Technological Study on Yttrium-Cerium Phosphate Production by Phosphoric Acid Precipitation AITranslate
Abstract AITranslate
The technology is introduced for yttrium-cerium phosphate production with ReCl3 solution as the raw material and phosphoric acid as the precipitation agent. The influencing factors were investigated on the rare earth recovery and yttrium-cerium phosphate medium diameter, and the optimal technological con- ditions were determined. The results show that when the precipitation temperature is about 80 ℃ and the phosphoric acid concentration in the precipitated solution is about 0.12 mol/L, the rare earth recovery is higher. The yttrium-cerium phosphate product can be produced in a certain range of medium diameter, by controlling of single reactor output and appropriate stirring. By proper control of technological conditions, the yttrium-cerium phosphate product with a medium diameter of 3-10μm can be obtained in mass pro duction,and the rare earth recovery is over 90%.
KeyWords AITranslate
1WangCS.我国灯用稀土产业发展综述[EB/OL].http://www.mining120.com/Html/1205/2012050927833.asp,2007-11-09.
2杨定明,朱达川,涂铭旌.机械力固相化学反应法合成稀土磷酸盐绿色荧光粉[J].四川大学学报:工程科学版,2005,37(3):61-63. 被引量:6
3刘南生,孙曰圣,彭宏博,熊瑛,张小林,邹建国.共沉淀法制备不球磨稀土磷酸盐绿色荧光粉研究[J].发光学报,2001,22(4):412-416. 被引量:12
4赵小山,陈其安.用稀土草酸盐作前驱物合成磷酸镧铈铽[J].稀土,2002,23(3):14-15. 被引量:4
1姚虎卿,陈国栋,孔庆震.氯化稀土与NaY沸石水热交换的研究[J].石油学报(石油加工),1991,7(1):103-108. 被引量:10
2邓波,汤洪敏.KMnO_4氧化法冷制淀粉粘合剂[J].企业科技与发展,1998,0(9):16-16.
3冯宜绥.浅析降低REY分子筛原材料氯化稀土的单耗[J].甘肃科技,2011,27(10):34-35. 被引量:2
4詹予忠,董佳佳,宋孟璐,韩丽,陈宜俍.SAPO-56分子筛的形貌和粒径控制[J].郑州大学学报:工学版,2014,35(6):23-26. 被引量:2
5张高文,叶莹,杨侃,刘嘉宁.无皂乳液聚合法合成阴离子PS微球及粒径控制[J].高分子通报,2013(5):60-64. 被引量:2
6蒋顺进,汤晓林.盐霉素发酵工艺的优化研究[J].今日药学,2010,20(10):23-25. 被引量:2
7姚虎卿,陈国栋,孔庆震.氯化稀土与NaY沸石的水热交换[J].南京化工学院学报,1990,12(1):16-21.
8蒋昌武,何喜庆,吴琳俐,陈纯,杨光,张俐娜.再生纤维素荧光膜[J].应用化学,1995,12(1):30-33. 被引量:6
9王学平,颜旸旸.REY分子筛生产工艺的分析与优化[J].山东工业技术,2017(2):12-12. 被引量:1
10孙瑞雪,史京京,郭燕川,陈丽娟.明胶微球粒径控制的研究[J].高分子学报,2008(8):779-784. 被引量:12
Basic Information:
DOI:
Chinese Library Classification Number:TQ422[化学工程]
Citation Information:
The technology is introduced for yttrium-cerium phosphate production with ReCl3 solution as the raw material and phosphoric acid as the precipitation agent. The influencing factors were investigated on the rare earth recovery and yttrium-cerium phosphate medium diameter, and the optimal technological con- ditions were determined. The results show that when the precipitation temperature is about 80 ℃ and the phosphoric acid concentration in the precipitated solution is about 0.12 mol/L, the rare earth recovery is higher. The yttrium-cerium phosphate product can be produced in a certain range of medium diameter, by controlling of single reactor output and appropriate stirring. By proper control of technological conditions, the yttrium-cerium phosphate product with a medium diameter of 3-10μm can be obtained in mass pro duction,and the rare earth recovery is over 90%.
quote
| GB/T 7714-2015 | [1] ZHAN Xian. Technological Study on Yttrium-Cerium Phosphate Production by Phosphoric Acid Precipitation[J]. Rare Metals and Cemented Carbides, 2013(4): 18-20. |
| MLA | [1] ZHAN Xian. "Technological Study on Yttrium-Cerium Phosphate Production by Phosphoric Acid Precipitation." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 18-20. |
| APA | [1] ZHAN Xian. (2013). Technological Study on Yttrium-Cerium Phosphate Production by Phosphoric Acid Precipitation. Rare Metals and Cemented Carbides(4), 18-20. |
| IEEE | [1] ZHAN Xian, "Technological Study on Yttrium-Cerium Phosphate Production by Phosphoric Acid Precipitation," Rare Metals and Cemented Carbides, no. 4, pp. 18-20, 2013. keywords: {rare earth phosphate;yttrium-cerium phosphate;rare earth chloride;precipitation method;medi- um diameter control;process optimization} |