Abstract AITranslate

The conversion of polyacrylonitrile (PAN) to carbonaceous structures is a complex but common processing step in the aerospace industry. Here, we show that this thermal stabilization process can occur based on the volumetric heating of PAN using radio frequency (RF) fields, in the 1–200 MHz range. Unlike many other polymers, neat PAN films show a surprisingly rapid RF heating response (5 °C/s at 103 MHz and 30 W power), without the need for any RF susceptor fillers. The RF response drops as the polymer oxidizes during heating and as the cyanide bond disappears to form a cyclic bond. Strangely, PAN nanofiber mats did not respond to RF fields. The measured AC conductivity and dielectric constant of fiber mats are lower (2.4 × 10–4 S/m and 3.66, respectively, at 103 MHz) compared to 1.4 × 10–2 S/m and 18.8 for PAN films. The dielectric properties are correlated with the bulk heating responses and stem from differences in morphology.

KeyWords AITranslate

polyacrylonitrile (PAN) dielectric heating carbon fibers RF heating nanofibers
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00319

Chinese Library Classification Number:

Citation Information:

The conversion of polyacrylonitrile (PAN) to carbonaceous structures is a complex but common processing step in the aerospace industry. Here, we show that this thermal stabilization process can occur based on the volumetric heating of PAN using radio frequency (RF) fields, in the 1–200 MHz range. Unlike many other polymers, neat PAN films show a surprisingly rapid RF heating response (5 °C/s at 103 MHz and 30 W power), without the need for any RF susceptor fillers. The RF response drops as the polymer oxidizes during heating and as the cyanide bond disappears to form a cyclic bond. Strangely, PAN nanofiber mats did not respond to RF fields. The measured AC conductivity and dielectric constant of fiber mats are lower (2.4 × 10–4 S/m and 3.66, respectively, at 103 MHz) compared to 1.4 × 10–2 S/m and 18.8 for PAN films. The dielectric properties are correlated with the bulk heating responses and stem from differences in morphology.

quote

GB/T 7714-2015 [1] Nutan Patil, Ju Hyun Oh, Sumit Khatri, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00319.
MLA [1] Nutan Patil, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00319.
APA [1] Nutan Patil, Ju Hyun Oh, Sumit Khatri, Mohammed A. Saed, Mohammed Naraghi, & Micah J. Green. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00319
IEEE [1] Nutan Patil, Ju Hyun Oh, Sumit Khatri, Mohammed A. Saed, Mohammed Naraghi, and Micah J. Green, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00319. keywords: {polyacrylonitrile (PAN);dielectric heating;carbon fibers;RF heating;nanofibers}