Effect of WC Grain Size of Ultrafine WC-Co Cemented Carbide on its Friction and Wear Properties AITranslate
Abstract AITranslate
In order to study the effect of WC grain size of ultrafine cemented carbide on its friction and wear properties, ultrafine cemented carbides with the average WC grain sizes of 0.25 μm, 0.35 μm and 0.50 μm were prepared by different sintering processes.The alloys were characterized and analyzed by density ba-lance, hardness tester, friction and wear tester, 3 D contour scanner and scanning electron microscope.The results show that the relative density and hardness of the alloys decrease with the increase of WC grain size.The alloy with an average WC grain size of 0.25 μm has high hardness, can effectively resist the effect of grinding balls during reciprocating friction, and has a shallow depth of wear scars, showing good wear resistance.When the average WC grain size increases to 0.35 μm, the penetration depth of the grinding ball significantly increases, and the wear resistance of the alloy decreases.Continuing to increase the average WC grain size to 0.50 μm, the hardness of the alloy continues to decrease, some broken WC particles appear in the wear morphology, the penetration depth of the grinding ball further increases, and the wear resistance is the worst.
KeyWords AITranslate
1羊求民,羊建高,苏伟,陈丽勇,陈颢,郭圣达.纳米/超细晶WC-Co类硬质合金的研究进展[J].稀有金属与硬质合金,2018,46(1):76-83. 被引量:18
2鄢志刚,雷纯鹏,蔡海燕,吴爱华,唐建成.原料形貌特性和高温梯度碳化工艺对纳米WC粉末及其WC-Co合金均匀性的影响[J].硬质合金,2021,38(4):255-263. 被引量:1
3张璐,李剑峰,尹运春,刘渊溢,陆必志.WC粉末特性对超细晶硬质合金烧结敏感性影响的研究[J].硬质合金,2020,37(1):51-59. 被引量:8
4马青龙,陈名海,刘宁,李清文,王达飞,曹浩.Cr_3C_2添加量对WC-12%Co超细硬质合金组织和性能的影响[J].硬质合金,2019,36(1):29-37. 被引量:4
5陈开远,全利铭,何颖晗,袁源,何朗,袁志,刘来君.高温高压烧结制备WC-6Co硬质合金及其力学性能研究[J].稀有金属与硬质合金,2021,49(3):80-86. 被引量:3
6李萌,弓满锋,张程煜,莫德云,李玫,韩栋,张洪军.超细、纳米晶WC-Co硬质合金烧结技术的研究现状[J].材料导报,2020,34(15):15138-15144. 被引量:8
7刘少存,吴鹏,童森,游天亨,曾广标.纳米WC-6%Co复合粉的放电等离子烧结研究[J].硬质合金,2017,34(6):413-418. 被引量:1
8汪振华,刘奎,黄雷,袁军堂.放电等离子烧结WC-6wt.%Co-VC超细晶硬质合金力学性能和微观组织研究[J].南京理工大学学报,2020,44(5):524-530. 被引量:2
9周瀚翔,汪振华,贾继恒.TiC含量对WC-8Co超细晶硬质合金力学性能和微观组织的影响[J].稀有金属与硬质合金,2020,48(2):75-81. 被引量:4
10刘益兴,雍薇,彭晖,王晓灵.退火热处理对WC-6%Co超细晶硬质合金抗弯强度的影响[J].硬质合金,2020,37(2):127-132. 被引量:3
1李蓉蓉,尹延国,张国涛,张开源,陈奇.以TiH2为造孔剂的球磨铁基含油材料孔隙表征及其摩擦学性能[J].润滑与密封,2020,45(7):75-80. 被引量:2
2邵志松,高伟,延鹏飞,王东雪.树脂金刚石线在硅晶体切片时的磨损形貌研究[J].工具技术,2022,56(6):61-64.
3刘英凯,周洋,刘建刚,郝文龙.钴粉包覆的铸造WC颗粒在金刚石锯片中的应用[J].金刚石与磨料磨具工程,2022,42(3):379-383.
4罗健,张国栋,胡文亮,魏晓晗,何玉春.低渗储层泥浆侵入特征与时移电阻率测井评价[J].海洋石油,2022,42(2):55-60. 被引量:1
5杨忠国,付欣悦,衣淑娟,王石,李强,郭胜杰.不同沉积方式对Ni-W/SiC复合镀层组织及摩擦性能的影响[J].功能材料,2022,53(6):6205-6211.
6门志远,刘硕,李昀东,宣立强,蔡璐瑶.哈尔滨新区不同下垫面悬浮大气微塑料污染特征及潜在生态风险评估[J].环境科学学报,2022,42(6):329-336. 被引量:1
7杨蕊,门天剑,李珂奕,于海,余昊翰,宋文,蒙萌.微观组织结构对纳米氟磷灰石饰瓷磨损行为的影响研究[J].实用口腔医学杂志,2022,38(3):310-316.
8段凯月,国秀花,宋克兴,钟建英,李凯,王旭,冯江,段俊彪,张颖.WC/CuCr30复合材料的组织性能及耐电弧侵蚀行为[J].材料热处理学报,2022,43(6):26-33.
9曾涛,郭亮,侯江,廖望,陈雪,王国强,黄晓宗.一种采用低阈值技术实现的高速模数转换器[J].微电子学,2022,52(2):206-210.
10钱维兴,李杰,盛耀飚,刘成威,覃恩伟,陈国星,陆海峰,魏少翀,尹嵩,吴树辉.2种FeCr基高速电弧涂层的组织和耐磨性能对比研究[J].材料保护,2022,55(5):10-17.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
In order to study the effect of WC grain size of ultrafine cemented carbide on its friction and wear properties, ultrafine cemented carbides with the average WC grain sizes of 0.25 μm, 0.35 μm and 0.50 μm were prepared by different sintering processes.The alloys were characterized and analyzed by density ba-lance, hardness tester, friction and wear tester, 3 D contour scanner and scanning electron microscope.The results show that the relative density and hardness of the alloys decrease with the increase of WC grain size.The alloy with an average WC grain size of 0.25 μm has high hardness, can effectively resist the effect of grinding balls during reciprocating friction, and has a shallow depth of wear scars, showing good wear resistance.When the average WC grain size increases to 0.35 μm, the penetration depth of the grinding ball significantly increases, and the wear resistance of the alloy decreases.Continuing to increase the average WC grain size to 0.50 μm, the hardness of the alloy continues to decrease, some broken WC particles appear in the wear morphology, the penetration depth of the grinding ball further increases, and the wear resistance is the worst.
quote
| GB/T 7714-2015 | [1] LUO Xin, HONG Yuan-kun, WU Jia-yi, et al. Effect of WC Grain Size of Ultrafine WC-Co Cemented Carbide on its Friction and Wear Properties[J]. Rare Metals and Cemented Carbides, 2022(3): 93-97. |
| MLA | [1] LUO Xin, et al., "Effect of WC Grain Size of Ultrafine WC-Co Cemented Carbide on its Friction and Wear Properties." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 93-97. |
| APA | [1] LUO Xin, HONG Yuan-kun, WU Jia-yi, LI Shao-xuan, & YANG Qiu-min. (2022). Effect of WC Grain Size of Ultrafine WC-Co Cemented Carbide on its Friction and Wear Properties. Rare Metals and Cemented Carbides(3), 93-97. |
| IEEE | [1] LUO Xin, HONG Yuan-kun, WU Jia-yi, LI Shao-xuan, and YANG Qiu-min, "Effect of WC Grain Size of Ultrafine WC-Co Cemented Carbide on its Friction and Wear Properties," Rare Metals and Cemented Carbides, no. 3, pp. 93-97, 2022. keywords: {ultrafine cemented carbide;WC grain size;friction and wear;density;hardness;morphology} |