Research on Microstructure and Mechanical Properties of Ti-1100 Alloy Containing Yb2O3 AITranslate
Abstract AITranslate
Ti-1100 alloys with varying Yb2O3contents were prepared by melting-casting method.The mi-crostructural evolution of the alloys were observed by field emission scanning electron microscopy,and the mechanical properties were analyzed through isothermal compression tests conducted on an electronic uni-versal testing machine.The results indicate that the addition of Yb2O3can significantly reduce the grain size of Ti-1100 alloy,the spacing betweenα-lamellae in the grains is smaller,and the distribution ofαla-mellae is denser.With the increase of Yb2O3content,the grain size of the alloy decreases first and then in-creases,and the strength initially increases before decreasing.When the Yb2O3content reaches 0.45%,the alloy exhibits the minimum grain size and maximum strength.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TG294[金属学及工艺]
Citation Information:
Ti-1100 alloys with varying Yb2O3contents were prepared by melting-casting method.The mi-crostructural evolution of the alloys were observed by field emission scanning electron microscopy,and the mechanical properties were analyzed through isothermal compression tests conducted on an electronic uni-versal testing machine.The results indicate that the addition of Yb2O3can significantly reduce the grain size of Ti-1100 alloy,the spacing betweenα-lamellae in the grains is smaller,and the distribution ofαla-mellae is denser.With the increase of Yb2O3content,the grain size of the alloy decreases first and then in-creases,and the strength initially increases before decreasing.When the Yb2O3content reaches 0.45%,the alloy exhibits the minimum grain size and maximum strength.
quote
| GB/T 7714-2015 | [1] JIA Bao-hua, ZANG Wen-qiang, LIU Xiang, et al. Research on Microstructure and Mechanical Properties of Ti-1100 Alloy Containing Yb2O3[J]. Rare Metals and Cemented Carbides, 2025(4): 92-96. |
| MLA | [1] JIA Bao-hua, et al., "Research on Microstructure and Mechanical Properties of Ti-1100 Alloy Containing Yb2O3." Rare Metals and Cemented Carbides, no. 4, 2025, pp. 92-96. |
| APA | [1] JIA Bao-hua, ZANG Wen-qiang, LIU Xiang, LI Ge, & GU Yong-qiang. (2025). Research on Microstructure and Mechanical Properties of Ti-1100 Alloy Containing Yb2O3. Rare Metals and Cemented Carbides(4), 92-96. |
| IEEE | [1] JIA Bao-hua, ZANG Wen-qiang, LIU Xiang, LI Ge, and GU Yong-qiang, "Research on Microstructure and Mechanical Properties of Ti-1100 Alloy Containing Yb2O3," Rare Metals and Cemented Carbides, no. 4, pp. 92-96, 2025. keywords: {rare earth;YbO;titanium alloy;microstructure;mechanical property} |