daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Selecting Doped Er3+/Ho3+/Tm3+ in the Perovskite-Like Material Cs3YF6: Yb3+ to Achieve Ultrasensitive Luminescence Intensity Ratio Temperature Sensing AITranslate

Jilin University; Jilin University; Jilin University; Jilin University;Zhong Sheng (Shen Zhen) Medical Equipment Science and Technology Co., Ltd.; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Luminescence intensity ratio (LIR) thermometry based on distinct up-conversion luminescence centers was established in Cs-based fluorides. By contrasting the nonthermally coupled luminescence intensity of Er3+/Ho3+/Tm3+, it is possible to determine which kind of up-conversion emission ion is more suited for the perovskite-like Cs3YF6 material. The best option is Er-doped Cs3YF6 samples with a relative sensitivity (Sr) of 0.96% K–1, according to a comparison of the LIR fitting findings. However, the extremely high absolute sensitivity (Sa) in Cs3YF6: Yb, Tm suggests that Sa is not trustworthy in the LIR temperature evaluation system according to the temperature resolution δT. This work provides recommendations for the LIR temperature sensing design for comparable Cs-based fluorides while minimizing time and expense.

KeyWords AITranslate

lanthanide dopant upconversion luminescence luminescence intensity ratio optical material temperature sensing relative sensitivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01306

Chinese Library Classification Number:

Citation Information:

Luminescence intensity ratio (LIR) thermometry based on distinct up-conversion luminescence centers was established in Cs-based fluorides. By contrasting the nonthermally coupled luminescence intensity of Er3+/Ho3+/Tm3+, it is possible to determine which kind of up-conversion emission ion is more suited for the perovskite-like Cs3YF6 material. The best option is Er-doped Cs3YF6 samples with a relative sensitivity (Sr) of 0.96% K–1, according to a comparison of the LIR fitting findings. However, the extremely high absolute sensitivity (Sa) in Cs3YF6: Yb, Tm suggests that Sa is not trustworthy in the LIR temperature evaluation system according to the temperature resolution δT. This work provides recommendations for the LIR temperature sensing design for comparable Cs-based fluorides while minimizing time and expense.

quote

GB/T 7714-2015 [1] Hanyu Xu, Mengmeng Dai, Kejie Li, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01306.
MLA [1] Hanyu Xu, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01306.
APA [1] Hanyu Xu, Mengmeng Dai, Kejie Li, Aijun Li, Tianqi Sheng, & Zuoling Fu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01306
IEEE [1] Hanyu Xu, Mengmeng Dai, Kejie Li, Aijun Li, Tianqi Sheng, and Zuoling Fu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01306. keywords: {lanthanide dopant upconversion luminescence luminescence intensity ratio optical material temperature sensing relative sensitivity}