Effect of Ti Element on the Microstructure and Mechanical Properties of Industrial Grade Zr-Ti Alloy Sheet AITranslate

Xi'an Western Energy Material Technologies Co.,Ltd.;Xi'an Western Energy Material Technologies Co.,Ltd.;Xi'an Western Energy Material Technologies Co.,Ltd.;Xi'an Western Energy Material Technologies Co.,Ltd.;Xi'an Western Energy Material Technologies Co.,Ltd.;Xi'an Western Energy Material Technologies Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Zr-Ti alloys with different Ti contents(0~15%by mass)were first prepared by vacuum consumable arc melting,and then turned into sheet samples.The metallographic microstructure of different alloy sheets was analyzed by optical microscope(OM),the mechanical properties by Vickers hardness tester and universal electronic tensile testing machine,and the fracture morphology by scanning electron microscope(SEM).The results show that Ti element can obviously refine the microstructure of Zr-Ti alloy.With the increase of Ti content,the hardness and strength of the Zr-Ti alloy sheets significantly improve,but the elongation decreases markedly.The fracture morphology of all the Zr-Ti alloy sheets is composed of dimples,indicating ductile fracture.And with the increase in Ti content,the fracture dimples of the alloy sheets become shallower,indicating that the ductile fracture characteristics of the alloy are weakened and the machinability is deteriorated.

KeyWords AITranslate

Zr-Ti alloy Ti content metallographic microstructure mechanical property fracture mode
No data

Basic Information:

DOI:

Chinese Library Classification Number:TG146.414[金属学及工艺—金属材料]

Citation Information:

Zr-Ti alloys with different Ti contents(0~15%by mass)were first prepared by vacuum consumable arc melting,and then turned into sheet samples.The metallographic microstructure of different alloy sheets was analyzed by optical microscope(OM),the mechanical properties by Vickers hardness tester and universal electronic tensile testing machine,and the fracture morphology by scanning electron microscope(SEM).The results show that Ti element can obviously refine the microstructure of Zr-Ti alloy.With the increase of Ti content,the hardness and strength of the Zr-Ti alloy sheets significantly improve,but the elongation decreases markedly.The fracture morphology of all the Zr-Ti alloy sheets is composed of dimples,indicating ductile fracture.And with the increase in Ti content,the fracture dimples of the alloy sheets become shallower,indicating that the ductile fracture characteristics of the alloy are weakened and the machinability is deteriorated.

quote

GB/T 7714-2015 [1] WEI Tong-yu, YAN Bao-hui, TIAN Feng, et al. Effect of Ti Element on the Microstructure and Mechanical Properties of Industrial Grade Zr-Ti Alloy Sheet[J]. Rare Metals and Cemented Carbides, 2024(4): 64-68.
MLA [1] WEI Tong-yu, et al., "Effect of Ti Element on the Microstructure and Mechanical Properties of Industrial Grade Zr-Ti Alloy Sheet." Rare Metals and Cemented Carbides, no. 4, 2024, pp. 64-68.
APA [1] WEI Tong-yu, YAN Bao-hui, TIAN Feng, ZHOU Xuan, YUAN Bo, & SUN Tao-tao. (2024). Effect of Ti Element on the Microstructure and Mechanical Properties of Industrial Grade Zr-Ti Alloy Sheet. Rare Metals and Cemented Carbides(4), 64-68.
IEEE [1] WEI Tong-yu, YAN Bao-hui, TIAN Feng, ZHOU Xuan, YUAN Bo, and SUN Tao-tao, "Effect of Ti Element on the Microstructure and Mechanical Properties of Industrial Grade Zr-Ti Alloy Sheet," Rare Metals and Cemented Carbides, no. 4, pp. 64-68, 2024. keywords: {Zr-Ti alloy;Ti content;metallographic microstructure;mechanical property;fracture mode}