Current Research of Mg-Gd-Y-Zr Heat-resistant Magnesium Alloys AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of alloying elements, strengthening approaches and mechanisms, current research of mechanical properties, heat treatment and aging precipitation behavior of Mg-Gd-Y-Zr alloys are introduced and their future development is forecasted.

KeyWords AITranslate

Mg-Gd-Y-Zr alloy heat-resistance mechanical property solid solution strengthening aging pre-cipitation

1Friedrich H E, Mordike B L. Magnesium technology= metallurgy, design data, applications [M]. New York: Springer,2006.

2Mordike B L, Ebert T. Magnesium: properties-applica tions-potential[J]. Materials Science and Engineering A, 2001,302(1) :37-45.

3曾荣昌,柯伟,徐永波,韩恩厚,朱自勇.Mg合金的最新发展及应用前景[J].金属学报,2001,37(7):673-685. 被引量:439

4Nayeb-Hashemi A A,Clark J B. Phase diagrams of bina- ry magnesium alloys [M]. Ohio: ASM International, 1988.

5Nie J F, Gao X, Zhu S M. Enhanced age hardening re- sponse and creep resistance of Mg-Gd alloys containing Zn[J]. Scripta Materialia, 2005,53:1 049-1 053.

6彭卓凯,张新明,陈健美,肖阳,蒋浩,邓桢桢.Mn,Zr对Mg-Gd-Y合金组织与力学性能的影响[J].中国有色金属学报,2005,15(6):917-922. 被引量:49

7孙明,吴国华,王玮,侯正全,陈斌,丁文江.Mg-Gd系镁合金的研究进展[J].材料导报,2009,23(11):98-103. 被引量:26

8Emley E F. Principles of magnesium technology [ M]. New York : Pergamon Press, 1966. 126-127.

9石德珂.位错与材料强度[M].西安:西安交通大学出版社,1986.90-120.

10Xiao B L,Yang Q,Yang J,et al. Enhanced mechanical properties of Mg-Gd-Y-Zr casting via friction stir pro cessing[J]. Journal of Alloys and Compounds, 2011, 509(6):2 879-2 884.

1李全安,陈志,程彬,周伟.Gd对Mg?Gd?Y?Sm?Zr系稀土镁合金显微组织和抗腐蚀性能的影响[J].稀有金属与硬质合金,2013,41(4):26-29. 被引量:4

2鲍叶琳,刘鹏宇.电感耦合等离子体原子发射光谱法(ICP-AES)测定稀土镁合金中锆[J].中国无机分析化学,2013,3(B10):83-85. 被引量:6

3邓璘.车用Mg-Gd-Nd-Sb-Zr合金高温蠕变行为及组织演变研究[J].兵器材料科学与工程,2017,40(2):65-68.

4杨晶晶,唐显升,谢江怀,莫玉梅.Mg-5Gd-3Y-0.8Zr合金的微观组织及耐NaCl溶液腐蚀性能研究[J].粉末冶金工业,2017,27(5):32-35. 被引量:4

5翟声明,王翔,冯霖,孙亚丽.电感耦合等离子体原子发射光谱(ICP-AES)法测定稀土镁合金中钆[J].中国无机分析化学,2022,12(2):76-80. 被引量:4

6唐昌平,成声亮,李国栋.固溶处理对Mg-Gd-Y-Nd-Zr合金挤压板材组织与织构的影响[J].材料科学,2016,6(5):277-284.

1李金宝,周古昕,杨润田,杜秀征,王生,郎玉婧,乔丽,毛华.轧态Mg-Gd-Y-Zr合金显微组织及耐腐蚀性能研究[J].兵器材料科学与工程,2020,0(2):42-47. 被引量:4

2曹爱青.直读光谱法测定海洋结构用钢中的锆[J].中国无机分析化学,2014,4(3):61-63.

3江民华.稀土元素Sm对AM60镁合金显微组织和耐腐蚀性能的影响[J].热加工工艺,2015,44(4):86-89. 被引量:7

4田永红,刘海生.电感耦合等离子体原子发射光谱法(ICP-AES)测定5XXX系铝合金中的高镁含量[J].中国无机分析化学,2015,5(2):62-64. 被引量:3

5卢文琪,张春兰,谢芬.ICP-AES法测定镁及镁合金中的锆[J].广州化工,2015,43(22):128-129.

6万晓东,冀克俭,赵华,李本涛,黄辉,李颖,巩琛,郝淑杰.电感耦合等离子体发射光谱法测定稀土发火合金中铁、镁、铜和锌[J].化学分析计量,2017,26(6):75-77. 被引量:3

7田春霞,刘文华,刘璟.稀土元素分析[J].分析试验室,2018,37(2):222-248. 被引量:13

8王文乐,季惠,张鹏程.拉伸温度对快速凝固Mg-8Zn-0.5Y合金组织和性能的影响[J].粉末冶金工业,2018,28(3):40-43. 被引量:4

9张帅,李全安,朱宏喜,陈晓亚.Mg-Gd-Y系镁合金的腐蚀与防护研究进展[J].材料保护,2019,0(8):158-165. 被引量:4

10魏竞智,郭磊磊,李徐凤.石墨炉原子吸收光谱法和电感耦合等离子体发射光谱法测定土壤中铅和镉的方法比较[J].中国卫生检验杂志,2020,30(7):797-801. 被引量:7

1黄德明,刘红梅,陈云贵,唐永柏,涂铭旌.耐热铸造镁合金的研究应用进展[J].轻金属,2005(8):49-54. 被引量:13

2许利军.提高烧结机台车炉篦条使用寿命的材质研究[J].湖南冶金,2002,30(1):12-14. 被引量:2

3程和法.高韧性铁素体球铁冷却壁耐热性能的研究[J].鞍钢技术,1996(10):14-17. 被引量:1

4程和法,陈其善,连金江.铁素体球铁高炉冷却壁的试验研究[J].现代铸铁,1994,0(2):6-9. 被引量:2

5胡本芙,尹法章,贾成厂,金开生,李慧英.热处理工艺对热挤压变形粉末高温合金FGH95组织与性能的影响[J].北京科技大学学报,2006,28(12):1121-1125. 被引量:6

6崔成松,范洪波,来忠红,沈军,蒋祖龄,李庆春.喷射沉积Al-3.8Li-0.8Mg-0.4Cu-0.13Zr合金的显微组织与拉伸性能[J].中国有色金属学报,1996,6(4):127-131. 被引量:5

7王勇.钢的化学热处理(上)[J].山东农机化,2004(10):18-18.

8崔建忠,胡卫民,卢连大,马龙翔.8090A1合金的时效析出[J].东北工学院学报,1990,11(1):40-45.

9何秋梅,何良胜.Al_2O_3-CeO_2-ZrO_2-Ni复合球磨粉末的热稳定性研究[J].热处理,2008,23(5):55-58.

10詹美燕,陈振华,夏伟军.8009耐热铝合金薄板高温组织与性能的研究[J].材料工程,2004,32(3):35-37. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF146.22[冶金工程—冶金物理化学]

Citation Information:

The effects of alloying elements, strengthening approaches and mechanisms, current research of mechanical properties, heat treatment and aging precipitation behavior of Mg-Gd-Y-Zr alloys are introduced and their future development is forecasted.

quote

GB/T 7714-2015 [1] ZHOU Wei, LI Quan-an, KANG Hai-juan, et al. Current Research of Mg-Gd-Y-Zr Heat-resistant Magnesium Alloys[J]. Rare Metals and Cemented Carbides, 2012(5): 51-56.
MLA [1] ZHOU Wei, et al., "Current Research of Mg-Gd-Y-Zr Heat-resistant Magnesium Alloys." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 51-56.
APA [1] ZHOU Wei, LI Quan-an, KANG Hai-juan, & WANG Yao-gui. (2012). Current Research of Mg-Gd-Y-Zr Heat-resistant Magnesium Alloys. Rare Metals and Cemented Carbides(5), 51-56.
IEEE [1] ZHOU Wei, LI Quan-an, KANG Hai-juan, and WANG Yao-gui, "Current Research of Mg-Gd-Y-Zr Heat-resistant Magnesium Alloys," Rare Metals and Cemented Carbides, no. 5, pp. 51-56, 2012. keywords: {Mg-Gd-Y-Zr alloy;heat-resistance;mechanical property;solid solution strengthening;aging pre-cipitation}