Interface and Border Traps in the Gate Stack of Carbon Nanotube Film Transistors with an Yttria Dielectric Interface and Border Traps in the Gate Stack of Carbon Nanotube Film Transistors with an Yttria Dielectric AITranslate
Abstract AITranslate
Measurement and optimization of interface states in metal oxide semiconductors are the premise of building high-performance and high-reliability field-effect transistors (FETs). Although FETs built on semiconducting carbon nanotube (CNT) films have been demonstrated as promising devices for many applications, including integrated circuits (ICs), thin-film electronics, and biosensors, systemic research on the interface state of CNT film FETs, including accurate measurement and optimization schemes, is lacking. In this work, we fabricate MOS capacitors with an area of 400 μm2 on a CNT network film with a Y2O3 gate dielectric and carry out admittance measurements to investigate electrically active traps near the Y2O3/CNT interface. Through the conductance method and high-low frequency method, we extract the energy-dependent interface trap density (Dit) and border trap density (Nbt) of CNT MOS FETs based on the measured admittance dataset. Postdeposition annealing (PDA) processes with different gases at 300 °C show the ability to lower the Dit and Nbt of the Y2O3/CNT interface and then improve the performance of CNT film FETs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00613
Chinese Library Classification Number:
Citation Information:
Measurement and optimization of interface states in metal oxide semiconductors are the premise of building high-performance and high-reliability field-effect transistors (FETs). Although FETs built on semiconducting carbon nanotube (CNT) films have been demonstrated as promising devices for many applications, including integrated circuits (ICs), thin-film electronics, and biosensors, systemic research on the interface state of CNT film FETs, including accurate measurement and optimization schemes, is lacking. In this work, we fabricate MOS capacitors with an area of 400 μm2 on a CNT network film with a Y2O3 gate dielectric and carry out admittance measurements to investigate electrically active traps near the Y2O3/CNT interface. Through the conductance method and high-low frequency method, we extract the energy-dependent interface trap density (Dit) and border trap density (Nbt) of CNT MOS FETs based on the measured admittance dataset. Postdeposition annealing (PDA) processes with different gases at 300 °C show the ability to lower the Dit and Nbt of the Y2O3/CNT interface and then improve the performance of CNT film FETs.
quote
| GB/T 7714-2015 | [1] Hongshan Xiao, Yifan Liu, Sujuan Ding, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00613. |
| MLA | [1] Hongshan Xiao, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00613. |
| APA | [1] Hongshan Xiao, Yifan Liu, Sujuan Ding, Yunfei Gao, Minglong Zhai, Xuelei Liang, Chuanhong Jin, Honggang Liu, & Zhiyong Zhang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00613 |
| IEEE | [1] Hongshan Xiao, Yifan Liu, Sujuan Ding, Yunfei Gao, Minglong Zhai, Xuelei Liang, Chuanhong Jin, Honggang Liu, and Zhiyong Zhang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00613. keywords: {carbon nanotube fieldeffect transistor interface state border trap gate dielectric} |