Research on the Microstructure and Properties of the As-cast Cr_xNbTiZr High Entropy Alloys AITranslate
Abstract AITranslate
The CrxNbTiZr high entropy alloys of mixed strengthening effects were designed according to the phase formation criterion.The effect of chromium on the microstructure and mechanical properties of the CrxNbTiZr high entropy alloys was researched by X-ray diffractometer,scanning electron microscope and universal mechanical testing machine.The results show that the CrxNbTiZr high entropy alloys are composed of BCC phase and some Cr2M(M=Nb,Ti,Zr) Laves-phase intermetallic compounds.The alloys present typical dendritic morphology,in which the second phase discontinuously precipitates.By the solid solution strengthening of Cr and the second phase strengthening of Laves phase,the Cr1.0 alloy possesses the yield strength up to 1 401 MPa,the compressive strength up to 1 677 MPa and the fracture strain down to 13.30%.The fracture morphology analysis shows that the series of alloys have the mixed fracture cha-racteristics of ductility and brittleness.
KeyWords AITranslate
1徐义库,李聪玲,黄兆皓,陈永楠,朱丽霞.定向凝固CoCrCuFeNiTi_(0.8)高熵合金的组织与力学性能[J].中国有色金属学报,2021,31(6):1494-1504. 被引量:1
2贺毅强,苏前航,徐虎林,任昌旭,徐苏,穆昱学,刘勇.AlxFeNiSiTi高熵合金的显微组织与力学性能研究[J].稀有金属与硬质合金,2021,49(4):71-75.
3应泽辰,高妞,谢伦杰,程奎,马县能,杨力,樊自田,刘鑫旺.多主元高熵合金的凝固组织及晶粒细化进展[J].特种铸造及有色合金,2021,41(8):944-951. 被引量:4
4刘亚玲,杨佳惠,武俊霞,董洪峰,李培友.难熔高熵合金的研究进展[J].稀有金属与硬质合金,2021,49(5):59-64. 被引量:1
5时海芳,李强.碳含量对Al_(0.5)Co_(0.5)NiCrFe高熵合金涂层组织与性能的影响[J].金属热处理,2022,47(3):136-141. 被引量:1
1王军,林凯茜,范嘉懿,李金山.难混溶高熵合金研究进展[J].特种铸造及有色合金,2022,42(12):1472-1479.
2蒋爱云,任波,陈冲,周亚军,耿和川,李鹏飞.Nb含量对Cu_(0.3)Cr_(2)Fe_(2)Ni_(3)Mn_(2)Nb_(x)高熵合金微观组织和性能的影响[J].特种铸造及有色合金,2022,42(8):930-935. 被引量:1
3李荣斌,邹传乐,张志玺,张如林,彭望君.硼对铸态Al_(0.3)CoCrFeNi高熵合金组织及性能的影响[J].稀有金属材料与工程,2023,52(2):667-674.
4张鸣鹤,纪国宁,刘博皓,赵荣达,伍复发.冷轧和退火对Ni_(40)(FeCoCrAl)_(60)高熵合金组织与性能的影响[J].特种铸造及有色合金,2023,43(3):370-373.
5李卫,李德香,鲁志杰,刘叶诚,吕笑文,徐志彪.碳含量对中频磁控溅射沉积MoCN涂层微观结构及摩擦学性能的影响[J].表面技术,2023,52(4):184-191.
6杨超敏,刘秀波,刘一帆,朱正兴,孟元,张世宏.激光熔覆FeCoCrNiCu_(x)高熵合金涂层的显微组织和摩擦性能[J].中国有色金属学报,2023,33(5):1514-1530.
7孟凡莹,张一凡,杨佳惠,张薇,王琳,武俊霞,李培友.高熵合金催化性能的研究进展[J].材料热处理学报,2023,44(6):20-27.
1胡轶嵩,王凯旋,姜葳,王志宏,赵小花,巨彪,张丰收,刘向宏.β锻造工艺对TC17钛合金组织和力学性能的影响[J].热加工工艺,2020,49(9):41-44. 被引量:3
2匡秀琴,李瑞雷,季清清,江俊杰,金曼.不同热处理对Al-7.95Zn-1.84Mg-0.65Cu合金力学性能和耐腐蚀性能的影响[J].西北工业大学学报,2020,38(3):596-603. 被引量:2
3吴姚莎,张亚民,王丽荣,石澎,张宁,刘孝青.钛对碳纳米管增强铝基复合材料组织与性能的尺寸效应[J].金属热处理,2020,45(8):64-70. 被引量:1
4林峰,陈兴伟,姚文艺,方艺辉,邓海军,吴杰峰,林炳青.基于SWAT模型的森林分布不连续流域水源涵养量多时间尺度分析[J].地理学报,2020,75(5):1065-1078. 被引量:20
Basic Information:
DOI:
Chinese Library Classification Number:TG113[金属学及工艺—物理冶金]
Citation Information:
The CrxNbTiZr high entropy alloys of mixed strengthening effects were designed according to the phase formation criterion.The effect of chromium on the microstructure and mechanical properties of the CrxNbTiZr high entropy alloys was researched by X-ray diffractometer,scanning electron microscope and universal mechanical testing machine.The results show that the CrxNbTiZr high entropy alloys are composed of BCC phase and some Cr2M(M=Nb,Ti,Zr) Laves-phase intermetallic compounds.The alloys present typical dendritic morphology,in which the second phase discontinuously precipitates.By the solid solution strengthening of Cr and the second phase strengthening of Laves phase,the Cr1.0 alloy possesses the yield strength up to 1 401 MPa,the compressive strength up to 1 677 MPa and the fracture strain down to 13.30%.The fracture morphology analysis shows that the series of alloys have the mixed fracture cha-racteristics of ductility and brittleness.
quote
| GB/T 7714-2015 | [1] XU Jin-liang, WANG Tao, ZHANG Shan-nan, et al. Research on the Microstructure and Properties of the As-cast Cr_xNbTiZr High Entropy Alloys[J]. Rare Metals and Cemented Carbides, 2020(4): 53-58. |
| MLA | [1] XU Jin-liang, et al., "Research on the Microstructure and Properties of the As-cast Cr_xNbTiZr High Entropy Alloys." Rare Metals and Cemented Carbides, no. 4, 2020, pp. 53-58. |
| APA | [1] XU Jin-liang, WANG Tao, ZHANG Shan-nan, WEI Wen-chao, & WANG Chun-yu. (2020). Research on the Microstructure and Properties of the As-cast Cr_xNbTiZr High Entropy Alloys. Rare Metals and Cemented Carbides(4), 53-58. |
| IEEE | [1] XU Jin-liang, WANG Tao, ZHANG Shan-nan, WEI Wen-chao, and WANG Chun-yu, "Research on the Microstructure and Properties of the As-cast Cr_xNbTiZr High Entropy Alloys," Rare Metals and Cemented Carbides, no. 4, pp. 53-58, 2020. keywords: {CrNbTiZr;high entropy alloy;phase formation criterion;microstructure;mechanical property} |