Combined Determination of Cobalt and Nickel inCemented Carbide by EDTA Direct Titration AITranslate

Department of Chemistry, Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper describes the combined determination of Co-Niin ammoniac ined'ium using M X as indicator and EDTA as titratant.Its Ni can be determine6 by EDTA titration from another part of samesample Co of which is covered' first with (NH4)2S2O8. This method hasbeen used for the determination of Co, and Ni in cementeds carbi ewith satisfactory results.

KeyWords AITranslate

cemented carbide Co Ni EDTA direct titration

1李习纯.络合电位滴定法连续测定矿石中铜、钴和镍[J].冶金分析,1994,14(2):41-42. 被引量:6

1徐洪文,姜鲁娜.合金钢中锰铬联测研究[J].烟台大学学报:自然科学与工程版,1997,10(1):76-78. 被引量:1

2赵洁芳.银焊条中银的化学分析[J].杭氧科技,2003(2):50-51. 被引量:1

3李习纯,曾晓晖.铜合金中锡和铜的快速测定[J].有色金属分析通讯,1992(4):19-20.

4付明.强碱—EDTA容量法测定中,高铝浅议[J].武汉冶金,1993(2):19-21. 被引量:1

5鲁静冬,马英,陈一琼,顾晓川,张显平.ICP-AES法联测合金钢中钼、镍、硅、锰、铬、钒[J].四川冶金,2008,30(1):47-49. 被引量:7

6吴岩青,郭润秀.络合滴定法连续测定钨镍铜合金中的镍和铜[J].理化检验:化学分册,1998,34(11):494-495. 被引量:12

7曾波,涂昀,范菁,姚汝胜.二次缩分直接滴定法测定钙铁线中钙、铁[J].特钢技术,2011,17(4):49-50. 被引量:3

8杨俊铭,王丽梅.高钨钢中八元素的原子吸收—化学联测法[J].冶金分析,1989,9(4):57-58. 被引量:2

9洪榕,苏洁雯,甘振杰.BH-铝合金浸锌液中锌的化学分析[J].电镀与涂饰,2006,25(9):56-57.

10朱映生.锡铅焊料中锡量的测定──EDTA络合滴定法[J].云锡科技,1993,20(1):46-52.

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程];TG115.314[金属学及工艺—物理冶金]

Citation Information:

This paper describes the combined determination of Co-Niin ammoniac ined'ium using M X as indicator and EDTA as titratant.Its Ni can be determine6 by EDTA titration from another part of samesample Co of which is covered' first with (NH4)2S2O8. This method hasbeen used for the determination of Co, and Ni in cementeds carbi ewith satisfactory results.

quote

GB/T 7714-2015 [1] LI Xi-chun. Combined Determination of Cobalt and Nickel inCemented Carbide by EDTA Direct Titration[J]. Rare Metals and Cemented Carbides, 1995(1): 9-11.
MLA [1] LI Xi-chun. "Combined Determination of Cobalt and Nickel inCemented Carbide by EDTA Direct Titration." Rare Metals and Cemented Carbides, no. 1, 1995, pp. 9-11.
APA [1] LI Xi-chun. (1995). Combined Determination of Cobalt and Nickel inCemented Carbide by EDTA Direct Titration. Rare Metals and Cemented Carbides(1), 9-11.
IEEE [1] LI Xi-chun, "Combined Determination of Cobalt and Nickel inCemented Carbide by EDTA Direct Titration," Rare Metals and Cemented Carbides, no. 1, pp. 9-11, 1995. keywords: {cemented carbide;Co;Ni;EDTA direct titration}