daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Xanthate-Type Photofunctional Chain Transfer Agent for the Synthesis of Macrophotoinitiators AITranslate

Harran University; Harran University; Harran University; Harran University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polystyrene (PSt), poly(methyl methacrylate) (PMMA), and poly(vinyl acetate) (PVAc) macrophotoinitiators with well-defined structures comprising a photoreactive group, benzoin (B), at the chain end were successfully synthesized by RAFT/MADIX polymerization. First, a photofunctional xanthate-type chain transfer agent (B-CTA) was produced by an efficient two-step one-pot synthesis. Then, B-CTA was used in the RAFT/MADIX polymerization of styrene (St), methyl methacrylate (MMA), acrylonitrile (AN) (more activated monomers), and vinyl acetate (VAc) (a less activated monomer). Based on spectral and GPC data, the RAFT/MADIX polymerizations of St, MMA, and VAc monomers produced well-controlled macrophotoinitiators with narrow molecular weight distributions and compatible theoretical and experimental number-average molecular weights. The resulting well-defined macrophotoinitiators, B-PSt, B-PMMA, and B-PAVc, were used as precursors to obtain block copolymers PSt-b-PCHO, PMMA-b-PCHO, PVAc-b-PCHO from cyclohexene oxide (CHO) and PSt-b-PBVE, PMMA-b-PBVE, PVAc-b-PBVE from butyl vinyl ether (BVE) monomers, respectively, via photoinduced free radical promoted cationic polymerization. Various analyses such as elemental, spectroscopic, and GPC techniques were used to confirm the structures of the synthesized molecules.

KeyWords AITranslate

xanthatetype CTA macrophotoinitiator RAFT/MADIX polymerization polystyrene poly(methyl methacrylate) poly(vinyl acetate) Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01495

Chinese Library Classification Number:

Citation Information:

Polystyrene (PSt), poly(methyl methacrylate) (PMMA), and poly(vinyl acetate) (PVAc) macrophotoinitiators with well-defined structures comprising a photoreactive group, benzoin (B), at the chain end were successfully synthesized by RAFT/MADIX polymerization. First, a photofunctional xanthate-type chain transfer agent (B-CTA) was produced by an efficient two-step one-pot synthesis. Then, B-CTA was used in the RAFT/MADIX polymerization of styrene (St), methyl methacrylate (MMA), acrylonitrile (AN) (more activated monomers), and vinyl acetate (VAc) (a less activated monomer). Based on spectral and GPC data, the RAFT/MADIX polymerizations of St, MMA, and VAc monomers produced well-controlled macrophotoinitiators with narrow molecular weight distributions and compatible theoretical and experimental number-average molecular weights. The resulting well-defined macrophotoinitiators, B-PSt, B-PMMA, and B-PAVc, were used as precursors to obtain block copolymers PSt-b-PCHO, PMMA-b-PCHO, PVAc-b-PCHO from cyclohexene oxide (CHO) and PSt-b-PBVE, PMMA-b-PBVE, PVAc-b-PBVE from butyl vinyl ether (BVE) monomers, respectively, via photoinduced free radical promoted cationic polymerization. Various analyses such as elemental, spectroscopic, and GPC techniques were used to confirm the structures of the synthesized molecules.

quote

GB/T 7714-2015 [1] Zafer Uyar, Ulku Arslan, Tugce Yuce Boyraz, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01495.
MLA [1] Zafer Uyar, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01495.
APA [1] Zafer Uyar, Ulku Arslan, Tugce Yuce Boyraz, & Mustafa Degirmenci. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01495
IEEE [1] Zafer Uyar, Ulku Arslan, Tugce Yuce Boyraz, and Mustafa Degirmenci, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01495. keywords: {xanthatetype CTA;macrophotoinitiator;RAFT/MADIX polymerization;polystyrene;poly(methyl methacrylate);poly(vinyl acetate);Show More}