Abstract AITranslate
Abstract. WC-6 %Co cemented carbide samples were prepared with WC powder (FSSS= 2.5 μm) and Co powder (FSSS= 1.0 μm) as the raw material and ZrO2 (3Y) and CeO2 as the additive. The influence was investigated of different additives on microstructure and properties of WC-6%Co cemented carbide. The results show the ZrO2 (3Y) is dispersed in the binder phase in spherical form to improve bending strength of the alloy without significant effect on the grain size of WC. CeO2 can refine the WC grains,re- duce the porosity of cemented carbide and result in uniform microstructure distribution and improved ben- ding strength of the alloy.
KeyWords AITranslate
1安林,韩静涛,陈军.ZrO_2(3Y)增韧增强WC-20%Co金属陶瓷复合材料[J].北京科技大学学报,2006,28(10):959-963. 被引量:1
2李规华,严兰英,张鸿绪,李福春.YG6R稀土硬质合金的研究[J].粉末冶金技术,1994,12(3):206-209. 被引量:11
3罗重麟.稀土元素对硬质合金性能影响的研究[J].硬质合金,1991,8(2):12-19. 被引量:24
4安林,韩静涛,陈军.WC-20%Co添加陶瓷颗粒ZrO_2的试验研究[J].粉末冶金工业,2005,15(3):19-22. 被引量:4
5朱泽华.Zr对WC—TiC—Co硬质合金性能的影响[J].硬质合金,1989(1):17-20. 被引量:1
6刘宝昌,孙友宏,张祖培.稀土强化金刚石-硬质合金复合凿岩柱齿的试验研究[J].矿冶工程,2002,22(2):99-102. 被引量:4
7熊继,沈保罗.混合稀土CeLa对WC-Ni硬质合金性能和显微结构的影响[J].工具技术,2003,37(6):18-20. 被引量:5
8黄长庚.稀土Y,Ce及其添加方式对硬质合金显微结构与性能的影响[J].粉末冶金材料科学与工程,2014,19(5):701-706. 被引量:10
1邹芹,张萌蕾,李艳国,罗永安.WC硬质合金强韧化的研究进展与展望[J].机械工程学报,2021,57(14):195-204. 被引量:6
1全温灿,艾志龙,吴彤,史冠勇,豆志河.自蔓延高温合成制备碳化钨粉的热力学研究[J].江西冶金,2022,42(2):13-17.
2曹瑞军,李开深,李腾飞,何盛亚.金刚石含量对金刚石强化硬质合金耐磨性影响[J].硬质合金,2022,39(3):165-171. 被引量:1
3张云龙,牛楚涵,牛广津,张宇民,李启荣,高志杨,张唯一.La_(2)O_(3)掺杂量对WC-12Co硬质合金微观结构和硬度的影响[J].中国钨业,2022,37(2):53-59.
4杨植富,唐思文,张浩,刘骞,吕峥.微波烧结工艺对NbC-10 vol%Ni金属陶瓷组织与性能的影响[J].材料热处理学报,2022,43(12):10-18.
5杨长春,丁翔,田英豪,袁成清,王韶毅.CeO_(2)改性多尺度WC-CoCr涂层组织结构及空蚀性能研究[J].功能材料,2023,54(4):4027-4033.
6邹芹,李壮,李艳国,贺文全,罗永安.中熵碳化物陶瓷TiC_(0.4)/VC/NbC结合的WC基硬质合金合成与性能[J].中国有色金属学报,2023,33(6):1914-1923.
1专利名称:一种Mo-Si-B金属间化合物棒材及其制备方法[J].中国钼业,2017,41(1):53-53.
2李詠侠,邹丹.纳米硬质合金制备技术的研究[J].稀有金属与硬质合金,2011,39(3):54-57. 被引量:6
3王丽利,李海艳,刘宁.Co含量对硬质合金组织和性能的影响[J].稀有金属与硬质合金,2011,39(1):66-69. 被引量:12
4李海艳,刘宁,王丽利.Cr_3C_2对WC-6.5%Co硬质合金组织和性能的影响[J].热处理,2010,25(2):31-34. 被引量:2
5高晓辉,李玉峰,祝晶晶,景晓燕,张密林.Mg-9.95Li合金表面致密铈转化膜制备及耐蚀性研究[J].稀有金属材料与工程,2017,46(5):1445-1451. 被引量:2
6庞秋,胡志力,王国荣.Ce含量对Ce/Cr涂层开孔Ni-Cr-Fe泡沫合金力学性能的影响(英文)[J].中国有色金属学报:英文版,2017,27(5):1052-1062. 被引量:1
7邱希亮,郝成丽,修子扬,何鹏.石墨烯纳米片对Sn-58Bi钎料显微组织和性能的影响[J].焊接学报,2017,38(4):63-66. 被引量:4
8黄跃,黄琦.机械球磨法制备AZ31合金及其组织性能研究[J].铸造技术,2017,38(5):1135-1137.
9杨林,胡斌,陶欣慈,林立,刘正.T6处理对真空压铸AM50镁合金腐蚀行为的影响[J].沈阳工业大学学报,2017,39(3):264-268. 被引量:3
10吴杰,王忠华,尚根峰,羊建高,刘芳,吕健.喷雾转换法制备超细晶WC-12Co复合粉末HVOF涂层性能研究[J].稀有金属与硬质合金,2017,45(2):39-44. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Abstract. WC-6 %Co cemented carbide samples were prepared with WC powder (FSSS= 2.5 μm) and Co powder (FSSS= 1.0 μm) as the raw material and ZrO2 (3Y) and CeO2 as the additive. The influence was investigated of different additives on microstructure and properties of WC-6%Co cemented carbide. The results show the ZrO2 (3Y) is dispersed in the binder phase in spherical form to improve bending strength of the alloy without significant effect on the grain size of WC. CeO2 can refine the WC grains,re- duce the porosity of cemented carbide and result in uniform microstructure distribution and improved ben- ding strength of the alloy.
quote
| GB/T 7714-2015 | [1] FU Kun, CHEN Er-dong, WU Rong-hua, et al. Influene of ZrO_2(3Y)and CeO_2 on Microstructure and Properties of Fine Grained WC-6%Co Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2017(2): 64-68. |
| MLA | [1] FU Kun, et al., "Influene of ZrO_2(3Y)and CeO_2 on Microstructure and Properties of Fine Grained WC-6%Co Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 2017, pp. 64-68. |
| APA | [1] FU Kun, CHEN Er-dong, WU Rong-hua, & ZHOU Jian-hua. (2017). Influene of ZrO_2(3Y)and CeO_2 on Microstructure and Properties of Fine Grained WC-6%Co Cemented Carbide. Rare Metals and Cemented Carbides(2), 64-68. |
| IEEE | [1] FU Kun, CHEN Er-dong, WU Rong-hua, and ZHOU Jian-hua, "Influene of ZrO_2(3Y)and CeO_2 on Microstructure and Properties of Fine Grained WC-6%Co Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 64-68, 2017. keywords: {fine grained cemented carbide;WC- 6% Co;ZrO2 (3Y);CeO2;WC grain size;porosity;ben-ding strength} |