Abstract AITranslate

Since the development of porous materials, porous organic polymers (POPs) have received much attention due to advantages such as attractive architecture, large pore volume, high surface area, and immense porosity. Furthermore, their porous structure can be functionalized with multiple chemical reagents, which will improve their performances in various applications. In the past, significant efforts have been made to synthesize POPs via Friedel–Crafts reaction. It is easy to handle and operates under mild synthesis conditions, requires low reaction temperature, uses considerably less expensive chemicals, and produces high-yield POPs with desirable surface areas. POPs prepared via this method act competitively in various fields. This review focuses on the recent applications of the POPs introduced in gas adsorption and separation, catalyst, water treatment, biomedical, and electrochemical applications, aiming to pave the way for researchers to develop new POPs for modern applications.

KeyWords AITranslate

porous organic polymers Friedel−Crafts reaction irreversible reaction gas adsorption water treatment covalent organic polymers Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00927

Chinese Library Classification Number:

Citation Information:

Since the development of porous materials, porous organic polymers (POPs) have received much attention due to advantages such as attractive architecture, large pore volume, high surface area, and immense porosity. Furthermore, their porous structure can be functionalized with multiple chemical reagents, which will improve their performances in various applications. In the past, significant efforts have been made to synthesize POPs via Friedel–Crafts reaction. It is easy to handle and operates under mild synthesis conditions, requires low reaction temperature, uses considerably less expensive chemicals, and produces high-yield POPs with desirable surface areas. POPs prepared via this method act competitively in various fields. This review focuses on the recent applications of the POPs introduced in gas adsorption and separation, catalyst, water treatment, biomedical, and electrochemical applications, aiming to pave the way for researchers to develop new POPs for modern applications.

quote

GB/T 7714-2015 [1] Nazanin Taheri, Mohammad Dinari, Mehrdad Asgari. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00927.
MLA [1] Nazanin Taheri, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00927.
APA [1] Nazanin Taheri, Mohammad Dinari, & Mehrdad Asgari. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00927
IEEE [1] Nazanin Taheri, Mohammad Dinari, and Mehrdad Asgari, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00927. keywords: {porous organic polymers;Friedel−Crafts reaction;irreversible reaction;gas adsorption;water treatment;covalent organic polymers;Show More}
+ titleDiv +`

`+ journalName + `

` + publish + `: ` + paperItem.year + `

`; newHtmlContent = newHtmlContent + paperDivString; } newHtmlContent = newHtmlContent + '
'; for (var i = 4; i < paperList.length; i++) { let paperItem = paperList[i]; let indexString = "[" + (i+1) + "]"; let hrefString = baseUrl + "paper/" + paperItem.contentId + `?webId=` + paperItem.webId; let title = ''; let journalName = ''; if (isEnglish) { title = paperItem.englishTitle != null ? paperItem.englishTitle : paperItem.chineseTitle; journalName = paperItem.journalNameEn != null ? paperItem.journalNameEn : paperItem.journalName; }else { title = paperItem.chineseTitle != null ? paperItem.chineseTitle : paperItem.englishTitle; journalName = paperItem.journalName != null ? paperItem.journalName : paperItem.journalNameEn; } if (!title || title.length == 0) { title = paperItem.title; } let titleDiv = `` + title +``; let paperDivString = ``; newHtmlContent = newHtmlContent + paperDivString; } newHtmlContent = newHtmlContent + `
` + showMore +``; }else { for (var i = 0; i < paperList.length; i++) { let paperItem = paperList[i]; let indexString = "[" + (i+1) + "]"; let hrefString = baseUrl + "paper/" + paperItem.contentId + `?webId=` + paperItem.webId; let title = ''; let journalName = ''; if (isEnglish) { title = paperItem.englishTitle != null ? paperItem.englishTitle : paperItem.chineseTitle; journalName = paperItem.journalNameEn != null ? paperItem.journalNameEn : paperItem.journalName; }else { title = paperItem.chineseTitle != null ? paperItem.chineseTitle : paperItem.englishTitle; journalName = paperItem.journalName != null ? paperItem.journalName : paperItem.journalNameEn; } if (!title || title.length == 0) { title = paperItem.title; } let titleDiv = `` + title +``; let paperDivString = ``; newHtmlContent = newHtmlContent + paperDivString; } } element.innerHTML=newHtmlContent; } function clickMoreLikeMoreBtnAction() { event.preventDefault(); // 防止跳转 event.stopPropagation(); // 阻止事件冒泡,防止触发全局a点击逻辑 var btn = event.target; var nav = btn.previousElementSibling; let showMore = isEnglish ? "Show More" : "展示更多"; let hide = isEnglish ? "Hide" : "收起"; if (nav && nav.classList.contains("more_nav")) { var isActive = nav.classList.toggle("active"); // 切换展开/折叠 btn.textContent = isActive ? hide : showMore; // 改文字 } }