Electrochromic Ru-Based Metallo-Supramolecular Polymer with a Layered Inorganic−Organic Hybrid Nanocomposite for Improved Electrochemical Properties AITranslate
Abstract AITranslate
Herein, we report improving the electrochromic (EC) properties of metallo-supramolecular polymers (MSPs) via forming nanocomposite with a layered inorganic-imidazoline covalently bonded hybrid (LIIm). Polymer-based nanocomposites exhibit improvements in mechanical, optical, gas barrier properties, etc. Clay minerals and organoclays are beneficial additives in synthesizing nanocomposites. However, only a few investigations of their EC properties have been reported. We have prepared the nanocomposites of Ru(II)-based metallo-supramolecular polymer (polyRu) and LIIm by mixing them in various polyRu/LIIm ratios in methanol. Then, the EC properties and structural features of the resulting red nanocomposites (polyRu–LIIm composites) were analyzed. The polyRu–LIIm composites exhibited strong metal-to-ligand charge transfer (MLCT) absorptions at ∼530 nm with a slight red shift (4–7 nm) than that of pristine polyRu. The MLCT absorptions of polyRu–LIIm composites were more intense than that of polyRu. Spin-coated polyRu–LIIm composite films showed a reversible pair of redox waves at half-wave potentials (E1/2) of 0.9 V in cyclic voltammetry (CV) curves and reversible EC changes between red and pale green caused by the redox of Ru(II/III) upon applied potential. The E1/2 and peak currents do not drastically change compared to those of polyRu. Furthermore, the composite thin films exhibited coloration efficiencies (CE) of 640–810 cm2/C higher than the 597 cm2/C of polyRu. The high optical contrasts (ΔT) of >70% and fast switching times were maintained. Scanning electron microscopy (SEM)–energy-dispersive X-ray (EDX) and X-ray diffraction (XRD) analyses revealed the characteristic structural features of polyRu–LIIm composites where polyRu-coated LIIm forms agglomerate (200 nm–10 μm), which varied with the polyRu/LIIm ratios. Furthermore, the EC memory times were improved to 26 min for one of the polyRu–LIIm composites from 170 s of polyRu.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00837
Chinese Library Classification Number:
Citation Information:
Herein, we report improving the electrochromic (EC) properties of metallo-supramolecular polymers (MSPs) via forming nanocomposite with a layered inorganic-imidazoline covalently bonded hybrid (LIIm). Polymer-based nanocomposites exhibit improvements in mechanical, optical, gas barrier properties, etc. Clay minerals and organoclays are beneficial additives in synthesizing nanocomposites. However, only a few investigations of their EC properties have been reported. We have prepared the nanocomposites of Ru(II)-based metallo-supramolecular polymer (polyRu) and LIIm by mixing them in various polyRu/LIIm ratios in methanol. Then, the EC properties and structural features of the resulting red nanocomposites (polyRu–LIIm composites) were analyzed. The polyRu–LIIm composites exhibited strong metal-to-ligand charge transfer (MLCT) absorptions at ∼530 nm with a slight red shift (4–7 nm) than that of pristine polyRu. The MLCT absorptions of polyRu–LIIm composites were more intense than that of polyRu. Spin-coated polyRu–LIIm composite films showed a reversible pair of redox waves at half-wave potentials (E1/2) of 0.9 V in cyclic voltammetry (CV) curves and reversible EC changes between red and pale green caused by the redox of Ru(II/III) upon applied potential. The E1/2 and peak currents do not drastically change compared to those of polyRu. Furthermore, the composite thin films exhibited coloration efficiencies (CE) of 640–810 cm2/C higher than the 597 cm2/C of polyRu. The high optical contrasts (ΔT) of >70% and fast switching times were maintained. Scanning electron microscopy (SEM)–energy-dispersive X-ray (EDX) and X-ray diffraction (XRD) analyses revealed the characteristic structural features of polyRu–LIIm composites where polyRu-coated LIIm forms agglomerate (200 nm–10 μm), which varied with the polyRu/LIIm ratios. Furthermore, the EC memory times were improved to 26 min for one of the polyRu–LIIm composites from 170 s of polyRu.
quote
| GB/T 7714-2015 | [1] Kazuko Fujii, Dines Chandra Santra, Manas Kumar Bera, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00837. |
| MLA | [1] Kazuko Fujii, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00837. |
| APA | [1] Kazuko Fujii, Dines Chandra Santra, Manas Kumar Bera, Takatsugu Wakahara, Ritsuko Nagahata, & Masayoshi Higuchi. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00837 |
| IEEE | [1] Kazuko Fujii, Dines Chandra Santra, Manas Kumar Bera, Takatsugu Wakahara, Ritsuko Nagahata, and Masayoshi Higuchi, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00837. keywords: {metallosupramolecular polymer;composite;electrochromism;layered inorganic−organic hybrid;clay} |