Strategies to Enhance Light Emission from Two-Dimensional Perovskite Light-Emitting Diodes: Challenges and Future Opportunities Strategies to Enhance Light Emission from Two-Dimensional Perovskite Light-Emitting Diodes: Challenges and Future Opportunities AITranslate

Indian Institute of Technology Roorkee; Indian Institute of Technology Roorkee
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional (2D) metal halide perovskites have paved a technological renaissance in light-emitting diode (LED) technology. These 2D perovskites possess tunable photophysical properties, including higher exciton binding energies, multiple quantum well structures, natural cascaded energy funneling, and band gap versatility, which render them an outstanding candidate for future LED development. However, there are still some challenges that exist in the field for developing perovskite-based commercial display devices, which include phase impurity in 2D perovskites, their inefficient energy funneling, the high density of surface defect states, and imbalance charge injection. Numerous efforts such as phase engineering, surface passivation, and interface modulation have been demonstrated to address these challenges and to improve light emission from these perovskite-based LEDs (PeLEDs). Here, we provide a detailed analysis of existing challenges in PeLEDs from a fundamental perspective and discuss different strategies adopted to address these challenges. Finally, we discuss a detailed roadmap for the development of future high-performance commercial PeLEDs.

KeyWords AITranslate

twodimensional perovskite lightemitting diodes phase engineering auger recombination surface passivation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01142

Chinese Library Classification Number:

Citation Information:

Two-dimensional (2D) metal halide perovskites have paved a technological renaissance in light-emitting diode (LED) technology. These 2D perovskites possess tunable photophysical properties, including higher exciton binding energies, multiple quantum well structures, natural cascaded energy funneling, and band gap versatility, which render them an outstanding candidate for future LED development. However, there are still some challenges that exist in the field for developing perovskite-based commercial display devices, which include phase impurity in 2D perovskites, their inefficient energy funneling, the high density of surface defect states, and imbalance charge injection. Numerous efforts such as phase engineering, surface passivation, and interface modulation have been demonstrated to address these challenges and to improve light emission from these perovskite-based LEDs (PeLEDs). Here, we provide a detailed analysis of existing challenges in PeLEDs from a fundamental perspective and discuss different strategies adopted to address these challenges. Finally, we discuss a detailed roadmap for the development of future high-performance commercial PeLEDs.

quote

GB/T 7714-2015 [1] Yukta, Soumitra Satapathi. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01142.
MLA [1] Yukta, and Soumitra Satapathi. ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01142.
APA [1] Yukta, & Soumitra Satapathi. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01142
IEEE [1] Yukta and Soumitra Satapathi, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01142. keywords: {twodimensional perovskite lightemitting diodes phase engineering auger recombination surface passivation}