Coordinative integration of amorphous nickel-imidazole framework with graphitic carbon nitride for enhanced photocatalytic hydrogen production AITranslate

SRM Institute of Science and Technology; SRM Institute of Science and Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, a new nickel metal-organic framework (Ni-MOF) was integrated with graphitic carbon nitride (g-C3N4) (prepared by polycondensation of different precursors, i.e., urea, thiourea and melamine) using the solvothermal method and used for the photocatalytic hydrogen production. Notably, crystalline Ni-MOF was unable to bond with g-C3N4 due to completely coordinated nickel sites in Ni-MOF, but amorphous Ni-MOF (aNi-MOF) successfully bonded with g-C3N4 owing to its uncoordinated nickel sites. The aNi-MOF incorporated with g-C3N4 (prepared by urea) exhibited hydrogen production of 2272.6 μmol g−1 h−1 which was ∼450, 4 and 7 times higher than aNi-MOF, thiourea and melamine derived g-C3N4 integrated with aNi-MOF, respectively. The substantial increment in photocatalytic activity can be attributed to the synergistic structural reconstruction of g-C3N4/aNi-MOF in accordance with varying dangling amine groups, surface area and porosity offered by different precursors in formation of g-C3N4. Remarkably, the proposed work is the first report on the photocatalytic hydrogen production by an amorphous metal-organic framework and also an imidazole-based nickel framework. Thus, this work provides insight into the designing amorphous MOF- extended polymer heterostructure and will open up a new avenue to their catalytic performances. Graphical abstract Download : Download high-res image (190KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2022.101524

Chinese Library Classification Number:

Citation Information:

Herein, a new nickel metal-organic framework (Ni-MOF) was integrated with graphitic carbon nitride (g-C3N4) (prepared by polycondensation of different precursors, i.e., urea, thiourea and melamine) using the solvothermal method and used for the photocatalytic hydrogen production. Notably, crystalline Ni-MOF was unable to bond with g-C3N4 due to completely coordinated nickel sites in Ni-MOF, but amorphous Ni-MOF (aNi-MOF) successfully bonded with g-C3N4 owing to its uncoordinated nickel sites. The aNi-MOF incorporated with g-C3N4 (prepared by urea) exhibited hydrogen production of 2272.6 μmol g−1 h−1 which was ∼450, 4 and 7 times higher than aNi-MOF, thiourea and melamine derived g-C3N4 integrated with aNi-MOF, respectively. The substantial increment in photocatalytic activity can be attributed to the synergistic structural reconstruction of g-C3N4/aNi-MOF in accordance with varying dangling amine groups, surface area and porosity offered by different precursors in formation of g-C3N4. Remarkably, the proposed work is the first report on the photocatalytic hydrogen production by an amorphous metal-organic framework and also an imidazole-based nickel framework. Thus, this work provides insight into the designing amorphous MOF- extended polymer heterostructure and will open up a new avenue to their catalytic performances. Graphical abstract Download : Download high-res image (190KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Aswathy Rajan, B. Neppolian. Applied Materials Today, 2022(28). DOI:10.1016/j.apmt.2022.101524.
MLA [1] Aswathy Rajan, and B. Neppolian. Applied Materials Today, no. 28, 2022, https://doi.org/10.1016/j.apmt.2022.101524.
APA [1] Aswathy Rajan, & B. Neppolian. (2022). Applied Materials Today(28). https://doi.org/10.1016/j.apmt.2022.101524
IEEE [1] Aswathy Rajan and B. Neppolian, Applied Materials Today, no. 28, 2022, doi: 10.1016/j.apmt.2022.101524.