Effects of Technological Conditions on Microstructure and Properties of In-situ Synthesized WC/W Surface Composites AITranslate

Zhuzhou Cemented Carbide Group Corp丒,Ltd丒;Zhuzhou Cemented Carbide Group Corp丒,Ltd丒
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tungsten carbide layers with a certain thickness were in-situ synthesized on the surface of sintered tungsten products by high temperature heat treatment in carbon atmosphere protected by hydrogen gas to prepare WC/W surface composites.The effects of heat treatment temperature and tungsten matrix density on microstructure and properties of in-situ synthesized WC/W surface composites were studied by density and hardness test and metallographic microscope.The element composition and phase composition of tungsten carbide layers were analyzed by SEM/EDS and XRD.The results show that high temperature heat treatment temperature has significant influence on the growth thickness and quality of tungsten carbide layer,while tungsten matrix density has no obvious influence on the growth of tungsten carbide layer.When the temperature is lower than 1 800 ℃,the thickness of the tungsten carbide layer is relatively thin and its strength is poor.However,too high temperature will lead to an increase in defects of the tungsten carbide layer.The tungsten carbide layer in-situ synthesized on the surface of tungsten matrix has columnar crystal microstructure and single phase composition,closely combining with tungsten matrix,and the interface is clean and free of impurities.The surface composites can fully exhibit the excellent properties of the two materials at high temperature.

KeyWords AITranslate

surface composite WC/W in-situ synthesis high temperature treatment matrix density

1张卫兵,颜练武,赵声志,杜承功.超细WC粉末微观缺陷的研究[J].硬质合金,2012,29(5):283-288. 被引量:9

2张小琴,姜银举,代清.真空蒸馏法制备高纯金属钆[J].包钢科技,2007,33(3):17-20. 被引量:13

3陈锦,熊宁,葛启录,刘国辉,刘桂荣,李强.钨坩埚的制备技术[J].中国钨业,2016,31(1):63-67. 被引量:8

4马捷,张好东,毕安园,王从曾,周美玲.化学气相沉积法制取异型钨制品研究[J].兵工学报,2006,27(2):315-319. 被引量:26

5郝占忠,许林成.金属钆中钨的演化迁移行为与调控[J].有色金属:冶炼部分,2018(4):65-70. 被引量:2

6李国栋,刘永林.高纯金属钪的制备工艺及提纯机理研究[J].内蒙古大学学报:自然科学版,1997,28(5):614-618. 被引量:6

7杨庆山,陈建军,谢建秋,朱剑军.金属镝中杂质钨控制的研究[J].湖南冶金,2006,34(4):19-21. 被引量:3

8季永刚.金相制备对碳化钨涂层组织评定的影响[J].科技创业家,2012(15):94-95. 被引量:1

9邝子奇,代明江,熊国刚,刘敏,邓畅光,周克崧.钼基体上真空等离子体喷涂钨涂层的研究[J].真空科学与技术学报,2005,25(5):381-384. 被引量:9

10庞思明,王志强,周林,陈博雨,徐立海,赵斌,颜世宏,李宗安.稀土超磁致伸缩材料用高纯金属铽、镝的制备工艺研究[J].稀土,2008,29(6):31-35. 被引量:15

1王芦燕,李曹兵,张宇晴.射流分级技术在钨制品中的应用[J].热喷涂技术,2019,11(3):70-78. 被引量:4

2王文雯.基于高校辅导员工作的思想政治教育手段研究探析[J].课程教育研究,2019,0(38):71-71.

3孙学荣.小儿腺样体肥大与分泌性中耳炎相关性研究[J].临床研究,2014,22(9):14-14. 被引量:1

4王超,段立辉,张来启.原位合成SiC颗粒增强MoSi2基复合材料的900℃长期氧化行为[J].工程科学学报,2019,0(9):1168-1175. 被引量:4

5刘文彬,梁超,陈伟,王铁军,王磊,裴新军.航空航天用粉末钛合金的热等静压工艺研究[J].材料研究与应用,2019,13(3):229-235. 被引量:4

6曹明.基于ABAQUS的螺栓连接结合面仿真与研究[J].机床与液压,2019,47(20):164-169. 被引量:3

7潘月秀,方圆,韩大为,宋轶军,李龙,高建丽,朱世鹏,杨云华.炭纤维上浆剂对浮沉法体密度测试的影响[J].新型炭材料,2019,34(5):482-488.

8李迎春,邹春生,邱明,庞晓旭,程蓓.乏油环境下不同掺杂GLC膜的摩擦学行为[J].中国机械工程,2019,30(20):2431-2438.

9周孟娇,杨思彤,贾清秀.纤维素纳米晶材料研究进展[J].化工新型材料,2019,0(9):40-44. 被引量:6

10张志,曾贞,周健,刘创,杨水金.C/Bi2MoO6复合材料的合成及其可见光光催化性能研究[J].湖北大学学报:自然科学版,2019,41(6):636-643. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TB333[一般工业技术—材料科学与工程]

Citation Information:

Tungsten carbide layers with a certain thickness were in-situ synthesized on the surface of sintered tungsten products by high temperature heat treatment in carbon atmosphere protected by hydrogen gas to prepare WC/W surface composites.The effects of heat treatment temperature and tungsten matrix density on microstructure and properties of in-situ synthesized WC/W surface composites were studied by density and hardness test and metallographic microscope.The element composition and phase composition of tungsten carbide layers were analyzed by SEM/EDS and XRD.The results show that high temperature heat treatment temperature has significant influence on the growth thickness and quality of tungsten carbide layer,while tungsten matrix density has no obvious influence on the growth of tungsten carbide layer.When the temperature is lower than 1 800 ℃,the thickness of the tungsten carbide layer is relatively thin and its strength is poor.However,too high temperature will lead to an increase in defects of the tungsten carbide layer.The tungsten carbide layer in-situ synthesized on the surface of tungsten matrix has columnar crystal microstructure and single phase composition,closely combining with tungsten matrix,and the interface is clean and free of impurities.The surface composites can fully exhibit the excellent properties of the two materials at high temperature.

quote

GB/T 7714-2015 [1] HUANG Guang-hua, LIU Wei. Effects of Technological Conditions on Microstructure and Properties of In-situ Synthesized WC/W Surface Composites[J]. Rare Metals and Cemented Carbides, 2019(5): 7-13.
MLA [1] HUANG Guang-hua, and LIU Wei. "Effects of Technological Conditions on Microstructure and Properties of In-situ Synthesized WC/W Surface Composites." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 7-13.
APA [1] HUANG Guang-hua, & LIU Wei. (2019). Effects of Technological Conditions on Microstructure and Properties of In-situ Synthesized WC/W Surface Composites. Rare Metals and Cemented Carbides(5), 7-13.
IEEE [1] HUANG Guang-hua and LIU Wei, "Effects of Technological Conditions on Microstructure and Properties of In-situ Synthesized WC/W Surface Composites," Rare Metals and Cemented Carbides, no. 5, pp. 7-13, 2019. keywords: {surface composite;WC/W;in-situ synthesis;high temperature treatment;matrix density}