Share with WeChat friends or Moments

Abstract AITranslate

Benefiting from the flexibility and low cost, polymer electrolytes are widely used in ultra-thin solid lithium-ion batteries. However, low room-temperature ion conductivity and poor mechanical and thermal stability are key defects hindering the wide application of the polymer solid-state electrolyte. In this work, a cross-linked polypropylene oxide (PPO) polymer solid electrolyte film with excellent mechanical, thermal and electrochemical properties was prepared by introducing the cellulose skeleton, polyglycol (peg400), and zirconia (ZrO2) additives. The cellulose skeleton and peg400 enhance the flexibility, tensile strength and thermal stability(>200 °C) of the electrolyte film, while ZrO2 promotes the movement of polymer segments and the dissociation of lithium salts to improve the ionic conductivity (6.67 × 10–4 S cm–1 at room temperature) and increase the potential window (>4.6 V vs Li/Li+) of the electrolyte. This composite electrolyte film can be used in LiFePO4(LFP) and LiNi0.6Co0.2Mn0.2 (NCM622) solid-state batteries and shows good cycling stability with 600 cycles for LFP. This rigid-flexible composite solid electrolyte film with high ion conductivity and good mechanical and thermal properties has good prospects for application in solid-state Li batteries.

KeyWords AITranslate

composite solid electrolyte polypropylene oxide ZrO2 thermal stability ion conductivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01248

Chinese Library Classification Number:

Citation Information:

Benefiting from the flexibility and low cost, polymer electrolytes are widely used in ultra-thin solid lithium-ion batteries. However, low room-temperature ion conductivity and poor mechanical and thermal stability are key defects hindering the wide application of the polymer solid-state electrolyte. In this work, a cross-linked polypropylene oxide (PPO) polymer solid electrolyte film with excellent mechanical, thermal and electrochemical properties was prepared by introducing the cellulose skeleton, polyglycol (peg400), and zirconia (ZrO2) additives. The cellulose skeleton and peg400 enhance the flexibility, tensile strength and thermal stability(>200 °C) of the electrolyte film, while ZrO2 promotes the movement of polymer segments and the dissociation of lithium salts to improve the ionic conductivity (6.67 × 10–4 S cm–1 at room temperature) and increase the potential window (>4.6 V vs Li/Li+) of the electrolyte. This composite electrolyte film can be used in LiFePO4(LFP) and LiNi0.6Co0.2Mn0.2 (NCM622) solid-state batteries and shows good cycling stability with 600 cycles for LFP. This rigid-flexible composite solid electrolyte film with high ion conductivity and good mechanical and thermal properties has good prospects for application in solid-state Li batteries.

quote

GB/T 7714-2015 [1] Huimin Xu, Maoxiang Jing, Zhenhao Huang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01248.
MLA [1] Huimin Xu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01248.
APA [1] Huimin Xu, Maoxiang Jing, Zhenhao Huang, Jie Li, Tengfei Wang, Weiyong Yuan, Bowei Ju, & Xiangqian Shen. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01248
IEEE [1] Huimin Xu, Maoxiang Jing, Zhenhao Huang, Jie Li, Tengfei Wang, Weiyong Yuan, Bowei Ju, and Xiangqian Shen, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01248. keywords: {composite solid electrolyte;polypropylene oxide;ZrO2;thermal stability;ion conductivity}