [1] Miyu Nakamichi, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01457. |
| APA | [1] Miyu Nakamichi, Mai Hattori, Goichiro Seo, Ryosuke Ohnuki, Shinya Yoshioka, & Kaname Kanai. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01457 |
| IEEE | [1] Miyu Nakamichi, Mai Hattori, Goichiro Seo, Ryosuke Ohnuki, Shinya Yoshioka, and Kaname Kanai, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01457. keywords: {potassium poly(heptazine imide) carbon nitride polymer photochromism persistent photoconductivity dark photocatalysis} |