Study on Microstructure and Properties of W-20%Cu Composite Material Prepared by SPS AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

W-20%Cu composite material was successfully prepared by SPS with W-20%Cu(mass fraction)composite powders as raw materials obtained by hydrothermal synthesis-coreduction,and its microstructure and properties were analyzed and studied.The results show that with the increase of sintering temperature and heat preservation time,microstructure distribution of W and Cu is more uniform with less porosity,and density,hardness and electrical conductivity of W-20%Cu composite material are subsequently increased.Under the conditions of sintering temperature 950 ℃ and heat preservation time 5min,the density,hardness and electrical conductivity of W-20%Cu composite material are 98.9%,HV222.8and 21.7 MS/m,respectively.

KeyWords AITranslate

hydrothermal synthesis-coreduction spark plasma sintering W-20%Cu composite material property microstructure

1章桥新.Microstructure and Properties of W-15Cu Alloys Prepared by Mechanical Alloying and Spark Plasma Sintering Process[J].武汉理工大学学报:材料科学英文版,2008,23(3):399-402. 被引量:2

2张久兴,张忻,岳明,周美玲,左铁镛.放电等离子烧结技术与新材料研究[J].功能材料信息,2004,1(3):14-21. 被引量:10

3冯海波,周玉,贾德昌.放电等离子烧结技术的原理及应用[J].材料科学与工艺,2003,11(3):327-331. 被引量:61

4张久兴,刘科高,周美玲.放电等离子烧结技术的发展和应用[J].粉末冶金技术,2002,20(3):129-134. 被引量:142

5Qiaoxin Zhang,Xiaoliang Shi,Hua Yang,Xinglong Duan.Microstructure and properties of W-15Cu alloys prepared by mechanical alloying and spark plasma sintering process[J]. Journal of Wuhan University of Technology - Mater. Sci. Ed. . 2008 (3)

6I. Sabirov,R. Pippan.Formation of a W–25%Cu nanocomposite during high pressure torsion[J]. Scripta Materialia . 2005 (12)

7Dae-Gun Kim,Gil-Su Kim,Myung-Jin Suk,Sung-Tag Oh,Young Do Kim.Effect of heating rate on microstructural homogeneity of sintered W–15wt%Cu nanocomposite fabricated from W–CuO powder mixture[J]. Scripta Materialia . 2004 (7)

8S.S Ryu,Y.D Kim,I.H Moon.Dilatometric analysis on the sintering behavior of nanocrystalline W–Cu prepared by mechanical alloying[J]. Journal of Alloys and Compounds . 2002 (1)

9Hungria T.,Castro A.,Galy J.Spark plasma sintering as a useful technique to the nanostructuration of piezo-ferroelectric materials. Advanced Engineering Materials . 2009

1李剑,马尧,梁力行,王海龙,张锐.放电等离子烧结聚晶立方氮化硼刀具的性能[J].机械工程材料,2019,43(1):8-12. 被引量:1

1林芳芳.WC-B-Al_(2)O_(3)作结合剂的聚晶立方氮化硼复合材料性能研究[J].矿冶工程,2022,42(4):164-166. 被引量:3

1刘涛,范景莲,成会朝,田家敏.W-20%Cu超细复合粉末的制备和烧结[J].粉末冶金技术,2007,25(4):259-261. 被引量:9

2张福斌,胡艳玲,胡业奇,许龙山,胡柏新.溶胶凝胶法制备超细W-Ag复合粉末[J].粉末冶金工业,2015,25(1):14-18. 被引量:4

3范景莲,刘军,严德剑,黄伯云.细晶钨铜复合材料制备工艺的研究[J].粉末冶金技术,2004,22(2):83-86. 被引量:46

4张迎晖,田海霞,朱根松,秦镜.碳纳米管对W-Cu复合材料致密度和硬度的影响[J].有色金属科学与工程,2012,3(3):33-35.

5Р.,ОГ.带入杂质沿变形时低合金化钨合金组织的再分布[J].钨钼材料,1993(2):35-38.

6董长升.掺杂三氧化二钕对钼丝显微组织和性能影响的研究[J].稀有金属材料与工程,1994,23(6):46-51. 被引量:1

7汪峰涛,吴玉程,王涂根,任榕.W-Cu纳米晶粉体的制备及表征[J].功能材料,2007,38(A06):2062-2065. 被引量:1

8陈春浩,薛丽红,史昆玉,沈涛,严有为,李乃湖,李慧杰.高能球磨时间对W-Cu纳米晶复合粉体组织和性能的影响[J].粉末冶金材料科学与工程,2011,16(6):832-836. 被引量:4

9朱旺喜.外刊科技文摘[J].中国钨业,1994,0(11):34-35.

10胡保全,白培康,程军.机械合金化法制备低质量分数Mo-Cu合金[J].功能材料,2010,41(5):837-839. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF124.5[冶金工程—粉末冶金]

Citation Information:

W-20%Cu composite material was successfully prepared by SPS with W-20%Cu(mass fraction)composite powders as raw materials obtained by hydrothermal synthesis-coreduction,and its microstructure and properties were analyzed and studied.The results show that with the increase of sintering temperature and heat preservation time,microstructure distribution of W and Cu is more uniform with less porosity,and density,hardness and electrical conductivity of W-20%Cu composite material are subsequently increased.Under the conditions of sintering temperature 950 ℃ and heat preservation time 5min,the density,hardness and electrical conductivity of W-20%Cu composite material are 98.9%,HV222.8and 21.7 MS/m,respectively.

quote

GB/T 7714-2015 [1] ZHAO Jing-jing, LI Ji-wen, ZHANG Pan-long, et al. Study on Microstructure and Properties of W-20%Cu Composite Material Prepared by SPS[J]. Rare Metals and Cemented Carbides, 2015(2): 17-21.
MLA [1] ZHAO Jing-jing, et al., "Study on Microstructure and Properties of W-20%Cu Composite Material Prepared by SPS." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 17-21.
APA [1] ZHAO Jing-jing, LI Ji-wen, ZHANG Pan-long, & WEI Shi-zhong. (2015). Study on Microstructure and Properties of W-20%Cu Composite Material Prepared by SPS. Rare Metals and Cemented Carbides(2), 17-21.
IEEE [1] ZHAO Jing-jing, LI Ji-wen, ZHANG Pan-long, and WEI Shi-zhong, "Study on Microstructure and Properties of W-20%Cu Composite Material Prepared by SPS," Rare Metals and Cemented Carbides, no. 2, pp. 17-21, 2015. keywords: {hydrothermal synthesis-coreduction;spark plasma sintering;W-20%Cu composite material;property;microstructure}