The Present Application of Microwave Heating in Tungsten Industry AITranslate
Abstract AITranslate
Principle and advantages of microwave heating are introduced,and the present application of microwave heating in tungsten industry is emphatically reviewed.
KeyWords AITranslate
1Galema S A. Microwave Chemistry[J]. Chem Soc Rev, 1997,26(3) :233-238.
2黄铭,彭金辉,王家强,张世敏,张利波,郭胜惠,夏洪应.微波与物质相互作用加热机理的理论研究[J].昆明理工大学学报:理工版,2005,30(6):15-17. 被引量:14
3卢凯.微波的原理及特点[J].农业机械化与电气化,2007(1):61-62. 被引量:16
4刘书祯,白燕,程艳明,钟文.微波技术在冶金中的应用[J].湿法冶金,2011,30(2):91-94. 被引量:15
5谷晋川,刘亚川,谢扩军,张允湘.难选冶金矿微波预处理研究[J].有色金属,2003,55(2):55-57. 被引量:32
6Nanthakumar B, Pickles C A, Kelebek S. Microwave pretreatment of a double refractory gold ore[J]. Minerals Engineering,2007,10(20):1 109-1 119.
7周晓东,张云梅,李理.微波辐照氨浸氧化铜矿的试验研究[J].红河学院学报,2007,5(2):31-33. 被引量:10
8Standish N,Worner H. Microwave application in the reduction of metal oxides with carbon[J]. Microwave Power and Electromagnetic Energy, 1990,25(3):177-180.
9黄孟阳,彭金辉,黄铭,张世敏,李雨,雷鹰.微波场中不同配碳量钛精矿的吸波特性[J].中国有色金属学报,2007,17(3):476-480. 被引量:22
10Kocakusak S, Koroglu H J, Tolun R. Drying of boric acid by microwave heating[J]. Chemical Engineering and Processing, 1998,37 : 197-201.
1曹占芳,钟宏,刘广义,王帅.我国矿产资源的特点及其加工技术与专业教学现状[J].稀有金属与硬质合金,2012,40(5):18-22. 被引量:2
2章晓波,孙文,陈永明,沈崇.粉末轧制-叠层烧结法制备较厚93W-4.9Ni-2.1Fe高密度钨合金片材的研究[J].稀有金属与硬质合金,2013,41(5):28-31. 被引量:3
3孙文,章晓波.高密度钨合金烧结新工艺研究现状[J].稀有金属与硬质合金,2014,42(2):36-40. 被引量:3
1刘吉波,杨涛,王志坚,苏正夫,成维.废旧稀土荧光灯资源的回收方法研究现状[J].稀有金属与硬质合金,2014,42(2):29-31. 被引量:3
2孙文,章晓波.高密度钨合金烧结新工艺研究现状[J].稀有金属与硬质合金,2014,42(2):36-40. 被引量:3
3邹树梁,颜亮,唐德文,谢宇鹏,张德.高密度W-Ni-Fe合金制备与应用研究进展[J].南华大学学报:自然科学版,2015,29(1):53-59. 被引量:3
4武杰,孙毅,王晖.烧结和热处理对WNiFe合金板材轧制性能的影响[J].热加工工艺,2016,45(20):239-241. 被引量:2
5田野,孙大智,李萍,梁辰,华睿.高压扭转对难熔金属粉末钨致密固结及强韧化的影响研究[J].稀有金属与硬质合金,2016,44(5):37-42. 被引量:1
6程琛,冯松宝.矿产资源综合利用课程教学改革[J].阴山学刊:自然科学版,2017,31(3):108-110.
7崔利群,韩胜利,施麒,李达人,胡建召,刘祖岩.钨铜粉末轧制的有限元模拟研究[J].粉末冶金材料科学与工程,2019,24(5):406-412. 被引量:1
1刘书祯,白燕,程艳明,钟文.微波技术在冶金中的应用[J].湿法冶金,2011,30(2):91-94. 被引量:15
2刘能生,彭金辉,张利波,张泽彪.微波技术在稀贵金属冶金中的研究应用进展[J].贵金属,2009,30(4):48-51. 被引量:5
3袁鹏,李保平,王介强.微波均相沉淀法合成纳米粉体的研究进展[J].中国粉体技术,2008,14(2):50-53. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF19[冶金工程—冶金物理化学]
Citation Information:
Principle and advantages of microwave heating are introduced,and the present application of microwave heating in tungsten industry is emphatically reviewed.
quote
| GB/T 7714-2015 | [1] LIU Shu-zhen, LI Jie, CHENG Yan-ming. The Present Application of Microwave Heating in Tungsten Industry[J]. Rare Metals and Cemented Carbides, 2012(1): 51-54. |
| MLA | [1] LIU Shu-zhen, et al., "The Present Application of Microwave Heating in Tungsten Industry." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 51-54. |
| APA | [1] LIU Shu-zhen, LI Jie, & CHENG Yan-ming. (2012). The Present Application of Microwave Heating in Tungsten Industry. Rare Metals and Cemented Carbides(1), 51-54. |
| IEEE | [1] LIU Shu-zhen, LI Jie, and CHENG Yan-ming, "The Present Application of Microwave Heating in Tungsten Industry," Rare Metals and Cemented Carbides, no. 1, pp. 51-54, 2012. keywords: {microwave heating;tungsten industry;application} |