Study on Tungsten Extraction from Crystal Mother Liquor of Ammonium Paratungstate in N235/Isooctanol System AITranslate
Abstract AITranslate
A new process for the extraction and recovery of tungsten from APT crystal mother liquor in N235/isooctanol system was proposed and studied.The effects of organic phase composition,feed pH,temperature and other factors on tungsten extraction were studied.The extraction and stripping isotherms were drawn.And the test of simulated multi-stage countercurrent extraction was conducted.The results show that high-fold enrichment and recovery of tungsten and efficient separation of SO42-and Cl-from the ammonium paratungstate crystal mother liquor can be achieved in the solvent extraction system of N235/isooctanol.When the acidified feed liquid with WO3content of 22.1g/L and pH value of 3.5is subjected to4-stage countercurrent extraction,1-stage washing and 2-stage stripping,and the organic phase consisting of 10%N235,20%isooctanol and sulfonated kerosene is used,the results are obtained as follows:WO3content in the raffinate is less than 0.02g/L,WO3recovery rate is higher than 99.5%,WO3content in the stripping solution is higher than 230g/L,and the removal rate of SO42-or Cl-is greater than 98.5%.
KeyWords AITranslate
1罗爱平,张启修.电渗析处理APT结晶母液的研究[J].中南矿冶学院学报,1994,25(1):44-48. 被引量:4
2孙培梅,李洪桂,李运姣,苏鹏抟,霍广生,赵中伟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼的工业试验[J].中国有色金属学报,2001,11(3):499-502. 被引量:22
3邓解德.离子交换法回收仲钨酸铵结晶母液中的钨[J].中国钨业,1999,14(1):29-32. 被引量:7
4牟德渊.离子交换法从APT结晶母液中回收钨酸钠[J].离子交换与吸附,1995,11(6):558-561. 被引量:5
5张启修,黄蔚庄,周志孝.N_(1923)-异辛醇体系萃取钨的研究[J].稀有金属与硬质合金,1989(2):16-21. 被引量:3
6张子岩,简椿林.溶剂萃取法在钨湿法冶金中的应用[J].湿法冶金,2006,25(1):1-9. 被引量:18
1张鹤鹏,陈金清.疏水低共熔溶剂萃取金属离子研究进展[J].有色金属科学与工程,2021,12(4):9-18. 被引量:4
2季宏祥,宋宗仁,江银,马晓雪,房大维.辛胺萃取银的热力学研究[J].稀有金属与硬质合金,2021,49(5):17-23. 被引量:1
3王欣欣,王俊杰,张建,刘德智,陈利革,王松涛,琚成新.N263-异辛醇-磺化煤油萃取碱浸出液中钨钼的研究[J].中国钨业,2022,37(6):48-52.
1王亚波.低共熔溶剂中苯乙烯-丙烯酰胺共聚行为研究[J].科学技术创新,2022(9):5-8.
2李宏,谭秀民,张秀峰,张利珍,伊跃军,王威.铍资源现状及其选冶技术进展[J].有色金属科学与工程,2022,13(4):44-53. 被引量:3
3吴霞,齐艳杰,周瑞,陕洁.《物理化学》课程中启发式教学[J].化工设计通讯,2022,48(8):128-131.
4曾颜亮,霍瑞浩,邹建柏,廖春发,刘付朋.铜阳极泥复合浸出渣选择性分离硒过程热力学分析[J].有色金属科学与工程,2023,14(1):1-7. 被引量:1
5姚贤锐,黄睿,虞育杰,唐瑜慕,何禹,李剑烽.疏水深共熔溶剂在绿色化学工艺中的应用[J].精细化工,2023,40(5):953-967.
1周洁英,杨幼明.240#新型环烷酸萃取铝的研究[J].稀有金属,2021,45(1):85-92. 被引量:1
2卿家林,张贵清,曾理,关文娟,巫圣喜,李青刚,曹佐英,武新生.P204/4PC协同萃取分离镍钴与镁钙的研究[J].矿冶工程,2021,41(1):101-105. 被引量:7
3廖惠云,吴洋,孙海平,叶远青,王晨辉,曹毅,张华,朱怀远.固相萃取净化-双填料反萃取-GC/MS法分析卷烟烟气中甲基丁香酚[J].烟草科技,2021,54(4):66-73. 被引量:1
4辛金妮,王丹君,李正,刘美芳,孙显锋.采用溶剂萃取技术生产环保橡胶填充油的研究进展[J].石化技术与应用,2021,39(2):143-146. 被引量:4
5房孟钊,余珊,李伟,彭明,宁瑞.赞比亚某铜钴矿金属回收试验研究[J].中国有色冶金,2021,50(1):86-89. 被引量:4
6罗进爱,肖超,陈宁,许名臣,郑继明,徐靖宸.工业氧化钼提纯新工艺研究[J].稀有金属与硬质合金,2021,49(1):7-12. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
A new process for the extraction and recovery of tungsten from APT crystal mother liquor in N235/isooctanol system was proposed and studied.The effects of organic phase composition,feed pH,temperature and other factors on tungsten extraction were studied.The extraction and stripping isotherms were drawn.And the test of simulated multi-stage countercurrent extraction was conducted.The results show that high-fold enrichment and recovery of tungsten and efficient separation of SO42-and Cl-from the ammonium paratungstate crystal mother liquor can be achieved in the solvent extraction system of N235/isooctanol.When the acidified feed liquid with WO3content of 22.1g/L and pH value of 3.5is subjected to4-stage countercurrent extraction,1-stage washing and 2-stage stripping,and the organic phase consisting of 10%N235,20%isooctanol and sulfonated kerosene is used,the results are obtained as follows:WO3content in the raffinate is less than 0.02g/L,WO3recovery rate is higher than 99.5%,WO3content in the stripping solution is higher than 230g/L,and the removal rate of SO42-or Cl-is greater than 98.5%.
quote
| GB/T 7714-2015 | [1] LONG Yu-chen, ZHANG Gui-qing, ZENG Li, et al. Study on Tungsten Extraction from Crystal Mother Liquor of Ammonium Paratungstate in N235/Isooctanol System[J]. Rare Metals and Cemented Carbides, 2021(1): 1-6. |
| MLA | [1] LONG Yu-chen, et al., "Study on Tungsten Extraction from Crystal Mother Liquor of Ammonium Paratungstate in N235/Isooctanol System." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 1-6. |
| APA | [1] LONG Yu-chen, ZHANG Gui-qing, ZENG Li, WU Xin-sheng, LI Zhi-hua, QIN Jia-lin, GUAN Wen-juan, LI Qing-gang, CAO Zuo-ying, & WU Sheng-xi. (2021). Study on Tungsten Extraction from Crystal Mother Liquor of Ammonium Paratungstate in N235/Isooctanol System. Rare Metals and Cemented Carbides(1), 1-6. |
| IEEE | [1] LONG Yu-chen, ZHANG Gui-qing, ZENG Li, WU Xin-sheng, LI Zhi-hua, QIN Jia-lin, GUAN Wen-juan, LI Qing-gang, CAO Zuo-ying, and WU Sheng-xi, "Study on Tungsten Extraction from Crystal Mother Liquor of Ammonium Paratungstate in N235/Isooctanol System," Rare Metals and Cemented Carbides, no. 1, pp. 1-6, 2021. keywords: {crystal mother liquor of ammonium paratungstate;tungsten;recovery;solvent extraction;N235} |