daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Dispersion and Tribological Properties of Molybdenum Disulfide Modified by Ultrasonic and Microwave Ball Milling AITranslate

College of Materials Science and Engineering,Hunan University;College of Materials Science and Engineering,Hunan University;College of Materials Science and Engineering,Hunan University;College of Materials Science and Engineering,Hunan University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using laboratory-made ultrasonic and microwave ball milling equipment,molybdenum disulfide(MoS2)was modified by the surface modifiers of oleic acid and stearic acid,and the modified molybdenum disulfide(MMD)was obtained.MMD was introduced into the base oil to test its dispersibility and tribological properties,and then the elements of the friction surface was analyzed.The results show that compared with the simple ultrasound method commonly used at present,the molybdenum disulfide modified by ultrasonic and microwave ball milling has more stable dispersion in the base oil.Besides,in the friction process,MMD is more likely to deposit on the friction surface,and tribochemically react with the friction surface to form a more complete lubrication film,thus achieving more excellent anti-friction and anti-wear performance.

KeyWords AITranslate

molybdenum disulfide(MoS2) modification ultrasonic ball-milling microwave ball-milling dispersion stability tribological property

1马少华,杨鹏.油溶性二硫化钼纳米微粒的制备及抗磨性能[J].合成材料老化与应用,2015,44(1):52-54. 被引量:6

2郭青.二硫化钼固体润滑性能及其应用[J].精密制造与自动化,2007(3):26-29. 被引量:32

3武存喜,杨海滨,李享,刘世凯.无机类富勒烯二硫化钼的减摩抗磨特性[J].润滑与密封,2007,32(7):118-121. 被引量:10

4仇磊,陈鼎,朱莉莉,陈耀彤,王思远,冯鹏飞.氧化石墨烯作为润滑油添加剂的分散稳定性[J].材料导报,2019,33(16):2638-2643. 被引量:8

5白鸽玲,吴壮志.二硫化钼纳米球的制备及其摩擦性能研究[J].润滑与密封,2013,38(4):93-96. 被引量:17

6张哲,陈国需,李华峰,杨皛,陈力.二硫化钼和层状二硅酸钠复配体系的摩擦学性能[J].石油学报(石油加工),2015,31(1):172-177. 被引量:2

7胡坤宏,沃恒洲,韩效钊,胡献国.纳米二硫化钼制备现状与发展趋势[J].现代化工,2003,23(8):14-17. 被引量:33

8李斌,谢凤,张蒙蒙,李磊.纳米二硫化钼作为润滑油添加剂的摩擦学性能研究[J].润滑与密封,2014,39(9):91-95. 被引量:19

1杨舒程,赵增兵,杨炳琪,李岩,成兰兴.油溶性二硫化钼分散稳定性影响因素探究[J].化学工程师,2022,36(1):5-7.

2陈远菲,严德林,莫雪婷,杨梅,苏佳月,韦巧艳.甘蔗叶多糖提取工艺优化及生物活性研究[J].食品研究与开发,2022,43(19):155-165. 被引量:1

1秦令祥,丁昱婵,赵俊芳,高愿军.蛹虫草多糖提取工艺优化及其抗菌、抗氧化活性[J].食品研究与开发,2023,44(11):159-165.

1王琍,张忠铧,黄志荣,孙建安,罗蒙.油套管特殊螺纹接头抗粘扣自润滑涂层性能研究[J].钢管,2018,47(2):16-20. 被引量:6

2乐金龙,乔波,项珊红,马彩慧,马新贤.超分子纳米银凝胶的制备[J].广州化工,2020,48(24):34-35.

3曲铭海,杨志权,王将兵,范丰奇,张朝阳,于强亮,蔡美荣.新型离子液体作为甘油润滑添加剂的摩擦性能[J].表面技术,2020,49(12):177-183. 被引量:1

4施琴,左文艳,赵光霞.含Cr和NbSe2铜基电接触复合材料的制备及性能研究[J].粉末冶金技术,2020,38(6):455-464. 被引量:1

5方勋,严志军,王剑豪,申子玉.考虑空化效应的表面微凸体织构摩擦副润滑性能研究[J].润滑与密封,2020,45(12):32-41. 被引量:4

6罗恒,王优强,张平.双液淬火下7A09铝合金的干滑动摩擦磨损性能[J].材料导报,2020,34(24):24109-24113. 被引量:5

7张鹏林,王斌,王文珍,赵高攀.Al2O3对Ni基复合材料摩擦学性能的影响及机理研究[J].有色金属工程,2020,10(12):22-28. 被引量:1

8曹源,周新聪,黄健,左后秀.UHMWPE与橡胶共混水润滑轴承摩擦磨损性能试验研究[J].润滑与密封,2020,45(12):26-31. 被引量:4

9李振东,詹华,柯庆航,邹卓然,汪瑞军.激光织构和碳基薄膜复合处理提高钛合金摩擦学性能研究[J].润滑与密封,2020,45(12):135-140. 被引量:2

10于鸣泉,王启立,高晓峰,张锋涛,胡建文.煤基浸锑石墨密封材料性能研究[J].润滑与密封,2020,45(12):97-102. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ136.12[化学工程—无机化工]

Citation Information:

Using laboratory-made ultrasonic and microwave ball milling equipment,molybdenum disulfide(MoS2)was modified by the surface modifiers of oleic acid and stearic acid,and the modified molybdenum disulfide(MMD)was obtained.MMD was introduced into the base oil to test its dispersibility and tribological properties,and then the elements of the friction surface was analyzed.The results show that compared with the simple ultrasound method commonly used at present,the molybdenum disulfide modified by ultrasonic and microwave ball milling has more stable dispersion in the base oil.Besides,in the friction process,MMD is more likely to deposit on the friction surface,and tribochemically react with the friction surface to form a more complete lubrication film,thus achieving more excellent anti-friction and anti-wear performance.

quote

GB/T 7714-2015 [1] WANG Si-yuan, CHEN Ding, CHEN Yao-tong, et al. Dispersion and Tribological Properties of Molybdenum Disulfide Modified by Ultrasonic and Microwave Ball Milling[J]. Rare Metals and Cemented Carbides, 2020(6): 46-51.
MLA [1] WANG Si-yuan, et al., "Dispersion and Tribological Properties of Molybdenum Disulfide Modified by Ultrasonic and Microwave Ball Milling." Rare Metals and Cemented Carbides, no. 6, 2020, pp. 46-51.
APA [1] WANG Si-yuan, CHEN Ding, CHEN Yao-tong, & ZHU Kai-ji. (2020). Dispersion and Tribological Properties of Molybdenum Disulfide Modified by Ultrasonic and Microwave Ball Milling. Rare Metals and Cemented Carbides(6), 46-51.
IEEE [1] WANG Si-yuan, CHEN Ding, CHEN Yao-tong, and ZHU Kai-ji, "Dispersion and Tribological Properties of Molybdenum Disulfide Modified by Ultrasonic and Microwave Ball Milling," Rare Metals and Cemented Carbides, no. 6, pp. 46-51, 2020. keywords: {molybdenum disulfide(MoS2);modification;ultrasonic ball-milling;microwave ball-milling;dispersion stability;tribological property}