Recent Advances in Flexible Nanogenerators for Microphone and Loudspeaker Applications Recent Advances in Flexible Nanogenerators for Microphone and Loudspeaker Applications AITranslate

Haojing College of Shaanxi University of Science & Technology; Qingdao University; Zhejiang University of Technology; Qingdao University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nowadays, ferroelectret nanogenerators have been proposed as a possible alternative method for kinetic energy collection. We describe the component’s inherent features, which enable the bidirectional transfer of energy between the electrical and mechanical fields, expanding its potential application in wearable electronics beyond power production. Such electromechanical linkage gives the device dual-functional transducing features, demonstrating its application as a small, portable, and self-powered loudspeaker or microphone patch. This coupling, together with the flexibility and thin-film-like shape, gives the device these characteristics. For three alternative configurations, the sound pressure level is assessed in the spatial and frequency domains to ascertain the device’s functionality and usability. Also, dependencies of sound pressure levels (SPLs) generated by a FENG due to an AC voltage stimulus, surface area, geometric shape, and addition of layers are presented here.

KeyWords AITranslate

ferroelectret nanogenerators electrets microphones selfpowered loudspeaker triboelectric
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01053

Chinese Library Classification Number:

Citation Information:

Nowadays, ferroelectret nanogenerators have been proposed as a possible alternative method for kinetic energy collection. We describe the component’s inherent features, which enable the bidirectional transfer of energy between the electrical and mechanical fields, expanding its potential application in wearable electronics beyond power production. Such electromechanical linkage gives the device dual-functional transducing features, demonstrating its application as a small, portable, and self-powered loudspeaker or microphone patch. This coupling, together with the flexibility and thin-film-like shape, gives the device these characteristics. For three alternative configurations, the sound pressure level is assessed in the spatial and frequency domains to ascertain the device’s functionality and usability. Also, dependencies of sound pressure levels (SPLs) generated by a FENG due to an AC voltage stimulus, surface area, geometric shape, and addition of layers are presented here.

quote

GB/T 7714-2015 [1] Dongfang Yang, Longlong Zhang, Licheng Wang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01053.
MLA [1] Dongfang Yang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01053.
APA [1] Dongfang Yang, Longlong Zhang, Licheng Wang, & Kai Wang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01053
IEEE [1] Dongfang Yang, Longlong Zhang, Licheng Wang, and Kai Wang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01053. keywords: {ferroelectret nanogenerators electrets microphones selfpowered loudspeaker triboelectric}