Direct Synthesis of Highly Siliceous ZnO-FAU Zeolite with Enhanced Performance in Hydrocarbon Cracking Reactions AITranslate
Abstract AITranslate
The hydrothermal stability and catalytic activity of zeolite Y (faujasite, FAU) is highly dependent on its composition. High silicon content is often desirable for catalytic applications; however, direct synthesis of faujasite with high silicon content (Si/Al > 2.5) is nontrivial. Here, we present an organic-free synthesis of FAU-type zeolite with Si/Al = 3.4 using zinc oxide as a modifier. A combination of spectroscopy and microscopy techniques confirms that ZnO is well-distributed within zeolite pores as extra-framework species, and the nature of these species differs from bulk ZnO and framework zinc in Zn-FAU crystals. We demonstrate that the increased Si/Al ratio leads to improved hydrothermal stability, while catalytic cracking of 1-hexene and cumene show that ZnO-FAU exhibits a significantly longer lifetime compared to in-house and commercial zeolite Y. Collectively, this study presents a facile and efficient method to prepare more siliceous FAU with enhanced catalytic performance.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c00978
Chinese Library Classification Number:
Citation Information:
The hydrothermal stability and catalytic activity of zeolite Y (faujasite, FAU) is highly dependent on its composition. High silicon content is often desirable for catalytic applications; however, direct synthesis of faujasite with high silicon content (Si/Al > 2.5) is nontrivial. Here, we present an organic-free synthesis of FAU-type zeolite with Si/Al = 3.4 using zinc oxide as a modifier. A combination of spectroscopy and microscopy techniques confirms that ZnO is well-distributed within zeolite pores as extra-framework species, and the nature of these species differs from bulk ZnO and framework zinc in Zn-FAU crystals. We demonstrate that the increased Si/Al ratio leads to improved hydrothermal stability, while catalytic cracking of 1-hexene and cumene show that ZnO-FAU exhibits a significantly longer lifetime compared to in-house and commercial zeolite Y. Collectively, this study presents a facile and efficient method to prepare more siliceous FAU with enhanced catalytic performance.
quote
| GB/T 7714-2015 | [1] Deependra Parmar, Adam J. Mallette, Noemi Linares, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00978. |
| MLA | [1] Deependra Parmar, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00978. |
| APA | [1] Deependra Parmar, Adam J. Mallette, Noemi Linares, Sarah A. Saslow, Tanguy Terlier, James J. Strohm, Lee P. Barber, Heng Dai, Javier GarcíaMartínez, & Jeffrey D. Rimer. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00978 |
| IEEE | [1] Deependra Parmar, Adam J. Mallette, Noemi Linares, Sarah A. Saslow, Tanguy Terlier, James J. Strohm, Lee P. Barber, Heng Dai, Javier GarcíaMartínez, and Jeffrey D. Rimer, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00978. |