daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Investigation on Oxidizing Kinetics of W Powder AITranslate

Zhongnan University of Technology;Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using the thin layer static method, the oxiding kinetics of W powder have been studied. The powder for study is classified by fluidized new technique. Results show that oxidization of W particles also follows the parabola-straight line oxidization mechanisin. On the basis of the exper imental results the mathematical model of oxidization for W powder has been established.

KeyWords AITranslate

W powder oxidizing kinetics mathematical model

1刘文胜,邹海平,杨立.球形钨粉制备技术的探讨[J].硬质合金,2011,28(4):261-266. 被引量:4

1德志强.高质量结晶钨粉制取的工艺研究[J].硬质合金,2014,31(3):166-172. 被引量:1

2张莹莹,周武平,王铁军,王学兵,杨怀超,梁俊才.球形钨粉的制备技术研究进展[J].粉末冶金工业,2018,28(3):67-73. 被引量:7

3陈伦江,陈文波,刘川东,童洪辉,赵青.钨粉的球化及前驱体钨粉注入对等离子温度的影响[J].稀有金属材料与工程,2019,48(10):3221-3226.

4李剑,刘宇.钨浆料用钨粉研究进展[J].陶瓷,2021(3):50-52.

1梁杰,郑东升,韦丽萍.锗烟尘中氧化锌浸出过程动力学研究[J].贵州工业大学学报:自然科学版,2004,33(4):43-46.

2姚耀春,王平.难选氧化锌矿氨浸的动力学研究[J].云南冶金,2001,30(3):22-24. 被引量:9

3王念卫,王成彦,尹飞,陈永强.高碱性脉石低品位氧化锌矿低浓度氨浸动力学研究[J].矿冶,2010,19(1):36-39. 被引量:1

4袁斌,邓舜勤.用D501树脂分离钨溶液中微量钼[J].铀矿冶,2001,20(4):245-250. 被引量:4

5张晴,彭西高.炼铜转炉用镁铬砖的静态坩埚法侵蚀试验分析[J].耐火材料,2004,38(6):447-447. 被引量:1

6时文中,李冠峰,赵永和,朱国才.氯化铵氯化氧化镧氧化铈混合物及其动力学[J].信阳师范学院学报:自然科学版,2005,18(2):155-158. 被引量:5

7刘恒,金作美.ZnS和ZnS/C浸出动力学研究[J].有色金属,1990(1):60-65. 被引量:1

8但勇,丰驰.氯化钴溶液中树脂交换除Cu(Ⅱ)新工艺试验报告[J].四川有色金属,2002(2):22-24. 被引量:2

9苏毅,金作美,代祖元.电解锌的SO_2阳极反应动力学[J].中国有色金属学报,2001,11(3):495-498. 被引量:10

10刘峙嵘,郭锦勇.D_(911)树脂吸附富集金的性能研究[J].黄金,1997,18(4):39-41. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF122.3[冶金工程—粉末冶金]

Citation Information:

Using the thin layer static method, the oxiding kinetics of W powder have been studied. The powder for study is classified by fluidized new technique. Results show that oxidization of W particles also follows the parabola-straight line oxidization mechanisin. On the basis of the exper imental results the mathematical model of oxidization for W powder has been established.

quote

GB/T 7714-2015 [1] LI Han-guang, PENG Zhi-hui. Investigation on Oxidizing Kinetics of W Powder[J]. Rare Metals and Cemented Carbides, 1995(4): 1-6.
MLA [1] LI Han-guang, and PENG Zhi-hui. "Investigation on Oxidizing Kinetics of W Powder." Rare Metals and Cemented Carbides, no. 4, 1995, pp. 1-6.
APA [1] LI Han-guang, & PENG Zhi-hui. (1995). Investigation on Oxidizing Kinetics of W Powder. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] LI Han-guang and PENG Zhi-hui, "Investigation on Oxidizing Kinetics of W Powder," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 1995. keywords: {W powder, oxidizing kinetics, mathematical model}