Preparation and Strengthening Mechanism Analysis of ZrO_2 Doped Molybdenum Alloy AITranslate
Abstract AITranslate
ZrO2 doped molybdenum powders were prepared by sol-gel process and two stage hydrogen reduction,and then ZrO2 doped molybdenum alloy was prepared by powder metallurgy process. ZrO2 doped molybdenum powders and ZrO2 doped molybdenum alloy were characterized by SEM, TEM, XRD and EDS,and the strengthening mechanism of ZrO2 doped molybdenum alloy was investigated. The results show that the prepared ZrO2 doped molybdenum powders have fine but uneven grains and show sphere-like shape, with slight agglomeration phenomenon. The doped ZrO2 of the prepared molybdenum alloy disperses into the grain boundary of molybdenum substrate in the form of the second phase,and the strength of the molybdenum alloy is enhanced by Orowan strengthening and fine grain strengthening.
KeyWords AITranslate
1王敬生,韩红卫.钼材在玻璃工业中的应用[J].中国钼业,2003,27(6):28-31. 被引量:5
2Jalaly M, Bafghi M Sh, Tamizifar M, et al. Formation mechanism of ZrB2- Al2O3 nanocomposite powder by mechanically induced self-sustaining reaction[J]. Journal of Materials Science,2013,48:7 557-7 567.
3许焕,李拴才.提高钼电极质量和使用性能的研究[J].玻璃与搪瓷,2007,35(F08):69-71. 被引量:5
4春燕,沈观清,杨浩,杨超,何林,马韦韦,贺来占,刘文泰,杨德林.熔制玻璃用电极的新进展[J].玻璃与搪瓷,2013,41(2):35-41. 被引量:8
5周文元,张久兴,周美玲,等.烧结工艺对Mo-La2O3合金组织的影响[J].稀有金属材料与工程.2002,31(Z2):112-114.
6孙世杰.普兰西公司开发出具有极强抗腐蚀能力的钼电极[J].粉末冶金工业,2010(5):53-53. 被引量:3
7Nian Hongqiang, Xia Jinfeng, Feng Tao. Corrosion be havior of ZrO2-Mo composite in Na2SO4 solution[J]. Key Engineering Materials, 2012,544 : 351-354.
8张俊,罗振中,李益民,王政伟.稀土镧对氧化钼氢还原的影响[J].中国钼业,2006,30(3):36-39. 被引量:8
9郭丽娜,胡本芙,刘安强,贾成厂,李慧英.氧化物弥散强化钢的强化机理[J].北京科技大学学报,2013,35(5):586-591. 被引量:9
1康蓉,颜建辉,李茂键.溶胶凝胶/高温氢还原法制备纳米Mo-ZrO_(2)(Y_(2)O_(3))复合粉末[J].稀有金属,2021,45(3):288-296. 被引量:4
1颜建辉,康蓉,唐幸,汪异,邱敬文.ZrO_(2)(Y_(2)O_(3))含量对双峰晶粒度分布Mo-12Si-8.5B-ZrO_(2)(Y_(2)O_(3))复合材料力学性能的影响[J].复合材料学报,2021,38(11):3747-3756. 被引量:3
2王晶,钱凌翼,郭云珊,Richard Wheatley,侯向辉,刘宇阳.R_(2)O_(3)+Er_(2)O_(3)稳定ZrO_(2)的新型TBC材料[J].稀有金属,2022,46(7):853-861.
3焦照临,徐流杰,徐照宁,周玉成,杨璐.Al_(2)O_(3)掺杂钼合金的显微组织及电化学腐蚀行为研究[J].稀有金属与硬质合金,2022,50(5):59-65.
4吴吉文,颜建辉,汪异,邱敬文.ZrO_(2)(Y_(2)O_(3))含量对Mo-12Si-8.5B-ZrO_(2)(Y_(2)O_(3))复合材料高温氧化性能的影响[J].材料热处理学报,2023,44(7):39-47.
1余乐英,刘志东,郭延风,尚玉华.含硼涂层的电子探针分析[J].电子显微学报,1991,10(3):260-265. 被引量:1
2姜超平,邢亚哲,郝建民.Mo基合金粉末对Fe基非晶涂层耐蚀性能影响[J].热加工工艺,2011,40(8):144-146. 被引量:8
3李渝.掺杂Mo的低温断裂特性及He退火脆性[J].钨钼材料,1990(4):39-42.
4马琰华,李继文,魏世忠,徐流杰,宫方方,赵晶晶.水热合成法制备稀土掺杂Mo粉的工艺研究[J].稀有金属与硬质合金,2013,41(5):15-18. 被引量:1
5李洲,徐流杰,魏世忠,潘昆明,肖方闹.水热法制备ZrO_2掺杂钨合金粉末的工艺研究及表征[J].稀有金属与硬质合金,2017,45(1):31-35. 被引量:4
6李建辉,杜文博,吴玉锋,左铁镛.Mg-6Al-2Sr-xNd镁合金的显微组织和力学性能[J].特种铸造及有色合金,2007,27(6):482-484. 被引量:8
7王小强,李全安,张兴渊.Y对AZ81镁合金组织和力学性能的影响[J].特种铸造及有色合金,2007,27(5):384-387. 被引量:14
8薛莹莹,纪武仁.稀土元素对Mo基合金高温退火后性能的影响[J].装备制造技术,2012(9):26-27.
9张令波,王可铮,徐丽娟,肖树龙,陈玉勇.Nb元素对β型Ti-Mo基合金显微组织、力学性能和铸造性能的影响(英文)[J].中国有色金属学报:英文版,2015,25(7):2214-2220. 被引量:3
10肖方闹,徐流杰,周玉成,潘昆明,魏世忠.ZrO_2增强钨基复合材料制备工艺与性能[J].材料热处理学报,2016,37(2):12-19.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]
Citation Information:
ZrO2 doped molybdenum powders were prepared by sol-gel process and two stage hydrogen reduction,and then ZrO2 doped molybdenum alloy was prepared by powder metallurgy process. ZrO2 doped molybdenum powders and ZrO2 doped molybdenum alloy were characterized by SEM, TEM, XRD and EDS,and the strengthening mechanism of ZrO2 doped molybdenum alloy was investigated. The results show that the prepared ZrO2 doped molybdenum powders have fine but uneven grains and show sphere-like shape, with slight agglomeration phenomenon. The doped ZrO2 of the prepared molybdenum alloy disperses into the grain boundary of molybdenum substrate in the form of the second phase,and the strength of the molybdenum alloy is enhanced by Orowan strengthening and fine grain strengthening.
quote
| GB/T 7714-2015 | [1] GUO Song-liang, ZHANG Guo-shang, WEI Shi-zhong, et al. Preparation and Strengthening Mechanism Analysis of ZrO_2 Doped Molybdenum Alloy[J]. Rare Metals and Cemented Carbides, 2014(5): 48-50. |
| MLA | [1] GUO Song-liang, et al., "Preparation and Strengthening Mechanism Analysis of ZrO_2 Doped Molybdenum Alloy." Rare Metals and Cemented Carbides, no. 5, 2014, pp. 48-50. |
| APA | [1] GUO Song-liang, ZHANG Guo-shang, WEI Shi-zhong, XU Liu-jie, & CUI Chao-peng. (2014). Preparation and Strengthening Mechanism Analysis of ZrO_2 Doped Molybdenum Alloy. Rare Metals and Cemented Carbides(5), 48-50. |
| IEEE | [1] GUO Song-liang, ZHANG Guo-shang, WEI Shi-zhong, XU Liu-jie, and CUI Chao-peng, "Preparation and Strengthening Mechanism Analysis of ZrO_2 Doped Molybdenum Alloy," Rare Metals and Cemented Carbides, no. 5, pp. 48-50, 2014. keywords: {ZrO2 doped molybdenum alloy;ZrO2 doped molybdenum powder;Orowan strengthening;fine grain strengthening} |