Effect of Hot Extrusion and Annealing on Microstructure and Properties of Mg-Zr-(Ca/Y) Alloys AITranslate
Abstract AITranslate
The influence of hot extruding and annealing on the microstructure and properties of three Mg-Zr alloys were investigated. The results showed that significant grain refinement during hot extrusion im- proved the mechanical property of the alloy. In cast condition,damping capacity increased with higher strain amplitude. However, upon hot extrusion, the damping capacity of the alloys is lowered remarkably, weakly depended on strain amplitude. Annealing of the hot extruded alloy resulted in damping capacity increase, but it was still lower than the as-cast alloy. The mechanical properties of Mg-0.6Zr-0.3Ca and Mg-0.6Zr- 0.3Ca-0.1Y alloys were higher than that of Mg-0.6Zr alloy in different conditions, and their damping ca- pacities were similar to that of Mg-0.6Zr alloy in cast condition, yet much lower after hot extrusion and an- nealing. The change of damping capacities of three alloys at different processing conditions could be ex- plained by the dislocation model of Granato and Lücke.
KeyWords AITranslate
1戴得沛.阻尼技术的工程应用[M].北京:清华大学出版社,1991.3..
2Zhenyan Zhang,Xiaoqin Zeng.Wenjiang Ding. The influence of heat treatment on damping response of AZ91D magnesium alloy[J]. Materials Science and Engineering A, 2005, 392 : 150-155.
3Cahn R W.非铁合金的结构与性能[M].丁道云,彦鸣皋,雷廷权,等,译.北京:科学出版社,1999.
4黄良余,叶青,翟春泉,丁文江.高阻尼高强度镁合金ZMJD—1S的应用研究[J].特种铸造及有色合金,1992,12(5):15-17. 被引量:8
5Zhang J, Perez R J, I.avernia, E J. Effect of SiC and graphite particulates on the damping behavior of metal Metall Mater, 1994,42(2)
6Granato A,Lcke K. Theory of Mechanical damping dueto dislocations[J]. Journal of Applied Physics, 1956,27 (6) :583-593.
7Granato A, Lu K cke. Application of dislocation theory to internal friction phenomena at high frequencies[J].Journal of Applied Physics, 1956,27(7) :789-809.
1于文浩,李宁,颜家振,胡斌.挤压工艺对Mg-0.6Zr-0.5Y合金力学和阻尼性能的影响[J].功能材料,2011,42(B06):408-410.
2于文浩,李宁,颜家振,胡斌.固溶处理对Mg-0.6Zr-0.5Y合金力学和阻尼性能的影响[J].热加工工艺,2011,40(16):147-150. 被引量:3
1姜自莲.镁钇合金固溶处理后组织和性能的研究[J].热加工工艺,2013,42(14):151-152. 被引量:1
2朱小华,左舜贵,金明江.封装热处理对Ti_50Ni_30Cu_20形状记忆合金弛豫内耗行为的影响[J].热加工工艺,2014,43(16):162-164.
3兰江林,李云玲,钟振前.热处理和锰含量对CuZnAl合金微观组织结构和宏观性能的影响[J].冶金分析,2022,42(4):75-82.
1张佳,刘楚明,朱秀荣,周海涛.热轧及退火对Mg-Zr系阻尼合金组织和性能的影响[J].金属热处理,2006,31(8):35-39. 被引量:4
2陈先毅,王锦程,林琳,王改芳,杨根仓.Pr对Mg-0.6Zr合金组织和力学性能的影响[J].特种铸造及有色合金,2009,29(3):261-263. 被引量:3
3刘先兰,刘楚明,李慧中,张文玉,曾苏民.Er、Nd对Mg-0.6Zr合金组织和性能的影响[J].特种铸造及有色合金,2009,29(2):173-175. 被引量:7
4纪仁峰,刘楚明.高强高阻尼Mg-Zr系合金的研究(Ⅰ)——Ca/Y变质处理Mg-0.6Zr合金阻尼行为的研究[J].稀有金属与硬质合金,2007,35(3):23-27. 被引量:1
5张佳,吴炜.热轧变形对Mg-0.6Zr合金组织和力学性能的影响[J].轻合金加工技术,2013,41(9):19-22. 被引量:1
6张佳,朱红梅,吴炜.轧制变形对Mg-0.6Zr合金阻尼性能的影响[J].热加工工艺,2014,43(14):53-55. 被引量:5
7刘先兰,张文玉.Er对Mg-0.6Zr合金显微组织和力学性能的影响[J].特种铸造及有色合金,2017,37(2):124-127. 被引量:1
8张佳,吴炜,蒋彦,樊湘芳.退火温度对热轧态Mg-0.6Zr合金阻尼性能的影响[J].金属热处理,2013,38(1):67-69. 被引量:1
9陈继衡,张西玉,陈全红,吴德芬.加拉式巧车微型细长轴[J].金属加工:冷加工,2013(22):32-32. 被引量:1
10胡斌,李宁,颜家振,于文浩.微量Y对Mg-0.6Zr合金阻尼性能和力学性能的影响[J].热加工工艺,2010,39(12):43-46. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TG146.22[金属学及工艺—金属材料]
Citation Information:
The influence of hot extruding and annealing on the microstructure and properties of three Mg-Zr alloys were investigated. The results showed that significant grain refinement during hot extrusion im- proved the mechanical property of the alloy. In cast condition,damping capacity increased with higher strain amplitude. However, upon hot extrusion, the damping capacity of the alloys is lowered remarkably, weakly depended on strain amplitude. Annealing of the hot extruded alloy resulted in damping capacity increase, but it was still lower than the as-cast alloy. The mechanical properties of Mg-0.6Zr-0.3Ca and Mg-0.6Zr- 0.3Ca-0.1Y alloys were higher than that of Mg-0.6Zr alloy in different conditions, and their damping ca- pacities were similar to that of Mg-0.6Zr alloy in cast condition, yet much lower after hot extrusion and an- nealing. The change of damping capacities of three alloys at different processing conditions could be ex- plained by the dislocation model of Granato and Lücke.
quote
| GB/T 7714-2015 | [1] JI Ren-feng, LIU Chu-ming. Effect of Hot Extrusion and Annealing on Microstructure and Properties of Mg-Zr-(Ca/Y) Alloys[J]. Rare Metals and Cemented Carbides, 2007(4): 22-26. |
| MLA | [1] JI Ren-feng, and LIU Chu-ming. "Effect of Hot Extrusion and Annealing on Microstructure and Properties of Mg-Zr-(Ca/Y) Alloys." Rare Metals and Cemented Carbides, no. 4, 2007, pp. 22-26. |
| APA | [1] JI Ren-feng, & LIU Chu-ming. (2007). Effect of Hot Extrusion and Annealing on Microstructure and Properties of Mg-Zr-(Ca/Y) Alloys. Rare Metals and Cemented Carbides(4), 22-26. |
| IEEE | [1] JI Ren-feng and LIU Chu-ming, "Effect of Hot Extrusion and Annealing on Microstructure and Properties of Mg-Zr-(Ca/Y) Alloys," Rare Metals and Cemented Carbides, no. 4, pp. 22-26, 2007. keywords: {Mg-Zr series alloys;hot extrusion;annealing;mechanical property;damping capacity} |