We report the design and synthesis of a class of hybrid latex particle that combines the elastomeric properties of polyolefins with the physicochemical diversity of acrylics. These hybrid polyolefin–acrylic particles are obtained in two steps, starting from the mechanical dispersion of a polyolefin resin to yield a colloidally stable particle dispersion, which is then used in a second step as a seed for the free radical emulsion polymerization of an acrylic phase. Imaging of the resulting particles by scanning electron and atomic force microscopy reveals a distinct lobed morphology, where acrylic polymer is associated with the surface of the polyolefin dispersion. Using gel permeation chromatography (GPC), we quantify the degree of grafting between the core and the acrylic phase, while analysis by dynamic mechanical analysis (DMA) shows that key properties of the polyolefin remain unaffected by the emulsion polymerization process. Process changes including varying the polyolefin/acrylic ratio, monomer addition method, initiator type, and acrylic composition can be used to control the surface coverage and size of the acrylic lobes, and therefore tune the particle morphology. This approach is modular both in terms of the polyolefin materials and additives that can be used to fabricate the core, as well as the physicochemical properties of the acrylic phase (composition, glass transition temperature, chemical functionality, etc.) and provides opportunities to design hybrid particles for a range of advanced applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00848
Chinese Library Classification Number:
Citation Information:
We report the design and synthesis of a class of hybrid latex particle that combines the elastomeric properties of polyolefins with the physicochemical diversity of acrylics. These hybrid polyolefin–acrylic particles are obtained in two steps, starting from the mechanical dispersion of a polyolefin resin to yield a colloidally stable particle dispersion, which is then used in a second step as a seed for the free radical emulsion polymerization of an acrylic phase. Imaging of the resulting particles by scanning electron and atomic force microscopy reveals a distinct lobed morphology, where acrylic polymer is associated with the surface of the polyolefin dispersion. Using gel permeation chromatography (GPC), we quantify the degree of grafting between the core and the acrylic phase, while analysis by dynamic mechanical analysis (DMA) shows that key properties of the polyolefin remain unaffected by the emulsion polymerization process. Process changes including varying the polyolefin/acrylic ratio, monomer addition method, initiator type, and acrylic composition can be used to control the surface coverage and size of the acrylic lobes, and therefore tune the particle morphology. This approach is modular both in terms of the polyolefin materials and additives that can be used to fabricate the core, as well as the physicochemical properties of the acrylic phase (composition, glass transition temperature, chemical functionality, etc.) and provides opportunities to design hybrid particles for a range of advanced applications.
quote
| GB/T 7714-2015 | [1] Matthew C. D. Carter, Liang Chen, Robert S. Moglia, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00848. |
| MLA | [1] Matthew C. D. Carter, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00848. |
| APA | [1] Matthew C. D. Carter, Liang Chen, Robert S. Moglia, Pu Luo, Tanvi S. Ratani, Miroslav Janco, Junsi Gu, Johnpeter N. Ngunjiri, Wei Gao, Catheryn L. Jackson, & Ralph C. Even. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00848 |
| IEEE | [1] Matthew C. D. Carter, Liang Chen, Robert S. Moglia, Pu Luo, Tanvi S. Ratani, Miroslav Janco, Junsi Gu, Johnpeter N. Ngunjiri, Wei Gao, Catheryn L. Jackson, and Ralph C. Even, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00848. keywords: {latex;hybrid;emulsion polymerization;dispersion;acrylic;polyolefin} |