Carrier Dynamics for the Collective Resonant Tunneling in Quantum Dot-Based Artificial Graphene AITranslate

Fudan University; Fudan University; Xidian University; Fudan University; Fudan University; Fudan University; Fudan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Semiconductor quantum-dot (QD)-based artificial graphene (AG) is of great interest thanks to its innovative properties associated with the honeycomb topology, the many-body effects and the spin–orbit coupling of carriers, and its promising device applications. Considering the carrier variation in the real space of QDs besides the momentum space of AG, it is a big challenge to clarify the carrier dynamics that is the key feature and the base for device applications of QD-based AG. Here, the carrier dynamics for the collective resonant tunneling (CRT) of holes among QDs of AG is demonstrated. The current peak due to the CRT is affected by the voltage sweeping rate that modulates the number and the miniband width of holes in QDs of AG. The time-dependent conductance discloses three transport phases intimately associated with the number of holes in QDs of AG. Particularly, the CRT-induced high conductance phase is the figure of merit of AG. The phase transition and even the dual stable phases of transport can be realized by temporarily manipulating holes in QDs of AG via programmable voltages. Our results provide a guide to manipulate carriers in QD-based AG using an electric field to explore unique features and innovative devices of AG.

KeyWords AITranslate

artificial graphene quantum dot collective resonant tunneling carrier dynamics transport phases
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01223

Chinese Library Classification Number:

Citation Information:

Semiconductor quantum-dot (QD)-based artificial graphene (AG) is of great interest thanks to its innovative properties associated with the honeycomb topology, the many-body effects and the spin–orbit coupling of carriers, and its promising device applications. Considering the carrier variation in the real space of QDs besides the momentum space of AG, it is a big challenge to clarify the carrier dynamics that is the key feature and the base for device applications of QD-based AG. Here, the carrier dynamics for the collective resonant tunneling (CRT) of holes among QDs of AG is demonstrated. The current peak due to the CRT is affected by the voltage sweeping rate that modulates the number and the miniband width of holes in QDs of AG. The time-dependent conductance discloses three transport phases intimately associated with the number of holes in QDs of AG. Particularly, the CRT-induced high conductance phase is the figure of merit of AG. The phase transition and even the dual stable phases of transport can be realized by temporarily manipulating holes in QDs of AG via programmable voltages. Our results provide a guide to manipulate carriers in QD-based AG using an electric field to explore unique features and innovative devices of AG.

quote

GB/T 7714-2015 [1] Peizong Chen, Jia Yan, Ningning Zhang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01223.
MLA [1] Peizong Chen, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01223.
APA [1] Peizong Chen, Jia Yan, Ningning Zhang, Yan Zhan, Qiang Huang, Zuimin Jiang, & Zhenyang Zhong. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01223
IEEE [1] Peizong Chen, Jia Yan, Ningning Zhang, Yan Zhan, Qiang Huang, Zuimin Jiang, and Zhenyang Zhong, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01223. keywords: {artificial graphene quantum dot collective resonant tunneling carrier dynamics transport phases}