Abstract AITranslate

Study is made of the genesis of the aggregate in WC powder. Results show that simple composition and stable properties of W oxide is a prerequisite for quality WC powder with uniform particle size and less aggregate. When normal blue W contains other phases,especially WO 2.72 , the aggregate is liable to form in W and WC powder. The increase of Fe in WC will result in distinct increase of aggregation of WC powder. Different processes will result in different aggregation of W and WC powders from the same raw material. The aggregation is unavoidable when normal blue W is used to produce fine W powder by conventional hydrogen reduction. But the aggregate can be disaggregated in the following operation. If the carburization temperature is too high,the previously loosened aggregate will be bonded more closely and grown, resulting in partial increase of WC Co particle size.

KeyWords AITranslate

WC powder aggregate genesis analysis

1HAUBNERR.etal.InfluenceofAliminium,Silicon,PhosphorusandArsenicontheStabilityofPseudomorphicAgglomeratesduringTungstenReduction[J].InternationalJournalofRefractoryMetalsandHardMaterials,1987,6(1):40.

2LASSNERErik.InfluenceofCarburisationTemperatureonTungstenCarbideProperties[J].InternationalJournalofRefractoryMetalsandHardMaterials,1989,8(3):185.

1彭卫珍.蓝钨物理性能对钨粉和碳化钨粉性能的影响[J].硬质合金,2004,21(3):142-148. 被引量:7

2谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2

3傅小明,吴晓东.用活性氧化钨制取中细W和WC工艺研究[J].稀有金属,2003,27(6):680-683. 被引量:7

1傅小明,钟云波,任忠鸣,邓康.紫钨循环还原氧化制备亚微米钨粉新工艺的研究[J].稀有金属,2005,29(6):851-855. 被引量:3

2罗斌辉,张华明.不同氧化钨原料对钨粉性能的影响研究[J].硬质合金,2006,23(3):139-142. 被引量:14

3刘清才,王海波,孙亚丽.以紫钨为原料制备优质超细WC粉末的实验[J].重庆大学学报:自然科学版,2007,30(5):100-102. 被引量:4

4傅小明.蓝钨循环氧化还原对钨粉末粒度分布的影响[J].硬质合金,2010,27(4):221-223. 被引量:6

5张华民,蔡新余,王在兴.多管炉工作状况下的温度分布[J].硬质合金,2010,27(6):370-375.

6沈志农,杨立.细WC配比对非均匀YG20C合金性能的影响[J].硬质合金,2011,28(3):163-165. 被引量:9

7时凯华,刘小胡,昝秀颀,闵召宇,廖军.深冷处理对添加CeO_2超细WC-9%Ni-Cr_3C_2硬质合金结构、性能与残余应力的影响[J].硬质合金,2014,31(5):283-289. 被引量:3

8钟毓斌,肖晗,孙娟,朱坤.碳化工艺对中细WC粉性能的影响[J].中国钨业,2016,31(4):58-60. 被引量:5

9时凯华,刘小胡,周科朝,闵召宇,廖军,昝秀颀.CeO_2添加及碳含量对超细WC-9Ni-0.4Cr_3C_2硬质合金热性能与表面形态的影响[J].稀有金属材料与工程,2016,45(10):2593-2597. 被引量:1

10姜平国,汪正兵,闫永播,刘文杰.W_(20)O_(58)(010)表面氢吸附机理的第一性原理研究[J].物理学报,2017,66(24):179-189. 被引量:4

1贺洪印,刘海涛,陈伟庆,王国君,付军,刘辉杰.高碳钢小方坯连铸参数优化及铸坯中心偏析控制[J].钢铁钒钛,2011,32(1):84-88. 被引量:17

2傅练英.降低细颗粒碳化钨中聚集体量的研究[J].硬质合金,2001,18(2):93-98. 被引量:4

3张振兴.生产重钨合金粉末新技术[J].中国钨业,1989(11):24-24.

4杨国军,王晓军,冯明昭.煤油聚团法提金新工艺[J].黄金,1995,16(8):26-27. 被引量:1

5包含铁粉、添加剂和流动剂的聚集体的粉末组合物及其制备方法[J].粉末冶金工业,2003,13(3):46-46.

6邹斌,李洪钟,夏亚沈,郭慕孙.快速流化床中聚团大小分布的统计模型[J].化工冶金,1993,14(1):36-43. 被引量:4

7冯强,崔雯雯,张盈,郑诗礼,魏昶,樊刚,张懿.硫酸铵焙烧与浸出提取碳素铬铁冶炼渣中有价金属[J].过程工程学报,2014,14(4):573-579. 被引量:4

8邱文冬,汪锡章,孙加林,潘海燕,洪彦若,金从进.铝锆炭滑板中锆莫来石分解的显微结构研究[J].耐火材料,1999,33(1):9-11. 被引量:7

9国伟林,王西奎.超声波作用下金红石型TiO2枝蔓晶的形成[J].功能材料,2004(z1):3098-3101.

10丁德玲,刘家祥,韩跃新.漩涡状纳米级氧化锌聚集体的制备[J].有色金属,2007,59(4):27-30. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF122.1[冶金工程—粉末冶金];TF125.3[冶金工程—粉末冶金]

Citation Information:

Study is made of the genesis of the aggregate in WC powder. Results show that simple composition and stable properties of W oxide is a prerequisite for quality WC powder with uniform particle size and less aggregate. When normal blue W contains other phases,especially WO 2.72 , the aggregate is liable to form in W and WC powder. The increase of Fe in WC will result in distinct increase of aggregation of WC powder. Different processes will result in different aggregation of W and WC powders from the same raw material. The aggregation is unavoidable when normal blue W is used to produce fine W powder by conventional hydrogen reduction. But the aggregate can be disaggregated in the following operation. If the carburization temperature is too high,the previously loosened aggregate will be bonded more closely and grown, resulting in partial increase of WC Co particle size.

quote

GB/T 7714-2015 [1] XIE Kang-de. Analysis of Genesis of the Aggregate in WC Powder[J]. Rare Metals and Cemented Carbides, 2000(3): 5-10.
MLA [1] XIE Kang-de. "Analysis of Genesis of the Aggregate in WC Powder." Rare Metals and Cemented Carbides, no. 3, 2000, pp. 5-10.
APA [1] XIE Kang-de. (2000). Analysis of Genesis of the Aggregate in WC Powder. Rare Metals and Cemented Carbides(3), 5-10.
IEEE [1] XIE Kang-de, "Analysis of Genesis of the Aggregate in WC Powder," Rare Metals and Cemented Carbides, no. 3, pp. 5-10, 2000. keywords: {WC powder;aggregate;genesis analysis}