Luminescent Solar Concentrators Based on Energy Transfer from an Aggregation-Induced Emitter Conjugated Polymer AITranslate

University of Cambridge; University of Cambridge; University of Cambridge;Macromolecular Chemistry Group (buwmakro) and Institute for Polymer Technology;Macromolecular Chemistry Group (buwmakro) and Institute for Polymer Technology;Macromolecular Chemistry Group (buwmakro) and Institute for Polymer Technology; Université de Montpellier; University of Cambridge
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Luminescent solar concentrators (LSCs) are solar-harvesting devices fabricated from a transparent waveguide that is doped or coated with lumophores. Despite their potential for architectural integration, the optical efficiency of LSCs is often limited by incomplete harvesting of solar radiation and aggregation-caused quenching (ACQ) of lumophores in the solid state. Here, we demonstrate a multilumophore LSC design that circumvents these challenges through a combination of nonradiative Förster resonance energy transfer (FRET) and aggregation-induced emission (AIE). The LSC incorporates a green-emitting poly(tetraphenylethylene), p-O-TPE, as an energy donor and a red-emitting perylene bisimide molecular dye (PDI-Sil) as the energy acceptor, within an organic–inorganic hybrid diureasil waveguide. Steady-state photoluminescence studies demonstrate the diureasil host induced AIE from the p-O-PTE donor polymer, leading to a high photoluminescence quantum yield (PLQY) of ∼45% and a large Stokes shift of ∼150 nm. Covalent grafting of the PDI-Sil acceptor to the siliceous domains of the diureasil waveguide also inhibits nonradiative losses by preventing molecular aggregation. Due to the excellent spectral overlap, FRET was shown to occur from p-O-TPE to PDI-Sil, which increased with acceptor concentration. As a result, the final LSC (4.5 cm × 4.5 cm × 0.3 cm) with an optimized donor–acceptor ratio (1:1 by wt %) exhibited an internal photon efficiency of 20%, demonstrating a viable design for LSCs utilizing an AIE-based FRET approach to improve the solar-harvesting performance.

KeyWords AITranslate

aggregationinduced emission conjugated polymer energy transfer organic−inorganic hybrid luminescent solar concentrator
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00718

Chinese Library Classification Number:

Citation Information:

Luminescent solar concentrators (LSCs) are solar-harvesting devices fabricated from a transparent waveguide that is doped or coated with lumophores. Despite their potential for architectural integration, the optical efficiency of LSCs is often limited by incomplete harvesting of solar radiation and aggregation-caused quenching (ACQ) of lumophores in the solid state. Here, we demonstrate a multilumophore LSC design that circumvents these challenges through a combination of nonradiative Förster resonance energy transfer (FRET) and aggregation-induced emission (AIE). The LSC incorporates a green-emitting poly(tetraphenylethylene), p-O-TPE, as an energy donor and a red-emitting perylene bisimide molecular dye (PDI-Sil) as the energy acceptor, within an organic–inorganic hybrid diureasil waveguide. Steady-state photoluminescence studies demonstrate the diureasil host induced AIE from the p-O-PTE donor polymer, leading to a high photoluminescence quantum yield (PLQY) of ∼45% and a large Stokes shift of ∼150 nm. Covalent grafting of the PDI-Sil acceptor to the siliceous domains of the diureasil waveguide also inhibits nonradiative losses by preventing molecular aggregation. Due to the excellent spectral overlap, FRET was shown to occur from p-O-TPE to PDI-Sil, which increased with acceptor concentration. As a result, the final LSC (4.5 cm × 4.5 cm × 0.3 cm) with an optimized donor–acceptor ratio (1:1 by wt %) exhibited an internal photon efficiency of 20%, demonstrating a viable design for LSCs utilizing an AIE-based FRET approach to improve the solar-harvesting performance.

quote

GB/T 7714-2015 [1] Guanpeng Lyu, James Kendall, Ilaria Meazzini, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00718.
MLA [1] Guanpeng Lyu, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00718.
APA [1] Guanpeng Lyu, James Kendall, Ilaria Meazzini, Eduard Preis, Sebnem Bayseç, Ullrich Scherf, Sébastien Clément, & Rachel C. Evans. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00718
IEEE [1] Guanpeng Lyu, James Kendall, Ilaria Meazzini, Eduard Preis, Sebnem Bayseç, Ullrich Scherf, Sébastien Clément, and Rachel C. Evans, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00718. keywords: {aggregationinduced emission;conjugated polymer;energy transfer;organic−inorganic hybrid;luminescent solar concentrator}