Development of New Ion-exchange Process in Tungsten Metallurgy AITranslate
Abstract AITranslate
In view of the low working capacity( penetrating capacity) ,low allowable concentration of WO3, Cl^- , OH^- in feed solution in ion exchange process, systematic study is made of the height difference of exchange zone and its adaptability to WO3, Cl^- , OH^- concentration of the modified resin. The results show that the property of the modified resin is remarkably better than that of the marketable resin 201 7 and the feed solution concentration of the commercial solution. A new ion exchange process is developed based on the new modified resin with equipment and operation concentration of the feed solution is doubled. process similar to that for the typical process and the concentration of the feed solution is doubled.
KeyWords AITranslate
1万林生,晏慧娟,肖学有,陈帮明,王辉.我国钨冶炼离子交换工艺的技术发展与工艺评价[J].中国钨业,2003,18(6):31-33. 被引量:20
2尹树普,侯利华.浅论湿冶离子交换工艺钨回收率[J].中国钨业,2004,19(3):34-35. 被引量:2
3赵中伟.用于处理高浓度钨酸钠溶液的离子交换新工艺[J].中国钨业,2005,20(1):33-35. 被引量:17
1赵中伟,方奇,李洪桂,霍广生,陈爱良.变参数离子交换的原理及其在钨冶金中的应用[J].稀有金属与硬质合金,2010,38(3):38-42. 被引量:2
2赵中伟,肖露萍,郭持皓,陈星宇,陈爱良,霍广生,李洪桂.Influence of earth gravity on reaction engineering of tubular reactor for high concentration tungsten ion-exchange[J].中国有色金属学报:英文版,2010,20(12):2379-2386. 被引量:3
3李洪桂,赵中伟.钨冶金强碱性阴离子交换过程的某些问题的理论分析[J].中国钨业,2010,25(5):35-39. 被引量:3
4王旭,廖春发.熔盐电解法制备金属钨粉的技术分析及发展前景[J].稀有金属,2011,35(4):587-592. 被引量:5
5关文娟,张贵清.用季铵盐从模拟钨矿苏打浸出液中直接萃取钨[J].中国有色金属学报,2011,21(7):1756-1762. 被引量:22
6万林生,孙丽,杨树生,陈玲,龚丹丹,李红超.钨冶炼溶液体系的非均匀化规律研究[J].稀有金属与硬质合金,2012,40(1):5-9.
7马运柱,刘业,刘文胜,龙路平,刘书华.高纯钨制备工艺的原理及其研究现状[J].稀有金属与硬质合金,2013,41(4):5-9. 被引量:6
8王明.钨冶炼离子交换工艺技术的研究进展[J].稀有金属与硬质合金,2013,41(6):13-16. 被引量:8
9赵中伟,杨茂峰,何利华,张家靓,陈星宇,刘旭恒.特性Na离子吸附剂的制备及其从钨酸铵溶液深度除钠(英文)[J].中国有色金属学报:英文版,2014,24(3):854-860. 被引量:2
10刘旭恒,胡芳,赵中伟.大孔型树脂处理高浓度钨酸钠溶液[J].中国有色金属学报,2014,24(7):1895-1900. 被引量:4
1Yuan-Lin Chen,Xue-Yi Guo,Qin-Meng Wang,Qing-Hua Tian,Shao-Bo Huang,Jin-Xiang Zhang.Tungsten and arsenic substance flow analysis of a hydrometallurgical process for tungsten extracting from wolframite[J].钨科技(英文),2021,3(3):348-360. 被引量:2
2王旭,廖春发.熔盐电解法制备金属钨粉的技术分析及发展前景[J].稀有金属,2011,35(4):587-592. 被引量:5
3叶章根,陈松,李文良,吴延科,王力军.熔盐电解精炼铪的研究[J].稀有金属,2012,36(5):791-798. 被引量:13
4柯兆华,张贵清,关文娟,尚广浩.季铵盐从碱性钨酸钠溶液中萃取钨的研究[J].稀有金属与硬质合金,2012,40(6):1-4. 被引量:10
5关文娟,张贵清,高从堦.蒸发脱氨络合法制备的双氧水络合萃取分离钨钼前驱体料液(英文)[J].中国有色金属学报:英文版,2013,23(4):1139-1146. 被引量:5
6关文娟,张贵清,高从堦,尚广浩.双氧水络合萃取分离钨钼的前驱体料液的制备[J].中南大学学报:自然科学版,2013,44(5):1766-1774. 被引量:4
7曾之琪,肖连生,张贵清.碱性钨萃余液返回高压浸出的试验研究[J].稀有金属与硬质合金,2013,41(6):1-6. 被引量:1
8张魁芳,曹佐英,张贵清,肖连生,周小舟.甲基碳酸酯季铵盐的合成、转型及萃取性能[J].中国有色金属学报,2013,23(12):3529-3536. 被引量:1
9李嘉豪,曹佐英,李嘉,张贵清,李青刚,曾理,关文娟.高级脂肪胺类萃取剂在稀有金属溶剂萃取中的应用[J].稀有金属与硬质合金,2018,46(6):10-18. 被引量:1
10刘旭恒,胡芳,赵中伟.大孔型树脂处理高浓度钨酸钠溶液[J].中国有色金属学报,2014,24(7):1895-1900. 被引量:4
1罗清平,郭朋成,杨志平,李存增,张海燕,陈亮,周敏,郎哲思,陈鹏,马宁,樊兴.用AI-9吸附剂从盐湖卤水中吸附锂的试验研究[J].湿法冶金,2012,31(3):152-154. 被引量:9
2邢学永,宁顺明,李斯佳.离子交换法从石煤直接酸浸液中提取钒的工艺研究[J].湿法冶金,2009,28(4):214-217. 被引量:17
3赵国惠(编译).在稀氯化物介质中利用水性臭氧浸出金和钯[J].黄金,2006,27(11):55-55.
4黄茜琳,李亮星,黄金堤,廖春发,童长仁.氯离子作用下N235对铋的萃取性能[J].有色金属科学与工程,2017,8(2):19-23. 被引量:1
5姜力强,张晓忠,毛信表,莫一平.超细镍粉电解制备工艺研究[J].材料科学与工艺,1999,7(1):87-92. 被引量:22
6蔡振春.高砷锑阳极铜电解生产始极片的实践[J].株冶科技,1999,27(4):6-8.
7蒋竹筠.东南钨公司仲钨酸铵的生产[J].中国有色冶金,1990,0(5):18-21.
8李剑锋.快速更换强力输送带效果好[J].煤矿机械,2005(7):89-89.
9郑清华,朱小坤.高钒铁生产系统铸件设备的改造[J].攀钢技术,1999,22(1):55-57.
10郑云.改善高速涡流探伤后交直流退磁效果的方法[J].冶金分析,2004(z2):618-621.
Basic Information:
DOI:
Chinese Library Classification Number:TF113.3[冶金工程—冶金物理化学]
Citation Information:
In view of the low working capacity( penetrating capacity) ,low allowable concentration of WO3, Cl^- , OH^- in feed solution in ion exchange process, systematic study is made of the height difference of exchange zone and its adaptability to WO3, Cl^- , OH^- concentration of the modified resin. The results show that the property of the modified resin is remarkably better than that of the marketable resin 201 7 and the feed solution concentration of the commercial solution. A new ion exchange process is developed based on the new modified resin with equipment and operation concentration of the feed solution is doubled. process similar to that for the typical process and the concentration of the feed solution is doubled.
quote
| GB/T 7714-2015 | [1] LI Hong-gui, LI Bo, ZHAO Zhong-wei. Development of New Ion-exchange Process in Tungsten Metallurgy[J]. Rare Metals and Cemented Carbides, 2007(1): 1-4. |
| MLA | [1] LI Hong-gui, et al., "Development of New Ion-exchange Process in Tungsten Metallurgy." Rare Metals and Cemented Carbides, no. 1, 2007, pp. 1-4. |
| APA | [1] LI Hong-gui, LI Bo, & ZHAO Zhong-wei. (2007). Development of New Ion-exchange Process in Tungsten Metallurgy. Rare Metals and Cemented Carbides(1), 1-4. |
| IEEE | [1] LI Hong-gui, LI Bo, and ZHAO Zhong-wei, "Development of New Ion-exchange Process in Tungsten Metallurgy," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2007. keywords: {tungsten metallurgy;ion exchange;ion exchange resin} |