daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of the Formation Process of Combustion-synthesized(Ti,W)C AITranslate

Department of Chemistry, Zhejiang University;Department of Chemistry, Zhejiang University;Department of Chemistry, Zhejiang University;Department of Chemistry, Zhejiang University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The phase composition and microstructures of the combustion-synthesized products with ratios of W/(Ti+W) of 0.4 and 0.54 in Ti-W-C system were studied.The kinetic high-temperature reaction process in the combustion front was analyzed through quenching of combustion front.The study results showed that there existed two reaction models.The first is defined as melt-solution-precipitation mechanism;Ti powder in the combustion front is molten at high combustion temperature,W and C are dissolved into liquid Ti,Ti-W-C melt is formed and (Ti,W)C is precipitated from the Ti-W-C melt.The second is described as diffusion-solution-in-solid state;when the combustion temperature is not high enough to melt Ti powder in the combustion front,C diffuses rapidly along cracks formed during combustion process and reacts with Ti to form TiC,meanwhile W 2C is formed and transformed to WC through C diffusion,then WC is dissolved into TiC to form(Ti,W)C.

KeyWords AITranslate

combustion synthesis (Ti W)C melting-solution-precipitation mechanism diffusion-solution-in solid state

1缪曙霞,殷声,李建勇,赖和怡.自蔓燃高温合成法(SHS)制备碳化钨[J].中国有色金属学报,1994,4(2):79-81. 被引量:6

2梁叔全,郑子樵.材料的自蔓延高温合成[J].硅酸盐学报,1993,21(3):261-271. 被引量:35

3李劲风,郑子樵,何国新,陶晓风.(W,Ti)C自蔓延高温合成[J].中南工业大学学报,1999,30(1):64-66. 被引量:3

4Li Jinfeng Zheng Ziqiao (Department of Materials Science and Engineering, Central South University of Technology, Changsha 410083, China) Zhang Zhao (Institute of Metallurgy Physicochemistry and Materials, Central South University of Technology,.SELF- PROPAGATING HIGH TEMPERATURE SYNTHESIS OF (W,Ti)C POWDERS[J].中南大学学报:英文版,1999,0(2):124-126. 被引量:3

1白鑫涛,王锦霞,谢宏伟,崔富辉,翟玉春.非传统TiC合成研究进展[J].有色金属科学与工程,2015,6(1):59-65. 被引量:2

2张正权,金永中,陈建,杨林,徐永琼,余明婷.纳米(Ti,50W)C固溶体粉末的制备研究[J].稀有金属与硬质合金,2016,44(3):29-31.

3卢蕾蓉,谭贤志,徐勇戈.基于协整理论的钼价格预测研究[J].稀有金属与硬质合金,2016,44(3):67-72. 被引量:1

4郑启文,杨天恩,熊计.(Ti,W)C固溶体基金属陶瓷的研究进展[J].硬质合金,2017,34(1):61-74. 被引量:5

5魏丹,罗铁钢,郑志斌,郑开宏,王娟,龙骏.原位合成(Ti,W)C增强高铬铸铁复合材料的形成过程及三体磨损性能[J].金属热处理,2020,45(7):153-158.

1杜军,杨吉哲,王尧.Zr/C纳米自蔓延反应薄膜制备及表征[J].表面技术,2016,45(8):98-102. 被引量:1

2刘文扬,张建波,陈婷婷,胡美俊.MAX/金属基自润滑复合材料摩擦学研究[J].有色金属科学与工程,2017,8(4):61-67. 被引量:3

3魏丹,罗铁钢,郑志斌,郑开宏,王娟,龙骏.原位合成(Ti,W)C增强高铬铸铁复合材料的形成过程及三体磨损性能[J].金属热处理,2020,45(7):153-158.

4边璐,王晓贺,张江朋,张璞.稀土产品价格决定:影响因素与预测方法综述[J].稀土,2020,41(4):146-158. 被引量:2

5马吉建.基于田口法的TN60刀具加工件表面质量影响因素的研究[J].硬质合金,2020,37(4):288-294.

6孙青竹,陈敏,张雪峰,王海波.WC对TiC基金属陶瓷显微组织和力学性能的影响[J].钢铁钒钛,2020,41(4):60-64. 被引量:1

7彭欣,高荣根,左锐.硬质相比例含量对Ti(C,N)基金属陶瓷微观组织和力学性能的影响[J].硬质合金,2021,38(1):16-22. 被引量:2

8梁艳,张立,李霞,余鹏,刘涛,凌群.钛、钨氧化物碳热还原-碳化的热力学和热分析[J].粉末冶金材料科学与工程,2021,26(2):91-98. 被引量:1

1李劲风,张昭,张鉴清,郑子樵,徐协文.W含量及预热温度对Ti-W-C体系燃烧合成产物的影响研究[J].稀有金属材料与工程,2002,31(1):64-68. 被引量:3

2李劲风,张昭,张鉴清.Ti-W-C体系燃烧合成产物颗粒形貌分析[J].粉末冶金技术,2002,20(2):71-74.

3李劲风,郑子樵,张昭,何国新,陶小风.Ti-W-C体系的自蔓延高温合成与反应机理[J].粉末冶金技术,2000,18(2):83-87. 被引量:5

4张守魁,王丹虹,赵红,苗华明.石英玻璃与铝液的反应[J].机械工程材料,2001,25(1):28-30. 被引量:9

5李兴田.聚酰胺6纳米复合材料的新进展[J].化学工业与工程技术,2001,22(2):29-30. 被引量:9

6王开东,常丽丽,王轶农,黄志青.搅拌摩擦加工技术制备Ti颗粒增强AZ31镁基复合材料[J].中国有色金属学报,2009,19(3):418-423. 被引量:10

7张耀宏.激冷Nd—Fe—B合金粉末的特性及其磁铁在汽车上的应用[J].国外汽车,1990(4):38-39.

8盛绍顶.热处理对硅增强粉末冶金AZ91镁基复合材料组织和性能的影响[J].热处理,2013,28(1):27-32. 被引量:2

9Binc.,GJ,兰力.铝工业炉渣的水激冷回收工艺简介[J].有色金属加工,1993(5):55-59.

10闫志巧,熊翔,肖鹏,李江鸿,黄伯云.Ta-C化合反应生成TaC的过程[J].稀有金属材料与工程,2006,35(A02):209-212. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:TF12[冶金工程—粉末冶金];TB39[一般工业技术—材料科学与工程]

Citation Information:

The phase composition and microstructures of the combustion-synthesized products with ratios of W/(Ti+W) of 0.4 and 0.54 in Ti-W-C system were studied.The kinetic high-temperature reaction process in the combustion front was analyzed through quenching of combustion front.The study results showed that there existed two reaction models.The first is defined as melt-solution-precipitation mechanism;Ti powder in the combustion front is molten at high combustion temperature,W and C are dissolved into liquid Ti,Ti-W-C melt is formed and (Ti,W)C is precipitated from the Ti-W-C melt.The second is described as diffusion-solution-in-solid state;when the combustion temperature is not high enough to melt Ti powder in the combustion front,C diffuses rapidly along cracks formed during combustion process and reacts with Ti to form TiC,meanwhile W 2C is formed and transformed to WC through C diffusion,then WC is dissolved into TiC to form(Ti,W)C.

quote

GB/T 7714-2015 [1] LI Jing-feng, ZHANG Zhao, ZHENG Zi-qiao, et al. Study of the Formation Process of Combustion-synthesized(Ti,W)C[J]. Rare Metals and Cemented Carbides, 2001(4): 1-6.
MLA [1] LI Jing-feng, et al., "Study of the Formation Process of Combustion-synthesized(Ti,W)C." Rare Metals and Cemented Carbides, no. 4, 2001, pp. 1-6.
APA [1] LI Jing-feng, ZHANG Zhao, ZHENG Zi-qiao, & XU Xie-wen. (2001). Study of the Formation Process of Combustion-synthesized(Ti,W)C. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] LI Jing-feng, ZHANG Zhao, ZHENG Zi-qiao, and XU Xie-wen, "Study of the Formation Process of Combustion-synthesized(Ti,W)C," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 2001. keywords: {combustion synthesis;(Ti,W)C;melting-solution-precipitation mechanism;diffusion-solution-in solid state}