Process Study of Fe,Ca and Mg Removal and Deep Impurity Removal with P204 from Low-concentration Cobalt Solution AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;Henan University of Science and Technology Nonferrous Metal Metallurgy Research Institute;Luoyang Luohua Kiln Industry Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The pH condition of Fe, Ca and Mg removal from low-concentration coibalt solution and the process of impurity removal by P204 extraction were studied. The results form the preliminary iron removal experiment show that the process of iron removal with sodium jarosite and a pH value of 3.0-4.0 has a good effect of more than 99% iron removal rate. Using the process together with sodium jarosite and goethite,the iron removal rate is 95.65% and the cobalt loss rate is decreased from 21.3% to 4. 74%. The optimal pH value of the low-concentration cobalt solution to remove Ca and Mg for the above process is 3.5 4.0,and the optimal technical parameters of impurity removal by P204 extraction from orthogonal experiments are as follows, the volume fractions of P204 and petrol are 25% and 75%, respectively,the phase ra rio of oil to aqua is 1/2,and the saponification rate is 75%.

KeyWords AITranslate

low-concentration cobalt solution iron removal Ca and Mg removal impurity removal by P204 extraction

1谢福标.钴废料中有价元素综合回收的生产实践[J].矿冶,2001,10(3):61-64. 被引量:20

2肖楚民,张环华.低浓度钴溶液的除铁镁和富集钴的研究[J].广东有色金属学报,1999,9(1):42-46. 被引量:5

3苏凯洲.复杂含钴物料提取钴[J].湖南有色金属,1999,15(4):22-24. 被引量:4

4方成开,谭佩君.从钴镍废料电溶液中分离回收钴镍[J].湿法冶金,2003,22(4):169-182. 被引量:21

5周炳珍.用P204和P507脱除含钴废料中的杂质生产高纯度氯化钴[J].有色金属:冶炼部分,2002(6):16-17. 被引量:13

1黄耀林,叶富华,杜昆,朱曼密.工业硫酸铜深度除铁工艺的研究[J].材料研究与应用,2012,6(4):259-262. 被引量:2

2王林生,汪发波,文小强.P204萃取法对锂云母浸出液的除杂效果研究[J].稀有金属与硬质合金,2013,41(1):24-27. 被引量:2

3谢英惠,赵欣,袁俊生.LSC-500螯合树脂脱除钙离子的工艺研究[J].无机盐工业,2013,45(12):27-30. 被引量:5

4程来星,康立武.电镍钴渣氧化除铁的试验研究[J].矿冶工程,2014,34(2):94-96. 被引量:3

5钟斌,曾清全.钴浸出液氧化中和除铁的实验研究[J].山西冶金,2015,38(1):42-44. 被引量:1

6皮露,何克杰,罗炎,孙维义,丁桑岚,苏仕军.萃取分离电解锰阳极液中锰、镁离子试验研究[J].湿法冶金,2015,34(3):229-232. 被引量:17

7管青军,骆朋辉,郭亮,孙伟,殷志刚,邹兴.Versatic10萃取分离微生物浸出液中钙镁和低含量镍钴[J].有色金属:冶炼部分,2016(3):1-5. 被引量:3

8李凡,朱军,白苗苗,赵兴红,赵奇,朱明明,余娟.用溶剂萃取法从硫酸镍溶液中去除钙、铁[J].湿法冶金,2016,35(2):132-135. 被引量:14

9陈炎,程洁红.黄钠铁矾法氧化去除废锂电池硫酸浸出液中的铁[J].化工环保,2017,37(6):688-692. 被引量:7

10李进,许万祥,王靖坤,王治军,郭瑞.用溶剂萃取法从含镍钴合金渣酸浸液中深度除钙试验研究[J].湿法冶金,2017,36(6):489-492. 被引量:2

1蒋德敏,刘代俊,陈建钧,孔婷婷.反胶团二壬基萘磺酸萃取镁的机理研究[J].离子交换与吸附,2019,0(6):518-529.

2卢国俭,卢国敏.用富铜渣制备硫酸铜工艺优化研究[J].湿法冶金,2014,33(3):182-184. 被引量:2

3黄斐荣,廖亚龙,周娟,李冰洁.镍火法冶炼废渣中钴、镍回收的研究进展[J].化工进展,2015,34(4):1133-1138. 被引量:12

4于兴峰,刘永红,张博菲,郭丽萍,陈西文.离子交换树脂对硬度去除效果的实验研究[J].广东化工,2015,42(18):9-10. 被引量:4

5柳承辉,戴慧敏,王文军,魏文武,周萍,王策.直浸铜渣制备硫酸铜除铁工艺研究[J].湖南有色金属,2016,32(3):27-30. 被引量:1

6蒋德敏,方荣美,钱洪梅,郑文,张立志,何阳,熊蕾.溶剂萃取镁的研究进展[J].四川化工,2016,19(6):43-46. 被引量:1

7段继华,包申旭,张一敏,周嘉郁.D860树脂对V(Ⅳ)的吸附性能研究[J].有色金属:冶炼部分,2016,0(12):32-36. 被引量:6

8谢子楠,杨凤.菱锰矿浸出液中杂质离子的分步净化试验研究[J].湿法冶金,2017,36(2):123-127. 被引量:2

9张晓峰,李林艳,张覃.盐酸体系中二(2-乙基己基)次膦酸(P227)萃取铁的性能研究[J].湿法冶金,2017,36(3):203-207. 被引量:2

10王国胜,房安娜,贾南,李磊.马-丙共聚物去除碳化硼用硼酸中钙离子的研究[J].无机盐工业,2017,49(6):66-68. 被引量:1

1肖楚民,张环华.低浓度钴溶液的除铁镁和富集钴的研究[J].广东有色金属学报,1999,9(1):42-46. 被引量:5

2J.Martins,李之甫.用铁矿石和木炭混合料制取生球生产海绵铁的初步试验[J].烧结球团,1989(1):54-55.

3冶金技术[J].中国学术期刊文摘,2008,14(22):6-6.

4蔡传算,刘荣义,陈进中,夏忠让.含钴高温合金废料的综合利用[J].中国有色金属学报,1996,6(1):49-52. 被引量:22

5梁妹.从废弃炉渣中分离回收钴、镍[J].湿法冶金,2007,26(3):157-162. 被引量:13

6方成开,谭佩君.从钴镍废料电溶液中分离回收钴镍[J].湿法冶金,2003,22(4):169-182. 被引量:21

7李昌林,贾根贵,沙涛.用活化焙烧-硫酸浸出-溶剂萃取法从钴渣中提取硫酸钴的试验研究[J].湿法冶金,2009,28(1):28-31. 被引量:8

8孙明生,刘三平.湿法炼锌中β-萘酚除钴的工业应用[J].有色金属:冶炼部分,2008(2):6-9. 被引量:5

9汪永斌,贺周初,刘艳,彭爱国,庄新娟.工业硫酸锰中钙、镁深度除杂的工艺研究[J].精细化工中间体,2014,44(3):54-57. 被引量:10

10张愈祖,蔡传算.高温合金废料中铜钴的回收[J].铜业工程,2000(2):34-36. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TF111.33[冶金工程—冶金物理化学]

Citation Information:

The pH condition of Fe, Ca and Mg removal from low-concentration coibalt solution and the process of impurity removal by P204 extraction were studied. The results form the preliminary iron removal experiment show that the process of iron removal with sodium jarosite and a pH value of 3.0-4.0 has a good effect of more than 99% iron removal rate. Using the process together with sodium jarosite and goethite,the iron removal rate is 95.65% and the cobalt loss rate is decreased from 21.3% to 4. 74%. The optimal pH value of the low-concentration cobalt solution to remove Ca and Mg for the above process is 3.5 4.0,and the optimal technical parameters of impurity removal by P204 extraction from orthogonal experiments are as follows, the volume fractions of P204 and petrol are 25% and 75%, respectively,the phase ra rio of oil to aqua is 1/2,and the saponification rate is 75%.

quote

GB/T 7714-2015 [1] HU Wei, HUANG Xing-yuan, LI Xiao-li. Process Study of Fe,Ca and Mg Removal and Deep Impurity Removal with P204 from Low-concentration Cobalt Solution[J]. Rare Metals and Cemented Carbides, 2011(3): 10-12.
MLA [1] HU Wei, et al., "Process Study of Fe,Ca and Mg Removal and Deep Impurity Removal with P204 from Low-concentration Cobalt Solution." Rare Metals and Cemented Carbides, no. 3, 2011, pp. 10-12.
APA [1] HU Wei, HUANG Xing-yuan, & LI Xiao-li. (2011). Process Study of Fe,Ca and Mg Removal and Deep Impurity Removal with P204 from Low-concentration Cobalt Solution. Rare Metals and Cemented Carbides(3), 10-12.
IEEE [1] HU Wei, HUANG Xing-yuan, and LI Xiao-li, "Process Study of Fe,Ca and Mg Removal and Deep Impurity Removal with P204 from Low-concentration Cobalt Solution," Rare Metals and Cemented Carbides, no. 3, pp. 10-12, 2011. keywords: {low-concentration cobalt solution;iron removal;Ca and Mg removal;impurity removal by P204 extraction}