Discussion on Soda Autoclaving Process for Treatment of Tungsten Ore AITranslate
Abstract AITranslate
The Paper describes the analysis and demonstration of NaOH substitution for some soda;soda solution initial concentratoon and min.temperature during dissolution,etc in soda autoclaving of tungsten ore.Some helpful conclusions are drawn.
KeyWords AITranslate
1叶帷洪.钨:资源、冶金、性质和用途[M].北京:冶金工业出版社,1983.102.
2Arriagada F J.白钨矿的高温溶解[J].有色金属:冶炼部分,1986,1:57-57.
3吴厚荣.复杂钨中矿的分解[J].有色冶炼,1985,14(8):33-33.
4AЛekceB A И.NaO2-CaO-CO2-H2O系中平衡过程的热力学和实验结果分析[J].轻金属,1986,1:14-14.
5吴鼎泉,胥正亮,屈松生.钨酸钠水溶液的活度系数和渗透系数[J].物理化学学报,1990,6(5):633-637. 被引量:1
6ЗeЛИkMaH A H 李汉广等(译).钨[M].长沙:中南矿冶学院科技情报科,1981.26.
1任慧川,唐忠阳,刘旭恒.钨湿法冶金工艺进展[J].稀有金属与硬质合金,2019,47(3):1-8. 被引量:1
1薛祥,张新英,杨亮.磷酸钠-氢氧化钠浸出氟化钙动力学研究[J].有色金属科学与工程,2021,12(1):8-12. 被引量:2
1宁华.苏打压煮钨矿工艺及其发展[J].稀有金属与硬质合金,1996,24(4):44-48. 被引量:4
2李伟勤,戴普.用高钼白钨精矿制取高纯三氧化钨工艺实践[J].中国钨业,2001,16(1):35-38. 被引量:3
3何立新,李洪桂,任洪九.离子交换法处理苏打压煮钨矿母液的研究[J].中国钨业,1996,11(1):16-20. 被引量:1
4赵中伟,李洪桂,孙培梅,刘茂盛,李运姣.一种特殊情况下的动力学参数测定方法研究[J].稀有金属与硬质合金,1993,21(S1):259-263. 被引量:1
5芦广超,陈伟,闫小林.T型中间包温度场数值模拟[J].河北理工大学学报:自然科学版,2011,33(3):38-41. 被引量:1
6黄坤林.调整碱压煮工艺参数 提高复杂钨矿分解率[J].硬质合金,2004,21(1):36-38.
7何立新,李洪桂,任鸿九.离子交换法处理钨矿物原料苏打压煮母液的研究[J].中南工业大学学报,1995,26(6):761-765. 被引量:7
8方觉,宋建新,高艳甲,李金龙,张波.球团矿氧化焙烧试验研究[J].钢铁研究,2012,40(4):11-13. 被引量:2
9吴雨晨,闫小林,李俊国,曾亚南,李守章.1700板坯中间包温度场的数值模拟及其优化[J].河北理工大学学报:自然科学版,2009,31(3):34-38. 被引量:7
10代传民,雷洪,毕乾,耿佃桥,陈洪民,赵岩.通道式感应加热中间包的数值模拟[J].炼钢,2015,31(4):54-58. 被引量:11
Basic Information:
DOI:
Chinese Library Classification Number:TF111.31[冶金工程—冶金物理化学]
Citation Information:
The Paper describes the analysis and demonstration of NaOH substitution for some soda;soda solution initial concentratoon and min.temperature during dissolution,etc in soda autoclaving of tungsten ore.Some helpful conclusions are drawn.
quote
| GB/T 7714-2015 | [1] ZHAO Zhong-wei, YANG Jin-hong. Discussion on Soda Autoclaving Process for Treatment of Tungsten Ore[J]. Rare Metals and Cemented Carbides, 2002(2): 1-3. |
| MLA | [1] ZHAO Zhong-wei, and YANG Jin-hong. "Discussion on Soda Autoclaving Process for Treatment of Tungsten Ore." Rare Metals and Cemented Carbides, no. 2, 2002, pp. 1-3. |
| APA | [1] ZHAO Zhong-wei, & YANG Jin-hong. (2002). Discussion on Soda Autoclaving Process for Treatment of Tungsten Ore. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] ZHAO Zhong-wei and YANG Jin-hong, "Discussion on Soda Autoclaving Process for Treatment of Tungsten Ore," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 2002. keywords: {soda autoclave;tungsten ore;leaching;thermodynamics} |