Research on the Genetic Characteristics of Morphology and Structure of Tungsten Oxide during Reduction AITranslate

School of Materials Science and Engineering, Nanchang University;School of Materials Science and Engineering, Nanchang University;School of Materials Science and Engineering, Nanchang University;School of Materials Science and Engineering, Nanchang University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tungsten oxides in different valence states were prepared by hydrogen reduction of yellow tung- sten at 660 ℃for different time,and their morphology and structure characteristics were observed and ana- lyzed. Nanometer W or WC powders were prepared by reducing WO3. The growth mechanism of nanome- ter powders during phase transformation was discussed. Effects of morphology and structure genetic char- acteristics of raw material powders on particle size uniformity of the products were analyzed. The selection of porous tungsten oxide powders of single-phase composition, high purity, fine and uniform particle size as the raw material is good for preparing fine and uniform nanometer W or WC powders.

KeyWords AITranslate

tungsten oxide nanometer W powder nanometer WC powder morphology and structure genetic characteristic

1Farid Akhtar, Islam S, Humail, et al. Effect of WC parti cle size on the microstructure, mechanical properties and fracture behavior of WC-(W,Ti,Ta)C-6wtCo cemen- ted carbides[J]. International Journal of Refractory Met- als Hard Materials,2007,25:405-410.

2Zhang Li,Wang Yuan-jie. Crack propagation characteris- tic and toughness of functionallygraded WC-Co cemented carbide[J]. International Journal of Refractory Metals Hard Materials, 2008,26 : 295-300.

3Fang Z Zak,Wang Xu. Sintering and mechanical proper- ties of nanocrystalline cemented tungsten earbide--A review[J]. International Journal of Refractory Metals Hard Materials, 2009,27 : 288-299.

4Michalski A, Siemiaszko D. Nanocrystalline cemented carbides sintered by the pulse plasma method[J]. Inter- national Journal of Refractory Metals Hard Materi- als, 2007,25 : 153-158.

5Mallika K, Komanduri R. Diamond coatings on cemented tungsten carbide tools by low-pressure microwave CVD[J].Wear, 1999,224 : 245-266.

6Arenas F,Arenas I B De. Infuence of VC on the micro structure and mechanical properties of WC-Co sintered cemented carbides[J]. International Journal of Refracto ry Metals ~ Hard Materials,1999,17:91-97.

7Hiroyuki Saito, Akira Iwabuchi, Tomoharu Shimizu. Effects of Co content and WC grain size on wear of WC cemented carbide[J].Wear, 2006, 261: 126-132.

8Bonache V,Salvador M D. Microstructural control of ul trafine and nanocrystalline WC-12Co-VC/Cra C2 mixture by spark plasma sintering[J].Ceramics International, 2011, 37: 1 139-1 142.

9Hwan-Cheol Kim, In-Jin Shon. One step synthesis and densification of ultra-fine WC by high-frequency induc- tion combustion[J].International Journal of Refractory Metals Hard Materials, 2006,24 : 202-209.

10Jinfeng Zhao, Troy Holland. Sparking plasma sintering of nanometric tungsten carbide[J]. International Jour- nal of Refractory Metals Hard Materials, 2009,27 130-139.

1谢中华,王文华,陈树茂,张秋和,徐绍梅,杜燕.仲钨酸铵自还原制备蓝色氧化钨工艺技术研究[J].中国钨业,2013,28(1):39-41. 被引量:8

2雷纯鹏,吴爱华,唐建成,叶楠.纳米钨粉形貌结构对碳化钨粉末性能的影响[J].稀有金属,2014,38(1):48-54. 被引量:13

3吴桐,唐建成,叶楠,卓海鸥,薛滢妤,周旭升.碳辅助氢还原制备纳米钨粉的工艺及机理[J].中国有色金属学报,2016,26(5):1027-1033. 被引量:8

4宋翰林,姜平国,刘文杰,汪正兵.氧化钨氢还原动力学的研究进展[J].有色金属科学与工程,2017,8(5):64-69. 被引量:6

5谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2

6陈杰,方奇,曾微微,齐宁.三氧化钨比表面积的影响因素研究[J].福建冶金,2022,51(3):41-43. 被引量:1

7张威,胡祖辉,徐双,余春荣,邓冲,陈亿.高比表面积黄色氧化钨制备工艺研究[J].中国钨业,2022,37(6):42-47.

1蒋涛,李军夏,刘建华,肖利,刘永.APT热分解动力学的研究[J].中国钨业,2014,29(3):29-33.

2易健宏,郭圣达,鲍瑞,张家敏,羊建高.超细晶碳化钨-钴复合粉短流程制备工艺研究[J].硬质合金,2018,35(5):305-314.

3王亚雄,董海刚.仲钨酸铵一步还原法制备钨粉的新工艺研究[J].有色金属:冶炼部分,2014(11):52-56. 被引量:4

4张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:63

5臧春城,王延忠,张以都,李金华,曾红,张德强.激光熔覆Ni60+35WC-Ni涂层的微观组织和摩擦磨损特性[J].稀有金属,2015,39(5):385-391. 被引量:12

6刘小胡,时凯华,闵召宇,杨新宇,廖军,吴翔.合金碳含量和烧结气氛对WC-6%Co超细硬质合金表面形貌及成分的影响[J].稀有金属,2015,39(9):799-806. 被引量:2

7金钟铃,林涛,邵慧萍,何新波,毕延,徐济安.球磨对制备钨钛封垫的原料粉末的影响[J].稀有金属,2016,40(7):679-686. 被引量:2

8温亚辉,李长亮,张清,张腾,淡新国,汤慧萍.粉末粒度对钨钼双金属性能影响[J].稀有金属,2016,40(11):1188-1192. 被引量:7

9黄晓星,刘祥庆,杨中元,汪礼敏,张晓峰.含油轴承用FeCu预合金粉末制备及烧结性能研究[J].稀有金属,2016,40(12):1249-1255. 被引量:3

10阳冬元,周春成.W粉球磨时间对W粉、WC粉及其制备的合金性能的影响[J].硬质合金,2016,33(5):322-328. 被引量:2

1罗骥,方哲成,郭志猛,邵慧萍.含V和Cr纳米W粉碳化热力学分析及实验[J].材料热处理学报,2011,32(2):26-29.

2雷纯鹏,刘刚,唐建成,张方.氧化钨形貌结构对纳米WC粉及其烧结性能的影响[J].稀有金属与硬质合金,2013,41(2):53-57. 被引量:1

3吴桐,唐建成,叶楠,卓海鸥,薛滢妤,周旭升.碳辅助氢还原制备纳米钨粉的工艺及机理[J].中国有色金属学报,2016,26(5):1027-1033. 被引量:8

4贾彦忠,王祥臻,胡长松,李仕超,张丽肖.菱铁矿的烧结特性[J].钢铁研究学报,2011,23(12):22-26. 被引量:2

5高海燕,曹顺华.机械合金化制备纳米晶硬质合金粉的进展[J].粉末冶金技术,2003,21(6):355-358. 被引量:6

6李铁超,王朋飞,朱立光,刘增勋,董亮.镀锡基板板坯连铸传热分析[J].铸造技术,2016,37(7):1435-1437. 被引量:1

7傅小明.纳米碳化钨的制备技术及研究现状[J].稀有金属与硬质合金,2011,39(1):57-60. 被引量:4

8罗骥,郭志猛,林涛,胡学晟.纳米WC粉氢处理脱除游离碳的研究[J].材料热处理学报,2007,28(1):38-41. 被引量:2

9周红宇.铸坯角部纵裂纹产生的原因及改进[J].河北冶金,2013(3):51-54. 被引量:5

10郭俊波.Al脱氧钢中Al_2O_3夹杂物形态控制的研究进展[J].安徽冶金,2014,0(4):19-23. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF122[冶金工程—粉末冶金]

Citation Information:

Tungsten oxides in different valence states were prepared by hydrogen reduction of yellow tung- sten at 660 ℃for different time,and their morphology and structure characteristics were observed and ana- lyzed. Nanometer W or WC powders were prepared by reducing WO3. The growth mechanism of nanome- ter powders during phase transformation was discussed. Effects of morphology and structure genetic char- acteristics of raw material powders on particle size uniformity of the products were analyzed. The selection of porous tungsten oxide powders of single-phase composition, high purity, fine and uniform particle size as the raw material is good for preparing fine and uniform nanometer W or WC powders.

quote

GB/T 7714-2015 [1] LEI Chun-peng, TANG Jian-cheng, LIU Gang, et al. Research on the Genetic Characteristics of Morphology and Structure of Tungsten Oxide during Reduction[J]. Rare Metals and Cemented Carbides, 2012(5): 1-6.
MLA [1] LEI Chun-peng, et al., "Research on the Genetic Characteristics of Morphology and Structure of Tungsten Oxide during Reduction." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 1-6.
APA [1] LEI Chun-peng, TANG Jian-cheng, LIU Gang, & LIU Yuan. (2012). Research on the Genetic Characteristics of Morphology and Structure of Tungsten Oxide during Reduction. Rare Metals and Cemented Carbides(5), 1-6.
IEEE [1] LEI Chun-peng, TANG Jian-cheng, LIU Gang, and LIU Yuan, "Research on the Genetic Characteristics of Morphology and Structure of Tungsten Oxide during Reduction," Rare Metals and Cemented Carbides, no. 5, pp. 1-6, 2012. keywords: {tungsten oxide;nanometer W powder;nanometer WC powder;morphology and structure;genetic characteristic}