Abstract AITranslate
A temperature-responsive photonic coating on a flexible substrate was prepared by a photoinduced phase-separation process. In this coating a low molecular weight cholesteric liquid crystal (Ch-LC) mixture was encapsulated between the substrate and an in situ formed protective polymer top layer. The photonic coating showed a blue-shift of the photonic reflection band of 100 nm by heating from 22 to 23 °C due to the close proximity to the smectic to cholesteric phase transition and an overall 330 nm blue-shift while heating from 22 to 45 °C. Hence, the red coating turned green upon contact with skin within seconds. Furthermore, the coating structure and composition were investigated in detail, revealing a thick top coat. The adhesion of the coating was improved by providing trays on the substrate (by etching or 3D printing), resulting in a link between arbitrary-shaped substrates and the protective polymer top layer. These bendable coatings could be of interest for sensors, anticounterfeit labels, or customizable aesthetic applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00841
Chinese Library Classification Number:
Citation Information:
A temperature-responsive photonic coating on a flexible substrate was prepared by a photoinduced phase-separation process. In this coating a low molecular weight cholesteric liquid crystal (Ch-LC) mixture was encapsulated between the substrate and an in situ formed protective polymer top layer. The photonic coating showed a blue-shift of the photonic reflection band of 100 nm by heating from 22 to 23 °C due to the close proximity to the smectic to cholesteric phase transition and an overall 330 nm blue-shift while heating from 22 to 45 °C. Hence, the red coating turned green upon contact with skin within seconds. Furthermore, the coating structure and composition were investigated in detail, revealing a thick top coat. The adhesion of the coating was improved by providing trays on the substrate (by etching or 3D printing), resulting in a link between arbitrary-shaped substrates and the protective polymer top layer. These bendable coatings could be of interest for sensors, anticounterfeit labels, or customizable aesthetic applications.
quote
| GB/T 7714-2015 | [1] Ellen P. A. van Heeswijk, Toob Meerman, Jos de Heer, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00841. |
| MLA | [1] Ellen P. A. van Heeswijk, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00841. |
| APA | [1] Ellen P. A. van Heeswijk, Toob Meerman, Jos de Heer, Nadia Grossiord, & Albert P. H. J. Schenning. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00841 |
| IEEE | [1] Ellen P. A. van Heeswijk, Toob Meerman, Jos de Heer, Nadia Grossiord, and Albert P. H. J. Schenning, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00841. keywords: {temperatureresponsive polymers;cholesteric liquid crystals;photonic materials;coatings;Show More} |